    • 2. 发明申请
    • Process of Manufacturing Antimicrobial Fabrics
    • 制造抗菌织物的工艺
    • US20170013844A1
    • 2017-01-19
    • US14801909
    • 2015-07-17
    • GRAND TEXTILE CO., LTD.
    • Jen-Huan Lu
    • A01N65/08A01N65/22A01N25/34A01N65/32A01N65/20A01N65/30A01N25/12A01N65/40
    • A01N65/08A01N65/20A01N65/22A01N65/30A01N65/32A01N65/40A01N25/12
    • A process of manufacturing antimicrobial fabrics includes drying Rheum rhabarbarum, Sophora flavescens var. Flavescens, Forsythia suspensa, Coptis chinensis Franch, Rehmannia glutinosa, Anemarrhena asphodeloides, and Scutellaria lateriflora at 50° C. for about 6 to 12 hours, and grinding same to nanoscale powders; adding the nanoscale powders to a solution containing 95% by volume of ethanol, heating the solution at 50° C., and extracting the ethanol; adding water to the container after extracting for two hours, thereby obtaining a solution containing antimicrobial herbal medicinal components; adding about 1 to 3 wt % of Sodium dodecyl sulfate to the solution containing antimicrobial herbal medicinal components for emulsification; adding about 5 wt % of acrylic resin to the emulsified solution to form Liposomes containing the nano powder; adding the Liposomes to foam resin to form a mixture; and applying the mixture to fabrics to manufacture antimicrobial fabrics containing herbal medicinal components.
    • 制造抗微生物织物的方法包括干燥Rheum rhabarbarum,Sophora flavescens var。 黄连,连翘,中华黄连,地黄,白芷,芦荟和黄芩在50℃下培养约6〜12小时,并研磨成纳米级粉末; 将纳米级粉末加入到含有95体积%乙醇的溶液中,在50℃下加热溶液,并萃取乙醇; 提取2小时后,向容器中加水,得到含抗菌草药成分的溶液; 向含有抗微生物草药成分的溶液中加入约1〜3重量%的十二烷基硫酸钠进行乳化; 向乳化溶液中加入约5重量%的丙烯酸树脂以形成含有纳米粉末的脂质体; 将脂质体加入泡沫树脂中以形成混合物; 并将混合物施加到织物上以制造含有中草药组分的抗微生物织物。
    • 8. 发明申请
    • Method of Manufacturing Fabric with Cool Effect
    • 制造具有酷效果的面料的方法
    • US20140057049A1
    • 2014-02-27
    • US14071868
    • 2013-11-05
    • Grand Textile Co., Ltd.
    • Jen-Huan Lu
    • D06C7/02
    • D06C7/02D06M11/44D06M11/79D06M15/263D06M15/564D06M23/04D06N3/0047D06N3/005D06N3/0063D06N3/14D06N2209/123
    • A method of manufacturing fabric is provided with adding 900 g of a material having a 92 wt % of SiO2, 5 wt % of ZnO, and 3 wt % of polypropylene acid sodium and 1,500 g of PU resin to water to mix until a first solution is formed; pouring the first solution into a first foaming tank; agitating the first solution in the first foaming tank to foam; adding a bridging agent and a foaming agent to a second foaming tank to mix with water to foam until a second solution is formed; pouring the first and second solutions into a third tank to mix and form a coating solution; continuously conveying a fabric sheet to a top of a platform; activating squeegees to spread the coating solution on the fabric sheet to form a cooling layer thereon; and performing a dry setting finish on the fabric sheet.
    • 提供一种制造织物的方法,向水中加入900g具有92重量%SiO 2,5重量%ZnO和3重量%聚丙烯酸钠和1,500g PU树脂的材料,以混合直到第一溶液 形成了; 将第一溶液倒入第一发泡罐中; 搅拌第一泡沫罐中的第一溶液以发泡; 向第二发泡罐中加入桥联剂和发泡剂以与水混合以发泡直到形成第二溶液; 将第一和第二溶液倒入第三罐中以混合并形成涂布溶液; 将织物片连续输送到平台的顶部; 激活刮板以将涂布溶液铺展在织物片上以在其上形成冷却层; 并在织物片上进行干燥设定。