    • Process for producing thermoplastic resin composition
    • 热塑性树脂组合物的制造方法
    • US07605208B2
    • 2009-10-20
    • US11589853
    • 2006-10-31
    • Hirotaka UosakiKuniaki KawabeMotoyasu Yasui
    • Hirotaka UosakiKuniaki KawabeMotoyasu Yasui
    • C08J3/22
    • C08J3/005C08J2323/02C08L23/06C08L23/10C08L91/08C08L101/00C08L2314/06C08L2666/06
    • The present invention provides a process for producing a thermoplastic resin composition comprising a polyolefin wax having good dispersibility for a thermoplastic resin, a molded product, which is excellent in physical properties such as blocking property and mechanical properties, from the thermoplastic resin composition and a process for producing the molded product.Specifically, a process for producing a thermoplastic resin composition comprises melt-kneading a mixture of a polyolefin wax (A) which has a passing ratio through a mesh having a sieve opening of 5.66 mmφ of 95% by weight or more, and a non-passing ratio through a mesh having a sieve opening of 2.00 mmφ of 95% by weight or more, and is in the particle form, and a thermoplastic resin (B), a molded product, which is excellent in physical properties such as blocking property and mechanical properties, obtained from the thermoplastic resin composition and a process for producing the molded product are provided.
    • 本发明提供一种热塑性树脂组合物的制造方法,该热塑性树脂组合物包含热塑性树脂具有良好分散性的聚烯烃蜡,热塑性树脂组合物的物理性能如机械性能优异的成型体,以及工序 用于生产模制产品。 具体而言,制造热塑性树脂组合物的方法包括将具有95重量%以上的筛孔5.66mmφ的筛网的通过率的聚烯烃蜡(A)的混合物熔融捏合, 通孔比为2.00mmφ的筛孔为95重量%以上的筛网,为粒状,热塑性树脂(B),成型品,其物理性质如粘合性优异, 提供从热塑性树脂组合物获得的机械性能和制造模塑产品的方法。
    • 4. 发明申请
    • Process for producing thermoplastic resin composition
    • 热塑性树脂组合物的制造方法
    • US20070100055A1
    • 2007-05-03
    • US11589853
    • 2006-10-31
    • Hirotaka UosakiKuniaki KawabeMotoyasu Yasui
    • Hirotaka UosakiKuniaki KawabeMotoyasu Yasui
    • C08L91/08
    • C08J3/005C08J2323/02C08L23/06C08L23/10C08L91/08C08L101/00C08L2314/06C08L2666/06
    • The present invention provides a process for producing a thermoplastic resin composition comprising a polyolefin wax having good dispersibility for a thermoplastic resin, a molded product, which is excellent in physical properties such as blocking property and mechanical properties, from the thermoplastic resin composition and a process for producing the molded product. Specifically, a process for producing a thermoplastic resin composition comprises melt-kneading a mixture of a polyolefin wax (A) which has a passing ratio through a mesh having a sieve opening of 5.66 mmφ of 95% by weight or more, and a non-passing ratio through a mesh having a sieve opening of 2.00 mmφ of 95% by weight or more, and is in the particle form, and a thermoplastic resin (B), a molded product, which is excellent in physical properties such as blocking property and mechanical properties, obtained from the thermoplastic resin composition and a process for producing the molded product are provided.
    • 本发明提供一种热塑性树脂组合物的制造方法,该热塑性树脂组合物包含热塑性树脂具有良好分散性的聚烯烃蜡,热塑性树脂组合物的物理性能如机械性能优异的成型体,以及工序 用于生产模制产品。 具体而言,制造热塑性树脂组合物的方法包括将具有95重量%以上的筛孔5.66mmφ的筛网的通过率的聚烯烃蜡(A)的混合物熔融捏合, 通孔比为2.00mmφ的筛孔为95重量%以上的筛网,为粒状,热塑性树脂(B),成型品,其物理性质如粘合性优异, 提供从热塑性树脂组合物获得的机械性能和制造模塑产品的方法。
    • 8. 发明申请
    • Process for producing injection molded product
    • 注塑产品生产工艺
    • US20070080483A1
    • 2007-04-12
    • US11543901
    • 2006-10-06
    • Hirotaka UosakiKuniaki KawabeMotoyasu Yasui
    • Hirotaka UosakiKuniaki KawabeMotoyasu Yasui
    • B29C45/00C08L91/08C08J3/22C08K5/01
    • B29C45/0001B29K2105/0094C08K5/01C08L23/02C08L23/06C08L23/10C08L23/16C08L91/06C08L91/08C08L2205/03C08L2666/04C08L2666/06C08L2666/02
    • The present invention provides an injection molding process of a thermoplastic resin which is capable of thin molding or precision molding by improving injection moldability, particularly releasability or fluidity, without deteriorating the characteristics of the injection molded article of the thermoplastic resin. The process for producing an injection molded product comprises injection molding a mixture containing a thermoplastic resin and a polyolefin wax, wherein the mixture has L/L0≧1.05, the L being a flow length in the case where the mixture contains the polyolefin wax and the Lo being a flow length in the case where the mixture contains no polyolefin wax, the L and L0 being measured under the conditions of a mold temperature of 40° C. and a resin temperature, Tr, as determined by the following equation: Tr=¾×Tm+100(wherein Tm represents a melting temperature (° C.) of the thermoplastic resin), using a spiral flow mold having a thickness of 1 mm and a width of 10 mm.
    • 本发明提供一种热塑性树脂的注射成型方法,其能够通过提高注射成型性,特别是脱模性或流动性而能够进行薄型化或精密成型,而不会降低热塑性树脂的注塑制品的特性。 制造注射成型制品的方法包括注射模塑含有热塑性树脂和聚烯烃蜡的混合物,其中混合物的L / L <0.01 / L = 1.05,L是在该情况下的流动长度 其中混合物包含聚烯烃蜡,并且在混合物不含聚烯烃蜡的情况下Lo为流动长度,在模具温度为40℃的条件下测量L和L 0 和树脂温度Tr,由以下等式确定:<?in-line-formula description =“In-line Formulas”end =“lead”?> Tr =¾xTm+ 100 <?in-line-formula description (“In-line Formulas”end =“tail”?>(其中Tm表示热塑性树脂的熔融温度(℃)),使用厚度为1mm,宽度为10mm的螺旋流动模具。