    • Hydrogenated block copolymer and composition of the same
    • 氢化嵌段共聚物及其组成
    • US06239218B1
    • 2001-05-29
    • US09057404
    • 1998-04-09
    • Jun YonezawaKiyoo KatoEiji SasayaTakashi Sato
    • Jun YonezawaKiyoo KatoEiji SasayaTakashi Sato
    • C08L5302
    • C08L53/00C08F297/04C08L23/10C08L53/005C08L53/025C08L2205/02C08L2205/03C08L2308/00G03F7/0002C08L2666/02C08L2666/24C08L2666/04
    • A hydrogenated block copolymer comprising: at least two polymer blocks A mainly comprising vinylaromatic hydrocarbon compound monomer units; and at least two polymer blocks B mainly comprising hydrogenated conjugated diene compound monomer units, in which at least 90% of the olefinically unsaturated double bonds contained in the unhydrogenated polymer block mainly comprising the conjugated diene compound monomer units is hydrogenated, wherein at least one of the terminal blocks is a polymer block B, the proportion of the terminal polymer block B in the hydrogenated block copolymer being 0.1% by weight or higher and lower than 9.1% by weight, and wherein the content of the vinylaromatic hydrocarbon compound units in the hydrogenated block copolymer is 12% by weight or higher and lower than 25% by weight. Also disclosed are a resin composition containing the hydrogenated block copolymer, and a molded article of the resin composition.
    • 一种氢化嵌段共聚物,其包含:至少两个主要包含乙烯基芳族烃化合物单体单元的聚合物嵌段A; 以及主要包含氢化共轭二烯化合物单体单元的至少两个聚合物嵌段B,其中主要包含共轭二烯化合物单体单元的未氢化聚合物嵌段中包含的至少90%的烯属不饱和双键被氢化,其中至少一个 端基是聚合物嵌段B,氢化嵌段共聚物中的末端聚合物嵌段B的比例为0.1重量%以上且低于9.1重量%,其中氢化的乙烯基芳烃化合物单元的含量 嵌段共聚物为12重量%以上且低于25重量%。 还公开了含有氢化嵌段共聚物的树脂组合物和树脂组合物的模塑制品。
    • 2. 发明授权
    • Hydrogenated block copolymer
    • 氢化嵌段共聚物
    • US06458891B1
    • 2002-10-01
    • US09554314
    • 2000-05-12
    • Jun YonezawaEiji Sasaya
    • Jun YonezawaEiji Sasaya
    • C08F29704
    • C08L25/04C08F8/04C08L23/10C08L23/12C08L25/06C08L53/025C08L71/12C08L71/123C08L2205/02C08L2205/03C08L2205/035C08F297/04C08L2666/24C08L2666/22C08L2666/02C08L2666/04
    • A hydrogenated block copolymer has at least two polymer blocks A each having an aromatic vinyl hydrocarbon compound monomer unit and at least two hydrogenated polymer blocks B each having a hydrogenated butadiene monomer unit. At least 90% of olefinically unsaturated double bonds in the polymer blocks mainly having a butadiene monomer unit before hydrogenation have been hydrogenated. At least one of the locks at the terminal of the hydrogenated block copolymer is the polymer block B. The proportion of the terminal polymer blocks B in the hydrogenated block copolymer is 0.1 wt % to 9.1 wt %. The proportion of the aromatic vinyl hydrocarbon compound in the hydrogenated block copolymer is 25 wt % to 80 wt %. The 1,2-bond content of the polymer blocks having a butadiene monomer unit before hydrogenation averages 60 mol % to 99 mol %. The resulting resin composition improves the balance among the appearance of its molded article, tensile elongation at break and moldability.
    • 氢化嵌段共聚物具有至少两个具有芳族乙烯基烃化合物单体单元和至少两个具有氢化丁二烯单体单元的氢化聚合物嵌段B的聚合物嵌段A. 在氢化之前,主要具有丁二烯单体单元的聚合物嵌段中的至少90%的烯属不饱和双键已被氢化。 氢化嵌段共聚物末端的至少一个锁是聚合物嵌段B.氢化嵌段共聚物中末端聚合物嵌段B的比例为0.1重量%至9.1重量%。 氢化嵌段共聚物中芳香族乙烯基烃化合物的比例为25重量%〜80重量%。 在氢化前具有丁二烯单体单元的聚合物嵌段的1,2-键含量平均为60mol%至99mol%。 所得到的树脂组合物改善了其模制品的外观,断裂拉伸伸长率和成型性之间的平衡。