    • 3. 发明授权
    • Acidproof, hydrolysis-resistant optical and ophathalmic glass of low
density
    • 耐酸,耐水解的光学和光学玻璃的低密度
    • US4400473A
    • 1983-08-23
    • US384462
    • 1982-06-02
    • Karl MennemannGeorg GliemerothVolkmar Geiler
    • Karl MennemannGeorg GliemerothVolkmar Geiler
    • C03C3/064C03C3/066C03C3/068C03C3/072C03C3/074C03C3/08C03C3/10
    • C03C3/074C03C3/064C03C3/066C03C3/068C03C3/072Y10S501/901Y10S501/903
    • An improved optical glass having an index of refraction of .gtoreq.1.69, an Abbe number of .gtoreq.38, and a density of .ltoreq.3.25 g/cm.sup.3, represents a further development of another optical glass recently provided by the same inventors. The new glass has improved suitability for continuous-tank manufacture and increased acidproofness and differs from the other glass in its content of 0.5-4.0% by weight of P.sub.2 O.sub.5 ; its sum total of SiO.sub.2 +B.sub.2 O.sub.3 +Al.sub.2 O.sub.3 +P.sub.2 O.sub.5 being 38.5-41.5% by weight; and its sum total of MgO+CaO being 13-17.5% by weight. The full glass composition, e.g. is in % by weight:______________________________________ SiO.sub.2 26.0-32.5 B.sub.2 O.sub.3 6.0-12.0 Al.sub.2 O.sub.3 0-3.0 P.sub.2 O.sub.5 0.5-4.0 SiO.sub.2 + B.sub.2 O.sub.3 + Al.sub.2 O.sub.3 + P.sub.2 O.sub.5 = 38.5-41.5 Li.sub.2 O 0-5 Na.sub.2 O 0-6 K.sub.2 O 0-8 Li.sub.2 O + Na.sub.2 O + K.sub.2 O = 4.5-12.0 MgO 0-8 CaO 9-16 MgO + CaO = 13-17.5 SrO 0-6 BaO 0-5 ZnO 0-7 PbO 0-4 SrO + BaO + ZnO + PbO = 0-7 MgO + CaO + SrO + BaO + ZnO + PbO = 17-24 La.sub.2 O.sub.3 6-11 ZrO.sub.2 5-8 La.sub.2 O.sub.3 + ZrO.sub.2 = 13.5-17.5 TiO.sub.2 5-9 Nb.sub.2 O.sub.5 6-11 WO.sub.3 0-4 TiO.sub.2 + Nb.sub.2 O.sub.5 + WO.sub.3 = 14-18 La.sub.2 O.sub.3 + ZrO.sub.2 + TiO.sub.2 + Nb.sub.2 O.sub.5 + WO.sub.3 = 28-33 ZrO.sub.2 + TiO.sub.2 + Nb.sub.2 O.sub.5 = 20-26 ______________________________________
    • 具有折射率> / = 1.69,阿贝数≥38,密度为3.25g / cm 3的改进的光学玻璃表示最近由同一发明人提供的另一种光学玻璃的进一步发展 。 新玻璃改善了连续罐制造的适用性和耐酸性,与其他玻璃不同,其含量为P2O5重量的0.5-4.0% 其总计SiO 2 + B 2 O 3 + Al 2 O 3 + P 2 O 5为38.5-41.5%(重量); MgO + CaO的总和为13〜17.5重量%。 全玻璃组合物,例如 为重量%:-SiO2 26.0-32.5 -B2O3 6.0-12.0 -Al2O3 0-3.0 -P2O5 0.5-4.0 -SiO2 + B2O3 + Al2O3 + P2O5 = 38.5-41.5 -Li2O 0-5 -Na2O 0-6-K2O 0-8 -Li2O + Na2O + K2O = 4.5-12.0 -MgO 0-8 -CaO 9-16 -MgO + CaO = 13-17.5 -SrO 0-6 -BaO 0-5 -ZnO 0-7 -PbO 0- 4 -SrO + BaO + ZnO + PbO = 0-7 -MgO + CaO + SrO + BaO + ZnO + PbO = 17-24 -a2O3 6-11-ZrO2 5-8 -La2O3 + ZrO2 = 13.5-17.5 -TiO2 5 -9 -Nb2O5 6-11 -WO3 0-4 -TiO2 + Nb2O5 + WO3 = 14-18 -La2O3 + ZrO2 + TiO2 + Nb2O5 + WO3 = 28-33-ZrO2 + TiO2 + Nb2O5 = 20-26 -