    • 1. 发明申请
    • Aqueous Self-Adhesive Coating for Electrical Steel and its Uses
    • 电工钢水性自粘涂层及其用途
    • US20070231463A1
    • 2007-10-04
    • US11587733
    • 2005-04-27
    • Changguo HuangFeng YuXiao ChenZhigang YuZhuolei ChenMeiping Zou
    • Changguo HuangFeng YuXiao ChenZhigang YuZhuolei ChenMeiping Zou
    • C09D163/00C09J169/00
    • C09D163/00C08G59/4021C08G59/686C08L2666/04
    • The present invention relates to a self-adhesive coating for electrical steel and its uses. The coating comprises 81-99.9 weight parts of aqueous epoxy resin emulsion, 0.07-17 weight parts of curing agent, and optionally 0.3 weight parts of accelerant. If required, said coating can optionally contain additives selected from diluent, filler, toughener, colorant, fire retardant, antirusting agent, antisettling agent, thixotropic agent or antifoamer, thickener, pigment dispersant, preservative, and the like. The coating can be used as electrical steel coating. The present coating is capable of making electrical steel with a self-adhesive coating in a way of heat by naked-flame, and also there are no poisonous organic solvents to volatilize during the entire process. Furthermore, the coating permits to omit apparatus for burning organic solvents, and the cost is thereby reduced.
    • 本发明涉及电工钢的自粘涂层及其用途。 涂层包含81-99.9重量份的水性环氧树脂乳液,0.07-17重量份的固化剂和任选的0.3重量份的促进剂。 如果需要,所述涂层可以任选地含有选自稀释剂,填料,增韧剂,着色剂,阻燃剂,防锈剂,抗沉降剂,触变剂或消泡剂,增稠剂,颜料分散剂,防腐剂等的添加剂。 涂层可用作电工钢涂层。 本涂料能够通过裸火焰以热粘合的方式制造具有自粘性涂层的电工钢,并且在整个过程中也没有有毒的有机溶剂挥发。 此外,涂层允许省略用于燃烧有机溶剂的设备,从而降低了成本。
    • 3. 发明申请
    • NON-ORIENTED ELECTRICAL STEEL PLATE WITHOUT CORRUGATED FAULT AND PRODUCTION METHOD THEREOF
    • 不具有纠正故障的非电导型钢板及其制造方法
    • US20130224064A1
    • 2013-08-29
    • US13823311
    • 2011-04-14
    • Feng ZhangXiao ChenWei CaoYezhong SunChangsong MaJianru ZhuZhuolei ChenXiandong Liu
    • Feng ZhangXiao ChenWei CaoYezhong SunChangsong MaJianru ZhuZhuolei ChenXiandong Liu
    • B22D25/00C22C38/00C22C38/02C22C38/06C22C38/04
    • B22D25/00B22D11/182B22D11/225C21D6/008C21D8/12C21D8/1205C21D8/1222C21D8/1233C21D8/1272C21D8/1277C21D2201/05C22C38/001C22C38/002C22C38/004C22C38/02C22C38/04C22C38/06H01F1/16
    • A non-oriented electrical steel sheet without corrugated defect and a manufacturing method thereof is provided, the weight percentage of the chemical composition of the non-oriented electrical steel sheet is that C is no more than 0.005%, Si is 1.2-2.2%, Mn is 0.2-0.4%, P is no more than 0.2%, S is no more than 0.005%, Al is 0.2-0.6%, N is no more than 0.005%, O is no more than 0.005%, and a balance substantially being Fe, a slab can be obtained by hot metal preprocessing, smelting with converter, RH refining, and continuous casting and pouring, wherein a secondary cooling water amount is controlled, the water flowrate of cooling water is controlled to 100-190 l/min, the average superheat of liquid steel in the continuous casting process is controlled to 10-45° C., the slab is heated and hot rolled; wherein the furnace tap temperature of the slab is 1050-1150 ° C., the temperature difference between random two points in the length direction when the slab is heated, is lower than 25° C., the hot rolling process includes a rough rolling process and a planishing process, the entry temperature in the planishing process is no lower than 970° C.; the finished non-oriented electrical steel sheet is obtained by acid pickling, cold rolling, annealing and coating. No corrugated defect can be accomplished by controlling the cooling speed of the slab in continuous casting and pouring process, the temperature difference in the length direction of the slab in the heating furnace, and by controlling the temperature drop before planishing the slab.
    • 本发明提供一种无波纹状缺陷的无取向电工钢板及其制造方法,其中,所述无方向性电工钢板的化学成分的重量百分比为C为0.005%以下,Si为1.2〜2.2% Mn为0.2〜0.4%,P为0.2%以下,S为0.005%以下,Al为0.2〜0.6%,N为0.005%以下,O为0.005以下,余量基本上为 是Fe,可以通过热金属预处理,转炉熔炼,RH精炼以及连续铸造和浇注获得板坯,其中控制二次冷却水量,将冷却水的水流量控制在100-190l / min ,连铸过程中液态钢的平均过热度控制在10-45℃,将板坯加热和热轧; 其特征在于,板坯的炉膛温度为1050〜1150℃,板坯加热时长度方向随机两点之间的温差低于25℃,热轧工序包括粗轧工序 和平整过程中,平整过程中的入口温度不低于970℃; 通过酸洗,冷轧,退火和涂布获得成品的无取向电工钢板。 通过在连续铸造和浇注过程中控制板坯的冷却速度,加热炉中板坯的长度方向的温差,以及通过控制板坯平整之前的温度下降来控制温度下降,可以不产生瓦楞缺陷。
    • 10. 发明申请
    • COLD ROLLED ELECTROMAGNETIC STEEL SHEET USED FOR RAPID CYCLING SYNCHROTRON AND PRODUCING METHOD THEREOF
    • 用于快速循环同步电动机的冷轧电磁钢板及其制造方法
    • US20120318411A1
    • 2012-12-20
    • US13520405
    • 2011-04-13
    • Lingfeng ChenXiao ChenZhanyuan Hu
    • Lingfeng ChenXiao ChenZhanyuan Hu
    • C21D8/12H01F1/01
    • C21D8/1233C21D8/12C22C38/001C22C38/002C22C38/004C22C38/02C22C38/04C22C38/06
    • A cold rolled electromagnetic steel sheet for rapid cycling synchrotron, and a manufacturing method thereof, the method includes the steps of 1) smelting and casting, the composition of the cold rolled electromagnetic steel sheet is C 0.001-0.003 wt %, Si 0.60%-0.90 wt %, Mn 0.40%-0.70 wt %, P≦0.04 wt %, Al 0.60-0.80 wt %, S≦0.0035 wt %, N≦0.003 wt %, and the rest is Fe; smelting and RH refining, and then casting to form semi-finished product; 2) hot rolling; 3) normalizing, in which the normalizing temperature is controlled between 960° C.-980° C., and the normalizing time is 30-60 sec; 4) pickling and cold rolling; 5) annealing, wherein the annealing temperature is controlled to be between 850° C.-870° C., and the annealing time is 13-15 sec; 6) obtaining non-oriented silicon steel product after coating. The cold rolled electromagnetic steel sheet of the present invention has low coercivity, specifically in case that the magnetizing intense returns to zero after reaching 10 Oersted (Oe), the coercivity of the material is Hc≦79.6 A/m; high magnetic induction, which is B50≧1.75 T; and low iron losses of P15/50≦4.2 W/kg, and the iron losses after strain-annealing is P15/50≦3.5 W/kg.
    • 一种用于快速循环同步加速器的冷轧电磁钢板及其制造方法,其特征在于,包括以下步骤:1)熔融铸造,冷轧电磁钢板的组成为0.001-0.003重量%,Si 0.60〜 0.90重量%,Mn 0.40重量%-0.70重量%,P< L; 0.04重量%,Al 0.60-0.80重量%,S& NEE; 0.0035重量%,N< 1E; 0.003重量%,其余为Fe; 冶炼和RH精炼,然后铸造形成半成品; 2)热轧; 3)归一化,其中归一化温度控制在960℃-980℃之间,标准化时间为30-60秒; 4)酸洗和冷轧; 5)退火,其中退火温度控制在850℃-870℃之间,退火时间为13-15秒; 6)涂布后获得无取向硅钢产品。 本发明的冷轧电磁钢板具有低的矫顽力,特别是在达到10奥斯特(Oe)后,磁化强度恢复到零的情况下,材料的矫顽力为Hc≦̸ 79.6A / m; 高磁感应,B50≥1.5T; P15 / 50&NlE低铁损; 4.2W / kg,应变退火后的铁损为P15 / 50≦̸ 3.5W / kg。