    • 1. 发明授权
    • Ash-free coal production method
    • 无灰煤生产方法
    • US09334457B2
    • 2016-05-10
    • US14358888
    • 2012-12-14
    • Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
    • Koji SakaiNoriyuki OkuyamaShigeru KinoshitaTakuya Yoshida
    • C10L5/04C10L9/00
    • C10L5/04C10L9/00C10L2290/06C10L2290/08C10L2290/24C10L2290/48C10L2290/544
    • Provided is an ash-free coal production method that can produce an ash-free coal efficiently with a higher solvent recovery rate. The ash-free coal production method includes an extraction step of mixing coal with a solvent to give a slurry and heating the slurry to extract a solvent-soluble coal component; a separation step of separating a solution containing the coal component from the slurry containing the extracted coal component; and an ash-free coal obtaining step of separating and recovering the solvent from the separated solution to give an ash-free coal. The ash-free coal obtaining step includes a pressure-reducing substep of reducing a pressure to a level lower than the solvent vapor pressure to evaporatively separate the solvent from the solution to thereby give a solid ash-free coal; and a heating substep of heating the solid ash-free coal to evaporatively separate a residual solvent from the ash-free coal.
    • 提供了一种无灰煤的生产方法,能够以更高的溶剂回收率有效地生产无灰煤。 无灰煤的生产方法包括将煤与溶剂混合以提供浆料并加热浆料以提取溶剂可溶性煤成分的提取步骤; 从含有提取的煤成分的浆料中分离含有煤成分的溶液的分离工序; 和无灰煤获取步骤,从分离的溶液中分离和回收溶剂,得到无灰煤。 无灰煤获取步骤包括将压力降低到低于溶剂蒸气压的水平的减压子步骤,以使溶剂从溶液中蒸发分离,从而得到固体无灰煤; 以及加热子步骤,加热固体无灰煤以将残留溶剂与无灰煤蒸发分离。
    • 3. 发明申请
    • SOLVENT SEPARATION METHOD
    • 溶剂分离方法
    • US20150013215A1
    • 2015-01-15
    • US14372584
    • 2013-01-09
    • Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
    • Koji SakaiNoriyuki OkuyamaShigeru KinoshitaTakuya Yoshida
    • C10L9/02
    • C10L9/02B01D17/0205B01D17/0214B01D17/042C10L1/326C10L9/08C10L2290/46C10L2290/52C10L2290/544C10L2290/547
    • A method for separating solvent-containing water, which is generated in the process for producing an ashless coal, into a solvent and water readily without using any adsorbent or the like (a solvent separation method). The solvent separation method comprises: a solvent-containing water supply step of supplying the solvent-containing water into a pressure vessel for solvent separation purposes; and a temperature retention step of retaining the temperature of the solvent-containing water that has been supplied into the pressure vessel for solvent separation purposes at a predetermined temperature (e.g., 100 to 180 DEG C. inclusive). In the pressure vessel for solvent separation purposes, water in the liquid form moves downward and the solvent moves upward due to the difference between the density of water and the density of the solvent at the predetermined temperature. In this manner, the solvent-containing water can be separated into the solvent and water.
    • 在不使用任何吸附剂等的情况下,容易地将无灰煤制造过程中生成的含有溶剂的水分离成溶剂和水的方法(溶剂分离法)。 溶剂分离方法包括:含溶剂的水供给步骤,将含溶剂的水供给到用于溶剂分离目的的压力容器中; 以及在预定温度(例如,包括100℃至180℃))保持已经供应到压力容器中用于溶剂分离目的的含溶剂的水的温度的温度保持步骤。 在用于溶剂分离的压力容器中,液体形式的水向下移动,溶剂由于水的密度与溶剂在预定温度下的密度之间的差异而向上移动。 以这种方式,可以将含溶剂的水分离成溶剂和水。
    • 6. 发明申请
    • ASH-FREE COAL PRODUCTION METHOD
    • 无ASH无煤生产方法
    • US20140305034A1
    • 2014-10-16
    • US14358888
    • 2012-12-14
    • Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
    • Koji SakaiNoriyuki OkuyamaShigeru KinoshitaTakuya Yoshida
    • C10L5/04
    • C10L5/04C10L9/00C10L2290/06C10L2290/08C10L2290/24C10L2290/48C10L2290/544
    • Provided is an ash-free coal production method that can produce an ash-free coal efficiently with a higher solvent recovery rate. The ash-free coal production method includes an extraction step of mixing coal with a solvent to give a slurry and heating the slurry to extract a solvent-soluble coal component; a separation step of separating a solution containing the coal component from the slurry containing the extracted coal component; and an ash-free coal obtaining step of separating and recovering the solvent from the separated solution to give an ash-free coal. The ash-free coal obtaining step includes a pressure-reducing substep of reducing a pressure to a level lower than the solvent vapor pressure to evaporatively separate the solvent from the solution to thereby give a solid ash-free coal; and a heating substep of heating the solid ash-free coal to evaporatively separate a residual solvent from the ash-free coal.
    • 提供了一种无灰煤的生产方法,能够以更高的溶剂回收率有效地生产无灰煤。 无灰煤的生产方法包括将煤与溶剂混合以提供浆料并加热浆料以提取溶剂可溶性煤成分的提取步骤; 从含有提取的煤成分的浆料中分离含有煤成分的溶液的分离工序; 和无灰煤获取步骤,从分离的溶液中分离和回收溶剂,得到无灰煤。 无灰煤获取步骤包括将压力降低到低于溶剂蒸气压的水平的减压子步骤,以使溶剂从溶液中蒸发分离,从而得到固体无灰煤; 以及加热子步骤,加热固体无灰煤以将残留溶剂与无灰煤蒸发分离。