    • Layer configuration with improved stability to sunlight exposure
    • 层状结构具有改善的阳光照射的稳定性
    • US07147936B2
    • 2006-12-12
    • US10642933
    • 2003-08-18
    • Frank LouwetGeert Van DyckJohan LoccufierBert GroenendaalHieronymus Andriessen
    • Frank LouwetGeert Van DyckJohan LoccufierBert GroenendaalHieronymus Andriessen
    • C07D211/021H01L51/50
    • C08G61/126C08L25/08C08L2666/06C09J165/00H01G11/48H01G11/56Y02E60/13Y10S428/917
    • A layer configuration on a support, the layer configuration comprising a layer containing a polymer containing optionally substituted 3,4-alkylenedioxythiophene structural units, in which the two alkoxy groups may be the same or different or together represent an optionally substituted oxy-alkylene-oxy bridge, and a compound selected from the group consisting of polyphosphoric acids, polyphosphoric acid salts, thia-alkanedicarboxylic acids, cyclohexadiene compounds and polyhydroxy-compounds selected from the group consisting of tetronic acid derivatives; ortho-dihydroxybenzene compounds with at least one sulpho group, compounds according to formula (I): HO—CH2—CH(OH)—(CH2)m—S—CH2—C(R1)(R2)—CH2—S—(CH2)n—CH(OH)—CH2—OH  (I) wherein R1 and R2 are independently H, —OH or alkyl, and n and m are independently 1, 2 or 3; compounds according to formula (II): HO—(CH2)p—S—CH2—S—(CH2)q—OH  (II) wherein p and q are independently 2, 3 or 4; compounds hydrolyzable to tetronic acid derivatives; compounds hydrolyzable to compounds according to formula (I); and sulpho-substituted 2-thia-alkyl-benzimidazole compounds.
    • 在支撑体上的层构型,该层构型包括含有含有任选取代的3,4-亚烷基二氧噻吩结构单元的聚合物的层,其中两个烷氧基可以相同或不同,或一起代表任选取代的氧基 - 桥,以及选自多磷酸,多磷酸盐,硫杂烷二羧酸,环己二烯化合物和选自由以下组成的组的多羟基化合物的化合物:四氢酸衍生物; 具有至少一个磺酸基的邻二羟基苯化合物,根据式(I)的化合物:<?in-line-formula description =“In-line formula”end =“lead”?> HO-CH 2 -CH(OH) - (CH 2 CH 2)m -S- CH 2 -C(R 1) (R 2) - CH 2 -S-(CH 2)n - (CH 2)n - (CH 2) -CH 2 -O-OH(I)<β在线公式描述=“在线式”末端=“尾”→其中R 1和R 2, SUP> 2独立地是H,-OH或烷基,n和m独立地是1,2或3; 根据式(II)的化合物:<?in-line-formula description =“In-line Formulas”end =“lead”?> HO-(CH 2) > -S-CH 2 -S-(CH 2)2 -O-OH(II)<β在线配方说明书=“ 其中p和q独立地为2,3或4; 可水解成四氢酸衍生物的化合物; 可水解成根据式(I)的化合物的化合物的化合物; 和磺基取代的2-硫代 - 烷基 - 苯并咪唑化合物。
    • 4. 发明申请
    • Process for preparing a substantially transparent conductive layer configuration
    • 制备基本上透明的导电层构型的方法
    • US20050042556A1
    • 2005-02-24
    • US10645160
    • 2003-08-21
    • Frank LouwetTom ClootsHieronymus Andriessen
    • Frank LouwetTom ClootsHieronymus Andriessen
    • H01B1/12H01B1/22H01L51/00H01L51/30H01L51/52H05K3/10G03C1/46
    • H05K3/106H01B1/127H01B1/22H01L51/0021H01L51/0037H01L51/445H01L51/5203H05K2201/0329Y02E10/549
    • A process for preparing a substantially transparent conductive layer configuration on a support, the layer configuration comprising in any order at least a first layer containing an intrinsically conductive polymer optionally containing structural units represented by formula (I): wherein n is larger than 1 and each of R1 and R2 independently represents hydrogen or an optionally substituted C1-4 alkyl group or together represent an optionally substituted C1-4 alkylene group or an optionally substituted cycloalkylene group, preferably an ethylene group, an optionally alkyl-substituted methylene group, an optionally C1-12 alkyl- or phenyl-substituted ethylene group, a 1,3-propylene group or a 1,2-cyclohexylene group; and a second layer consisting of a non-continuous layer of conductive silver, the process comprising the step of: preparing the second layer by a photographic process; and light emitting diodes, photovoltaic devices, transistors and electroluminescent devices comprising a layer configuration prepared according to this process.
    • 一种用于在载体上制备基本上透明的导电层构型的方法,所述层构型至少包含含有本发明的导电聚合物的第一层,所述固有导电聚合物任选含有由式(I)表示的结构单元:其中n大于1, R 1和R 2独立地表示氢或任选取代的C 1-4烷基或一起表示任选取代的C 1-4亚烷基或任选取代的亚环烷基,优选亚乙基,任选烷基取代的 亚甲基,任选的C 1-12烷基或苯基取代的亚乙基,1,3-亚丙基或1,2-亚环己基; 以及由不连续的导电银层组成的第二层,该方法包括以下步骤:通过摄影法制备第二层; 以及发光二极管,光电器件,晶体管和电致发光器件,其包括根据该工艺制备的层构型。
    • 5. 发明授权
    • Process for preparing a substantially transparent conductive layer configuration
    • 制备基本上透明的导电层构型的方法
    • US07026079B2
    • 2006-04-11
    • US10645160
    • 2003-08-21
    • Frank LouwetTom ClootsHieronymus Andriessen
    • Frank LouwetTom ClootsHieronymus Andriessen
    • G03C1/89G03C5/29G03C8/28G03C8/52G03C8/32
    • H05K3/106H01B1/127H01B1/22H01L51/0021H01L51/0037H01L51/445H01L51/5203H05K2201/0329Y02E10/549
    • A process for preparing a substantially transparent conductive layer configuration on a support, the layer configuration comprising in any order at least a first layer containing an intrinsically conductive polymer optionally containing structural units represented by formula (I): wherein n is larger than 1 and each of R1 and R2 independently represents hydrogen or an optionally substituted C1-4 alkyl group or together represent an optionally substituted C1-4 alkylene group or an optionally substituted cycloalkylene group, preferably an ethylene group, an optionally alkyl-substituted methylene group, an optionally C1-12 alkyl- or phenyl-substituted ethylene group, a 1,3-propylene group or a 1,2-cyclohexylene group; and a second layer consisting of a non-continuous layer of conductive silver, the process comprising the step of: preparing the second layer by a photographic process; and light emitting diodes, photovoltaic devices, transistors and electroluminescent devices comprising a layer configuration prepared according to this process.
    • 一种用于在载体上制备基本上透明的导电层构型的方法,所述层构型至少包含含有本发明的导电聚合物的第一层,所述第一层含有任选含有由式(I)表示的结构单元的固有导电聚合物:其中n大于1, R 1和R 2独立地表示氢或任选取代的C 1-4烷基,或者一起表示任选取代的C 1 -C 4烷基, 1-4个亚烷基或任选取代的亚环烷基,优选亚乙基,任选烷基取代的亚甲基,任选的C 1-12烷基或苯基取代的亚乙基 ,1,3-亚丙基或1,2-亚环己基; 以及由不连续的导电银层组成的第二层,该方法包括以下步骤:通过摄影法制备第二层; 以及发光二极管,光电器件,晶体管和电致发光器件,其包括根据该工艺制备的层构型。
    • 6. 发明授权
    • 3,4-alkylenedioxythiophenedioxide compounds and polymers comprising monomeric units thereof
    • 3,4-亚烷基二氧基噻吩二氧化物化合物和包含其单体单元的聚合物
    • US06927298B2
    • 2005-08-09
    • US10649761
    • 2003-08-27
    • Bert GroenendaalFrank LouwetHieronymus Andriessen
    • Bert GroenendaalFrank LouwetHieronymus Andriessen
    • C07D333/36C07D333/64C07D495/02C07D495/04C08G61/12C08G65/34C08G75/00C08G75/32
    • C07D495/04C08G61/126H01G11/48Y02E60/13
    • A 3,4-alkylenedioxythiophenedioxide compound represented by formula (I): in which: A represents a C1-5-alkylene bridge; R represents an optionally substituted C1-24-alkyl, C3-18-cycloalkyl, C1-18-alkoxy or polyethylene oxide group (optionally with at least one substituent selected from the group consisting of an alcohol, amide, ether, ester or sulphonate group) or an optionally substituted aryl group; a polymer comprising monomeric units represented by formula (I); an aqueous dispersion of a polymer comprising monomeric units corresponding to at least one compound according to formula (I) and a polyanion; a chemical polymerization process for preparing the aqueous dispersion comprising the steps of: (i) providing a solution of a polyanion; (ii) adding a compound according to formula (I) and a thiophene or pyrrole compound to the solution provided in step (i); and (iii) adding an oxidizing or reducing system to the mixture provided in step (ii); a printable paste containing the aqueous dispersion; an electroconductive layer containing the polymer; the use of the electroconductive layer in a light emitting diode; an antistatic layer containing the polymer; and an electroconductive pattern and a process for preparing the electroconductive pattern.
    • 由式(I)表示的3,4-亚烷基二氧基噻吩二氧化物化合物:其中:A表示C 1-5烷基亚烷基桥; R代表任选取代的C 1-14 - 烷基,C 3-18 - 环烷基,C 1-18 - 烷氧基或聚环氧乙烷基 (任选地具有至少一个选自醇,酰胺,醚,酯或磺酸酯基的取代基)或任选取代的芳基; 包含由式(I)表示的单体单元的聚合物; 包含对应于至少一种根据式(I)的化合物和聚阴离子的单体单元的聚合物的水分散体; 用于制备水分散体的化学聚合方法,包括以下步骤:(i)提供聚阴离子的溶液; (ii)将式(I)化合物和噻吩或吡咯化合物加入到步骤(i)中提供的溶液中; 和(iii)向步骤(ii)中提供的混合物中加入氧化或还原体系; 含有水分散体的可印刷浆料; 含有聚合物的导电层; 在发光二极管中使用导电层; 含有聚合物的抗静电层; 导电图案和制备导电图案的方法。
    • 9. 发明申请
    • Process for Preparing Electroconductive Coatings
    • US20080017833A1
    • 2008-01-24
    • US11749617
    • 2007-05-16
    • Frank LouwetBert Groenendaal
    • Frank LouwetBert Groenendaal
    • C08K3/00
    • H01B1/127C08G61/126C09D5/24H01G9/028H01G11/48H01G11/56H01L51/0037Y02E60/13
    • An aqueous dispersion of latex particles, said latex particles containing a polymer containing monomer units according to formula (I): in which R1 and R2 independently of one another represent hydrogen or a C1-5-alkyl group or together form an optionally substituted C1-5-alkylene residue and at least one polyanion compound, said latex having a primary particle size of less than 40 nm and said dispersion contains an organic compound containing a di- or polyhydroxy- and/or carboxy groups or amide or lactam group or an aprotic compound with a dielectric constant, ε, ≧15, wherein said latex particles contain said at least one polyanion compound and said polymer in a weight ratio of at least 4; a process for preparing an electroconductive coating comprising the steps of: preparing an aqueous solution or dispersion of the above-mentioned polymer by polymerization with an initiator in a reaction medium in the presence of at least one polyanion compound under oxidizing or reducing conditions, wherein the weight ratio of the at least one polyanion compound to said structural units during the reaction is in the range of 4:1 to 20:1; preparing a first coating composition containing said polymer associated with said at least one polyanion compound and an organic compound containing a di- or polyhydroxy- and/or carboxy groups or amide or lactam group in a aqueous or non-aqueous medium; coating said first coating composition on an object thereby producing a first layer; and heating said first layer at a temperature of at least 100° C.; and a process for preparing an electroconductive coating comprising the steps of: preparing an aqueous solution or dispersion of the above-mentioned polymer by polymerization with an initiator in a reaction medium in the presence of at least one polyanion compound under oxidizing or reducing conditions, wherein the weight ratio of said at least one polyanion compound to said structural units during the reaction is in the range of 4:1 to 20:1; preparing a second coating composition containing said polymer associated with said at least one polyanion compound and an aprotic compound with a dielectric constant, ε, ≧15 in an aqueous or non-aqueous medium; coating said second coating composition on an object thereby producing a second layer; and heating said second layer at a temperature of at least 50° C.
    • 10. 发明授权
    • 3,4-alkylenedioxy-thiophene copolymers
    • 3,4-亚烷基二氧基 - 噻吩共聚物
    • US07105620B2
    • 2006-09-12
    • US10844551
    • 2004-05-12
    • Bert GroenendaalFrank Louwet
    • Bert GroenendaalFrank Louwet
    • C08F234/04C08F28/06C08L45/00C08G61/12
    • C08G61/126C09D165/00H01G11/48H01G11/56Y02E60/13
    • An aqueous dispersion of a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion; a preparation process therefor; its use for coating; a printing ink containing the aqueous dispersion; an electro-conductive layer containing a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion derived from an aqueous dispersion thereof; and an antistatic layer containing a copolymer of at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of less than 2.2 g/L with at least one 3,4-alkylenedioxythiophene compound with a solubility in water at 25° C. of at least 2.2 g/L and a polyanion derived from an aqueous dispersion thereof.
    • 至少一种3,4-二亚烷基二氧噻吩化合物在25℃下在水中的溶解度小于2.2g / L的共聚物的水分散体与至少一种在水中溶解度为25的3,4-亚烷基二氧噻吩化合物 至少2.2g / L的聚阴离子; 其准备过程; 其用于涂料; 含有水分散体的印刷油墨; 含有至少一种在25℃下在水中的溶解度低于2.2g / L的3,4-亚烷基二氧噻吩化合物与至少一种在水中溶解度的3,4-亚烷基二氧噻吩化合物的共聚物的导电层 在25℃下为至少2.2g / L,衍生自其水分散体的聚阴离子; 以及含有至少一种在25℃下在水中的溶解度低于2.2g / L的3,4-亚烷基二氧噻吩化合物与至少一种在水中溶解度的3,4-亚烷基二氧噻吩化合物的共聚物的抗静电层 25℃至少为2.2g / L和衍生自其水分散体的聚阴离子。