    • 4. 发明授权
    • Polyester films for magnetic recording medium
    • 用于磁记录介质的聚酯薄膜
    • US5328745A
    • 1994-07-12
    • US996172
    • 1992-12-23
    • Hideshi KuriharaMasahito SatohTsuyoshi NagaiSadayoshi MiuraToshifumi Osawa
    • Hideshi KuriharaMasahito SatohTsuyoshi NagaiSadayoshi MiuraToshifumi Osawa
    • C08J7/04G11B5/73G11B5/733G11B5/64B32B5/16G11B5/704
    • C08J7/047G11B5/733C08J2367/02Y10S428/90Y10S428/91Y10T428/24355Y10T428/24372Y10T428/25Y10T428/3179Y10T428/31794Y10T428/31797
    • There is provided a polyester film useful for production of a magnetic recording medium excellent in runnability, electromagnetic conversion characteristics and storage stability. In the polyester film, a continuous thin film which contains a resin as a matrix and acts as a primer layer for a magnetic layer is coated on one surface of a support film composed of a polyester. According to one embodiment thereof, the surface of the continuous thin film has (A) small protuberances each containing particles with an average particle size of less than 0.06 micrometer as a nucleus and having a height of 13 nm or less, (B) large protuberances each containing particles with an average particle size of 0.06 micrometer or more as a nucleus and having a height of 30 nm or less, and (C) micro-protuberances composed of a matrix resin alone, the numbers, per mm.sup.2 of the film, of these protuberances satisfying the formulas,An=1.0.times.10.sup.4 -1.0.times.10.sup.8 /mm.sup.2,Bn=0-4.times.10.sup.4 /mm.sup.2, andCn.ltoreq.4.0 .times.10.sup.6 /mm.sup.2wherein An is the number of the small protuberances, Bn is the number of the large protuberances, and Cn is the number of the micro-protuberances,the fine surface roughness Ra.sup.s of the continuous thin film portion composed of the matrix resin alone being 1.10 nm or less, and the surface roughness Ra of the overall continuous thin film being 1 to 10 nm.
    • 提供了可用于制造运行性,电磁转换特性和储存稳定性优异的磁记录介质的聚酯膜。 在聚酯薄膜中,将包含树脂作为基体并用作磁性层底漆层的连续薄膜涂覆在由聚酯构成的支撑薄膜的一个表面上。 根据其一个实施方案,连续薄膜的表面具有(A)小的突起,每个小突起均含有平均粒径小于0.06微米的颗粒,高度为13nm或更小,(B)大的突起 各自含有平均粒径为0.06微米以上且具有30nm以下的高度的粒子,(C)由单独的基质树脂构成的微突起,每mm2的数量为 这些突起满足公式An = 1.0×104-1.0×108 / mm2,Bn = 0-4×104 / mm2,Cn <= 4.0×106 / mm2其中An为小突起数,Bn为大数 突起和Cn是微突起的数量,由基体树脂单独构成的连续薄膜部分的细小表面粗糙度Ras为1.10nm以下,整个连续薄膜的表面粗糙度Ra为1〜 10 nm。