    • 1. 发明授权
    • Flash roasting of molybdenum sulfide concentrates in a slagging reactor
    • 将硫化钼精矿在造渣反应器中进行快速焙烧
    • US4555387A
    • 1985-11-26
    • US583905
    • 1984-02-27
    • Bruce J. SabackyMalcolm T. Hepworth
    • Bruce J. SabackyMalcolm T. Hepworth
    • C01G39/02C22B1/02C22B34/34
    • C01G39/02C22B1/02C22B34/34
    • A process and system are provided for flash-roasting molybdenum sulfide containing slag-forming constituents. The process comprises feeding a pneumatically suspended stream of particulate molybdenum sulfide and a mixture of fuel and oxidizing gases through a nozzle into a confined furnace chamber, the fuel gas-oxidizing gas mixture exiting from the nozzle being ignited to provide a flame thereof, the flame being maintained at a condition to provide a temperature in the furnace chamber sufficient to oxidize the molybdenum sulfide and form a volatile gas comprising molybdenum trioxide. The temperature is at least sufficient to melt the slag-forming constituents such that the slag formed is sufficiently liquid to separate from the gaseous mixture and collect at a selected portion of said chamber for removal therefrom. The resulting gases in the volatile molybdenum trioxide are caused to flow from the furnace chamber to and through a condensing chamber, the temperature of the condensing chamber being controlled to condense the volatilized molybdenum trioxide and separate it from the off-gases.
    • 提供了一种快速焙烧含硫化钼的成渣成分的方法和系统。 该方法包括将气体悬浮的颗粒状硫化钼料流和燃料和氧化气体的混合物通过喷嘴进入限制炉室,从喷嘴排出的燃料气体 - 氧化气体混合物被点燃以提供其火焰,火焰 保持在炉室中提供足以氧化硫化钼并形成包含三氧化钼的挥发性气体的温度的条件。 温度至少足以熔化形成成渣的成分,使得形成的炉渣充分地液体以与气体混合物分离并收集在所述室的选定部分以从中除去。 使挥发性三氧化钼中的所得气体从炉室流出并通过冷凝室,冷凝室的温度被控制以冷凝挥发的三氧化钼并将其与废气分离。
    • 2. 发明授权
    • Flash sublimation and purification of molybdenum oxide
    • 闪蒸升华和纯化氧化钼
    • US4551313A
    • 1985-11-05
    • US583566
    • 1984-02-27
    • Bruce J. SabackyMalcolm T. Hepworth
    • Bruce J. SabackyMalcolm T. Hepworth
    • C01G39/02C22B34/34
    • C22B34/34C01G39/02C01P2006/80
    • A process and system are provided for flash-sublimation of molybdic oxide containing slag-forming constituents. The process comprises feeding a pneumatically suspended stream of particulate molybdic oxide and a mixture of fuel and oxidizing gases through a nozzle into a confined furnace chamber, the fuel gas-oxidizing gas mixture exiting from the nozzle being ignited to provide a flame thereof, the flame being maintained at a condition to provide a temperature in the furnace chamber in excess of that required to sublime molybdic oxide. The temperature is preferably at least sufficient to melt slag-forming constituents contained in said molybdic oxide such that the slag formed is sufficiently liquid to separate from the gaseous mixture and collect at a selected portion of the chamber for removal therefrom. The resulting gases and suspended solids including sublimed molybdenum trioxide are caused to flow from said furnace chamber to and through a condensing chamber, the temperature of the condensing chamber being controlled to above the condensing temperature of the sublimed molybdenum trioxide but below the volatilization temperature of the impurities present and thereby effect a separation of the molybdenum trioxide from the impurities. The separated molybdenum trioxide vapors are then passed to a condenser to condense and recover the molybdenum trioxide as solids and separate it from off-gases.
    • 提供了一种用于使含有氧化钼的成矿成分组分快速升华的方法和系统。 该方法包括将气体悬浮的颗粒状氧化钼和燃料和氧化气体的混合物通过喷嘴供入到限定的炉室中,从喷嘴排出的燃料气体 - 氧化气体混合物被点燃以提供其火焰,火焰 保持在炉室中提供超过使氧化钼氧化所需温度超过的温度的条件。 该温度优选至少足以熔化所述氧化钼中所含的成渣成分,使得形成的炉渣充分地液体以与气体混合物分离并收集在室的选定部分以从中除去。 使所产生的气体和包括升华的三氧化钼的悬浮固体从所述炉室流出并通过冷凝室,冷凝室的温度被控制在高于升华的三氧化钼的冷凝温度但低于 存在杂质,从而使三氧化钼与杂质分离。 然后将分离的三氧化钼蒸气通入冷凝器以冷凝和回收作为固体的三氧化钼,并将其与废气分离。
    • 4. 发明授权
    • Membrane process for separating contaminant anions from aqueous
solutions of valuable metal anions
    • 从有价值金属阴离子的水溶液中分离污染物阴离子的膜工艺
    • US4234393A
    • 1980-11-18
    • US31325
    • 1979-04-18
    • Malcolm T. HepworthJohn M. Laferty
    • Malcolm T. HepworthJohn M. Laferty
    • C25B15/08C25C1/22
    • C25C1/22C25B15/08
    • An aqueous solution of at least one valuable oxyanion containing molybdenum, tungsten, vanadium, or uranium is refined to lower the content of contaminant anions such as PO.sub.4.sup.-3, SO.sub.4.sup.-2, NO.sub.3.sup.-, Cl.sup.-, ClO.sub.3.sup.-, and ClO.sub.4.sup.-, by subjecting the solution to electrolysis at a pH of from 0.5 to 4.0 between a cation-permselective membrane and an anion-permselective membrane having tertiary amine or quaternary ammonium anion exchange groups, to cause contaminant anions to pass from the solution into the anolyte. Ammonium molybdates, tungstates, vanadates, and uranates are formed from the thus-refined solution by subjecting it to a second stage of electrolysis at a pH of at least 7 between a cation-permselective membrane and an anion-permselective membrane to cause valuable oxyanions to pass from the solution into an anolyte which comprises an aqueous solution of ammonia and to form the desired ammonium compound.
    • 精制含有钼,钨,钒或铀的至少一种有价值的含氧阴离子的水溶液以降低污染物阴离子如PO4-3,SO4-2,NO3-,Cl-,ClO3-和ClO4-的含量, 通过在阳离子 - 选择性选择性膜和具有叔胺或季铵阴离子交换基团的阴离子 - 选择性选择性膜之间,使pH为0.5〜4.0的溶液进行电解,使污染物阴离子从溶液中通入阳极电解液。 钼酸铵,钨酸盐,钒酸盐和铀酸盐由如此精制的溶液通过在阳离子 - 选择性渗透膜和阴离子 - 选择性选择性膜之间经受至少7的pH的第二阶段的电解而形成,以引起有价值的含氧阴离子 从溶液中通入包含氨水溶液并形成所需铵化合物的阳极电解液。
    • 6. 发明授权
    • Coal combustion to produce clean low-sulfur exhaust gas
    • 煤燃烧产生清洁的低硫废气
    • US4598652A
    • 1986-07-08
    • US772524
    • 1985-09-04
    • Malcolm T. Hepworth
    • Malcolm T. Hepworth
    • F23C3/00F23D1/02F23J11/00F23J15/00
    • F23C3/008F23D1/02
    • A process is provided for combusting sulfur-containing coal in a combustion stage to which is provided at least 60% of the oxygen stoichiometrically required for substantially complete combustion of the coal and combustion is conducted under highly turbulent conditions in a furnace burner cavity to which finely divided iron oxide and/or iron powder is provided and in which a high heat release rate is maintained to form a liquid iron oxysulfide phase which acts to scrub sulfur-containing gaseous species from the combustion atmosphere and is separated from the combustion atmosphere with substantially the sulfur originally contained in the coal. Following separation, the hot fuel gas resulting is burned to completion in a heat exchanging furnace, gas turbine or other energy extracting device.
    • 提供了一种在燃烧阶段中燃烧含硫煤的方法,其中提供了煤的基本完全燃烧所需的化学计量的至少60%的氧气,并且燃烧在高度湍流条件下在炉燃烧器空腔中进行,其中精细地 提供了分开的氧化铁和/或铁粉,并且其中保持高的热释放速率以形成液氧铁硫氧化物相,其用于从燃烧气氛中洗涤含硫气体物质,并从燃烧气氛与基本上 硫原来含在煤中。 在分离之后,所产生的热燃料气体在热交换炉,燃气轮机或其他能量提取装置中燃烧完成。
    • 10. 发明授权
    • Coal combustion to produce clean low-sulfur exhaust gas
    • 煤燃烧产生清洁的低硫废气
    • US4572085A
    • 1986-02-25
    • US698705
    • 1985-02-06
    • Malcolm T. Hepworth
    • Malcolm T. Hepworth
    • C10L9/10F23C3/00F23J7/00F23J11/00F23J15/00
    • F23J7/00C10L9/10F23C3/006
    • A process is provided for combusting sulfur-containing coal in a single step while producing an off-gas low in sulfur. The process comprises combusting finely divided coal in a furnace burner cavity in the presence of a finely divided iron oxide or iron powder and at least about 60% of the oxygen stoichiometrically required for substantially complete combustion of the coal to form a liquid iron oxysulfide phase and a turbulent atmosphere of combustion-product gases, liquid iron oxysulfide acting to scrub sulfur-containing gaseous species from the atmosphere to yield an essentially sulfur-free flue gas and a liquid iron oxysulfide slag containing substantially the sulfur originally contained in the coal.
    • 提供了在单一步骤中燃烧含硫煤同时产生低硫的废气的方法。 该方法包括在细分的氧化铁或铁粉的存在下在炉燃烧器腔中燃烧细碎的煤,并且至少约60%的氧气用于煤的基本完全燃烧以形成硫化铁铁硫化物相,并且 燃烧产物气体的紊乱气氛,硫氧化亚铁作用于从大气中洗涤含硫气体物质,产生基本上无硫的烟道气和基本上含有煤中所含硫的液体硫铁矿渣。