    • C08L53/02C08L9/06
    • C08F297/04
    • A block copolymer comprised of a polymer block or blocks (A) comprising conjugated diene monomer units and a polymer block or blocks (B) comprising conjugated diene monomer units and aromatic vinyl monomer units, wherein (1) the polymer block or blocks (A) have a glass transition temperature in the range of −88 to −45° C., (2) the polymer block or blocks (B) have a glass transition temperature in the range of 30 to 90° C., (3) the content of aromatic vinyl monomer units in the block copolymer is in the range of 30 to 52% by weight based on the total weight of the block copolymer, (4) the block copolymer has an aromatic vinyl block ratio of smaller than 69% by weight based on the total weight of the block copolymer, and (5) the viscosity of a 5% by weight solution of the block copolymer in styrene is at least 5 mPa·s but smaller than 30 mPa·s. This block copolymer is used as a modifier for resin.
    • 由包含共轭二烯单体单元的聚合物嵌段或嵌段(A)和包含共轭二烯单体单元和芳族乙烯基单体单元的聚合物嵌段(B)组成的嵌段共聚物,其中(1)聚合物嵌段(A) 玻璃化转变温度在-88〜-45℃的范围内,(2)聚合物嵌段(B)的玻璃化转变温度在30〜90℃的范围内,(3)含量 嵌段共聚物中的芳香族乙烯基单体单元的含量相对于嵌段共聚物的总重量为30〜52重量%的范围,(4)嵌段共聚物的芳香族乙烯基嵌段比小于69重量% 关于嵌段共聚物的总重量,和(5)嵌段共聚物在苯乙烯中的5重量%溶液的粘度为至少5mPa.s但小于30mPa.s。 该嵌段共聚物用作树脂的改性剂。
    • 4. 发明授权
    • Block copolymer, resin composition comprising same, and process for producing the resin composition
    • 嵌段共聚物,包含其的树脂组合物,以及树脂组合物的制造方法
    • US08153727B2
    • 2012-04-10
    • US11920163
    • 2006-05-08
    • Kazuya ItoHidenori YamagishiMasao Nakamura
    • Kazuya ItoHidenori YamagishiMasao Nakamura
    • C08F297/04C08L53/02
    • C08F297/04
    • A block copolymer comprised of a polymer block or blocks (A) comprising conjugated diene monomer units and a polymer block or blocks (B) comprising conjugated diene monomer units and aromatic vinyl monomer units, wherein (1) the polymer block or blocks (A) have a glass transition temperature in the range of −88 to −45° C., (2) the polymer block or blocks (B) have a glass transition temperature in the range of 30 to 90° C., (3) the content of aromatic vinyl monomer units in the block copolymer is in the range of 30 to 52% by weight based on the total weight of the block copolymer, (4) the block copolymer has an aromatic vinyl block ratio of smaller than 69% by weight based on the total weight of the block copolymer, and (5) the viscosity of a 5% by weight solution of the block copolymer in styrene is at least 5 mPa·s but smaller than 30 mPa·s. This block copolymer is used as a modifier for resin.
    • 由包含共轭二烯单体单元的聚合物嵌段或嵌段(A)和包含共轭二烯单体单元和芳族乙烯基单体单元的聚合物嵌段(B)组成的嵌段共聚物,其中(1)聚合物嵌段(A) 玻璃化转变温度在-88〜-45℃的范围内,(2)聚合物嵌段(B)的玻璃化转变温度在30〜90℃的范围内,(3)含量 嵌段共聚物中的芳香族乙烯基单体单元的含量相对于嵌段共聚物的总重量为30〜52重量%的范围,(4)嵌段共聚物的芳香族乙烯基嵌段比小于69重量% 对于嵌段共聚物的总重量,(5)嵌段共聚物在苯乙烯中的5重量%溶液的粘度为至少5mPa·s,但小于30mPa·s。 该嵌段共聚物用作树脂的改性剂。