    • 1. 发明授权
    • Fusing station including multilayer fuser roller
    • 定影台包括多层定影辊
    • US06582222B1
    • 2003-06-24
    • US10139464
    • 2002-05-06
    • Jiann-Hsing ChenJoseph PavliskoRobert A. LancasterNataly Boulatnikov
    • Jiann-Hsing ChenJoseph PavliskoRobert A. LancasterNataly Boulatnikov
    • F27B928
    • B32B1/08B32B15/06G03G15/2057G03G2215/2019
    • A fusing station including an externally heated deformable fuser roller and a relatively harder pressure roller, the fuser roller including a heat distribution layer. A fuser roller embodiment includes a core member, a base cushion layer around the core member, a heat storage layer around the base cushion layer, a heat distribution layer around the heat storage layer, and a thin gloss control layer around the heat distribution layer. Ratios of thermal conductivity divided by thickness for the layers are, respectively: for the base cushion layer, less than approximately 13.3 BTU/hr/ft2/°F.; for the heat storage layer, approximately between 300 BTU/hr/ft2/°F.-1400 BTU/hr/ft2/°F.; for the heat distribution layer, approximately between 600 BTU/hr/ft2/°F.-4,800 BTU/hr/ft2/°F.; and, for the gloss control layer, approximately between 600 BTU/hr/ft2/°F.-6,000 BTU/hr/ft2/°F.
    • 定影台包括外部加热的可变形定影辊和相对较硬的压力辊,该定影辊包括散热层。 定影辊实施例包括芯构件,围绕芯构件的基垫缓冲层,围绕基垫层的储热层,储热层周围的散热层,以及分布层周围的薄光泽控制层。 导热系数除以层的厚度分别为:基底垫层小于约13.3BTU / hr / ft 2 /°F; 大约在300BTU / hr / ft 2 /°F-1400BTU / hr / ft 2 /°F之间的储热层。 大约在600BTU / hr / ft 2 /°F-4,800BTU / hr / ft 2 /°F之间的热分布层; 并且对于光泽度控制层,大约在600BTU / hr / ft 2 /°F-6,000BTU / hr / ft 2 /°F之间。
    • 8. 发明申请
    • Oil-free process for full color digital printing
    • 全彩数字印刷无油过程
    • US20050266332A1
    • 2005-12-01
    • US10857460
    • 2004-05-28
    • Joseph PavliskoJiann-Hsing ChenDinesh TyagiMuhammed Aslam
    • Joseph PavliskoJiann-Hsing ChenDinesh TyagiMuhammed Aslam
    • G03G15/20
    • G03G15/2057G03G2215/2074
    • An oil-free process for forming a fused toner image on a receiver includes forming on a receiver, an image including toner particles that contain a non-crosslinked linear polymeric binder, a wax, and a colorant; and contacting the receiver bearing the toner particle image with a fuser member containing a support, a cushion layer overlying the support, and a release layer overlying the cushion layer. The release layer includes a cured fluorocarbon thermoplastic random copolymer, a cured aminosiloxane copolymer, and a zinc oxide particulate filler. The cured fluorocarbon thermoplastics random copolymer contains —(CH2CF2)x—, —(CF2CF(CF3)y—, and —(CF2CF2)z— subunits, wherein x is from 1 to 40 or 60 to 80 mole percent, y is from 10 to 90 mole percent, z is from 10 to 90 mole percent, and x+y+z equals 100 mole percent. The receiver in contact with the fuser member is subjected to conditions effective in the absence of a release oil for fixing the toner particle image to the receiver.
    • 用于在接收器上形成熔融调色剂图像的无油方法包括在接收器上形成包括含有非交联线性聚合物粘合剂,蜡和着色剂的调色剂颗粒的图​​像; 以及使带有调色剂颗粒图像的接收器与包含支撑件的定影器部件,覆盖在支撑体上的缓冲层和覆盖缓冲层的释放层接触。 脱模层包括固化的氟碳热塑性无规共聚物,固化的氨基硅氧烷共聚物和氧化锌颗粒填料。 固化的碳氟化合物热塑性塑料无规共聚物含有 - (CH 2 CH 2)x - , - (CF 2 C (CF 3)3 - 和 - (CF 2 CH 2 CH 2)z
    • 9. 发明申请
    • Fuser member with tunable gloss level and methods and apparatus for using the same to fuse toner images
    • 具有可调节光泽度的定影器构件以及使用该定影构件来调色剂图像的方法和装置
    • US20050111891A1
    • 2005-05-26
    • US10974141
    • 2004-10-27
    • Jiann-Hsing ChenAndrew CiaschiJoseph PavliskoRobert Lancaster
    • Jiann-Hsing ChenAndrew CiaschiJoseph PavliskoRobert Lancaster
    • G03G15/20
    • G03G15/2057G03G15/6585G03G2215/0081Y10S428/906Y10T428/3154Y10T428/31544Y10T428/31663
    • Disclosed are fuser members, apparatus and methods which employ compositions that can be varied to provide a fused toner image with a selected gloss level. In embodiments, the apparatus and methods employ a fusing member having an outer contact surface thereon which contacts a previously fused toner image under conditions of elevated temperature and pressure. The contact surface has a Gardner G60 gloss of up to about 35 and is comprised of a fluorocarbon thermoplastic random copolymer co-cured with a fluorinated resin, such as polyfluoroethylenepropylene (FEP). In embodiments, the contact surface comprises a fluorocarbon thermoplastic random copolymer co-cured with a fluorinated resin including subunits of: —(CH2 CF2)x-, —(CF2CF(CF3))y-, and —(CF2 CF2)z-, wherein: x is from 1 to 50 or 60 to 80 mole percent, y is from 10 to 89 mole percent, z is from 10 to 89 mole percent, and x+y+z equals 100 mole percent.
    • 公开了使用可以变化以提供具有所选光泽度的熔融调色剂图像的组合物的定影器构件,设备和方法。 在实施例中,该装置和方法采用其上具有外部接触表面的定影构件,其在升高的温度和压力的条件下接触预先熔化的调色剂图像。 接触表面具有高达约35的Gardner G60光泽度,并且由与氟化树脂(例如聚氟乙烯丙烯(FEP))共固化的碳氟化合物热塑性无规共聚物组成。 在实施方案中,接触表面包括与包含以下子基团的氟化树脂共固化的氟碳热塑性无规共聚物:<?in-line-formula description =“In-line formula”end =“lead”→> - (CH 2 CF 2) x-, - (CF 2 CF(CF 3))y - 和 - (CF 2 CF 2)z - ,<βin-line-formula description =“In-line Formulas”end =“tail”?>其中:x为1 至50或60至80摩尔%,y为10至89摩尔%,z为10至89摩尔%,x + y + z为100摩尔%。