    • 1. 发明授权
    • Process for production of low phosphorus alloy
    • 低磷合金生产工艺
    • US4522650A
    • 1985-06-11
    • US537025
    • 1983-09-29
    • Hidemasa NakajimaShozo OkamuraMasanobu SueyasuSakae FurujhoKohji OkaneShoji Anezaki
    • Hidemasa NakajimaShozo OkamuraMasanobu SueyasuSakae FurujhoKohji OkaneShoji Anezaki
    • C21B13/00C21C5/28C21C5/35C21C7/00
    • C21B13/0013C21C5/28C21C5/35Y02P10/136
    • Herein is disclosed a process for producing an alloy of low phosphorus content by means of a furnace equipped with a lance for injection. The process is characterized by producing an alloy of low phosphorus content and at the same time by gasifying the carbonaceous material.The process comprises the steps of:forming a bath of molten metal by pouring a molten metal in the furnace, said molten metal containing not more than 0.040% of phosphorus;injecting by means of said lance into said bath of molten metal a carbonaceous material together with a gasifying agent to gasify the carbonaceous material with the heat of the bath of molten metal and to increase the carbon content of the bath of molten metal, said carbonaceous material containing not more than 0.035% of phosphorus;adding to said bath of molten metal an alloying element to react with the molten metal thereby forming an alloy; andrecovering the formed gas and, at the same time, obtaining the alloy of low phosphorus content.The process is suitable for producing Cr steel, Mn steel and Ni steel.
    • 本文公开了一种通过装备有注射用喷枪的炉来制造低磷含量的合金的方法。 该方法的特征在于生产低磷含量的合金,同时通过气化碳质材料。 该方法包括以下步骤:通过将熔融金属倒入炉中而形成熔融金属浴,所述熔融金属含有不超过0.040%的磷; 通过所述喷枪将所述喷枪喷射到所述熔融金属浴中,将碳质材料与气化剂一起用熔融金属浴的热量气化碳质材料并增加熔融金属浴的碳含量,所述碳质材料 含磷不超过0.035% 向所述熔融金属浴中加入合金元素以与熔融金属反应从而形成合金; 并回收形成的气体,同时获得低磷含量的合金。 该工艺适用于生产Cr钢,Mn钢和Ni钢。