    • Silica aerogel coating and its production method
    • 二氧化硅气凝胶涂料及其制备方法
    • US08298622B2
    • 2012-10-30
    • US11407907
    • 2006-04-21
    • Hiroyuki NakayamaKazuhiro YamadaYasuhiro SakaiMaki Yamada
    • Hiroyuki NakayamaKazuhiro YamadaYasuhiro SakaiMaki Yamada
    • C08F2/48
    • B01J19/123C01B33/1585
    • Methods for producing a silica aerogel coating by: producing a wet gel formed by the hydrolysis and polymerization of an alkoxysilane having an ultraviolet-polymerizable unsaturated group; organically modifying the wet gel with an organic-modifying agent to obtain an organically modified silica having a modification ratio of 10-30% based on a total amount of Si—OH in the wet gel; coating a dispersion of the organically modified silica on a substrate to form a layer; and subjecting the layer of the organically modified silica to ultraviolet irradiation and baking, wherein the silica aerogel coating includes the organically modified silica and wherein the silica aerogel coating has a refractive index in the range of 1.05-1.2.
    • 二氧化硅气凝胶涂层的制造方法:制造通过具有紫外线聚合性不饱和基团的烷氧基硅烷的水解和聚合而形成的湿凝胶; 用有机改性剂有机改性湿凝胶,得到基于湿凝胶中Si-OH总量的改性比为10-30%的有机改性二氧化硅; 将有机改性二氧化硅的分散体涂布在基材上以形成层; 并对有机改性二氧化硅层进行紫外线照射和烘烤,其中二氧化硅气凝胶涂层包括有机改性二氧化硅,其中二氧化硅气凝胶涂层的折射率在1.05-1.2范围内。