    • 2. 发明授权
    • Apparatus for improving the degree of graphitization of carbon black,
and its use
    • 用于提高炭黑石墨化程度的设备及其用途
    • US4601887A
    • 1986-07-22
    • US428947
    • 1982-09-30
    • Friedrich-Wilhelm DornManfred WolterGero Heymer
    • Friedrich-Wilhelm DornManfred WolterGero Heymer
    • C09C1/00C09C1/56F27B9/06C01B31/04C09C1/46
    • C09C1/56C01P2006/12
    • The invention relates to improving the degree of graphitization of carbon black produced by subjecting hydrocarbons which are liquid or gaseous under normal conditions to a thermal conversion reaction in the presence of oxygen or an oxygen-containing gas and steam, if desired, at temperatures of 1200.degree. to 2000.degree. C. and pressures of 1 to 80 bars. To this end, the carbon black is conveyed downwardly in a quasi-fluid state, within 1 to 5 hours through a sojourn zone in upright position, the sojourn zone being maintained at a temperature of at least 1200.degree. C.The invention relates to an apparatus for carrying out this process, the apparatus comprising a graphite tube; a steel container concentrically surrounding the graphite tube; a feed pipe penetrating into the interior of the graphite tube; a water-cooled discharge means; and a nitrogen feed inlet arranged below the lower end of the graphite tube; the space left between the graphite tube and steel container being occupied by insulating material.
    • 本发明涉及通过在氧气或含氧气体和蒸汽的存在下,在正常条件下对液态或气态烃进行热转化反应,如果需要,在1200℃的温度下,提高炭黑的石墨化程度 DEG至2000℃,压力为1至80巴。 为此,炭黑在准流体状态下通过直立位置的居住区域在1至5小时内向下输送,住宅区域保持在至少1200℃的温度。本发明涉及一种 用于执行该处理的装置,该装置包括石墨管; 围绕石墨管的钢制容器; 进料管穿入石墨管的内部; 水冷式排放装置; 以及配置在所述石墨管的下端下方的氮气进料口; 石墨管和钢容器之间留下的空间被绝缘材料占据。
    • 4. 发明授权
    • Process and apparatus for making phosphorus pentoxide with utilization
of reaction heat
    • 利用反应热制造五氧化二磷的工艺和装置
    • US4525329A
    • 1985-06-25
    • US601027
    • 1984-04-16
    • Bernhard KuxdorfPeter LuhrHugo WernerUrsus ThummlerFriedrich-Wilhelm Dorn
    • Bernhard KuxdorfPeter LuhrHugo WernerUrsus ThummlerFriedrich-Wilhelm Dorn
    • B01J19/00C01B25/12
    • C01B25/12B01J19/0013B01J2219/00094
    • The disclosure relates to a process for making phosphorus pentoxide by subjecting elemental yellow phosphorus to combustion with dried air inside a steel-made combustion chamber with utilization of the reaction heat for the production of energy. To this end, the disclosure provides for the combustion to be effected inside a combustion chamber of which the walls are arranged so as to form a cooling system with cavities therein; for a liquid or liquid/steam-mixture as a heat carrier abstracting the reaction heat to be circulated through the cooling system, the liquid or liquid/steam-mixture assuming an increased temperature being preferably so circulated under increased pressure; for steam formed in the cooling system to be continuously taken therefrom; for an equivalent proportion of fresh liquid to be introduced into the cooling system; for hot P.sub.2 O.sub.5 issuing in vapor form from the combustion chamber to be condensed or worked up into desirable final product, the combustion chamber being a cylindrical vessel with a height/diameter-ratio of 2.5:1 to 5:1 and having 1 to 10 burners disposed axisymmetrically in its circular base plate.The disclosure also relates to an apparatus for carrying out the process.
    • 本公开内容涉及通过利用反应热用于生产能量的方法,通过使元素黄磷与干燥的空气在钢制燃烧室内燃烧来制备五氧化二磷的方法。 为此,本公开提供了在燃烧室内进行燃烧,其中壁的布置以便形成其中具有空腔的冷却系统; 对于作为热载体的液体或液体/蒸汽混合物,其提取要循环通过冷却系统的反应热,假设温度升高的液体或液体/蒸汽混合物优选在增加的压力下循环; 对于在冷却系统中形成的蒸汽连续从其中取出; 将相当比例的新鲜液体引入冷却系统; 对于来自燃烧室的蒸汽形式的热P2O5将被冷凝或加工成所需的最终产品,燃烧室是高度/直径比为2.5:1至5:1的圆柱形容器,并具有1至10个燃烧器 在其圆形基板中轴对称设置。 本公开还涉及一种用于执行该过程的装置。
    • 5. 发明授权
    • Process for producing aluminum nitride
    • 生产氮化铝的方法
    • US5221527A
    • 1993-06-22
    • US715489
    • 1991-06-14
    • Friedrich-Wilhelm DornHeinz Zschach
    • Friedrich-Wilhelm DornHeinz Zschach
    • C01B21/072
    • C01B21/0726C01P2004/51C01P2004/61C01P2006/12
    • For producing finely disperse aluminum nitride by reacting hydroxides of aluminum with carbon in a molar ratio of (1:1.5) to (1:2.5), the hydroxides of aluminum are intensively ground together with carbon, in particular carbon black, using a non-aqueous grinding fluid. After the non-aqueous grinding fluid has been separated off from the suspension, the ground material obtained is calcined at 400.degree. to 1000.degree. C., while passing nitrogen through. The material obtained is then treated under intensive contact with nitrogen for 1 to 100 hours at 1400.degree. to 1700.degree. C., before the excess carbon contained in the reaction product is removed by heating to 500.degree. to 900.degree. C. in contact with oxygen-containing gases.The hydroxides of aluminum and the carbon can also be intensively ground separately from one another, using a non-aqueous grinding fluid, and the suspensions obtained can be mixed.
    • 为了通过使铝的氢氧化物与摩尔比为(1:1.5)至(1:2.5)的碳反应来生产精细分散的氮化铝,铝的氢氧化物与碳(特别是炭黑)一起用非 - 水性研磨液。 将非水性研磨液与悬浮液分离后,将得到的研磨材料在400〜1000℃下煅烧,同时通过氮气。 然后将得到的材料在1400℃至1700℃下与氮气密切接触处理1至100小时,然后通过加热至与氧接触的500℃至900℃除去反应产物中所含的过量碳。 含气体。 铝和碳的氢氧化物也可以使用非水性研磨液彼此分开地集中研磨,并且可以混合获得的悬浮液。