    • 1. 发明授权
    • Catalyst and support, and their methods of preparation
    • 催化剂和配方及其制备方法
    • US4456699A
    • 1984-06-26
    • US485308
    • 1983-04-15
    • Albert L. Hensley, Jr.Leonard M. Quick
    • Albert L. Hensley, Jr.Leonard M. Quick
    • B01J21/02B01J21/12B01J27/16B01J35/10B01J37/10C10G45/04B01J27/14
    • B01J37/10B01J21/02B01J21/12B01J27/16B01J35/10B01J35/1019B01J35/1047B01J35/1061C10G2300/107
    • A catalyst support is prepared from a composite comprising alumina and one or more oxides of phosphorus by forming the composite into a shaped support material having at least 0.8 cc/gm of its pore volume in pores having diameters of 0 nm (0 .ANG.) to 120 nm (1,200 .ANG.) and at least 0.1 cc/gm of its pore volume in pores having diameters of 120 nm (1,200 .ANG.) to 5,000 nm (50,000 .ANG.) and heating said shaped support material in the presence of steam at sufficient elevated temperature, steam pressure, and time period to increase the average pore diameter of said shaped support in the absence of any appreciable reduction in pore volume.A catalyst is prepared by impregnating the steam-treated support with at least one hydrogenating metal.The catalyst can be used suitably in hydrocarbon conversion processes, such as a process for the hydrodemetallization of a hydrocarbon stream containing asphaltenes and a substantial amount of metals.
    • 催化剂载体由包含氧化铝和一种或多种磷的氧化物的复合材料制成,通过将复合材料形成为直径为0nm(0安格姆)至120的孔中至少具有0.8cc / gm孔体积的成形载体材料 nm(1200 ANGSTROM),并且在直径为120nm(1,200)至5,000nm(50,000)的孔中,其孔体积至少为0.1cc / gm,并且在足够高的温度下在蒸汽存在下加热所述成形载体材料, 蒸汽压力和时间段,以在没有任何明显的孔体积减小的情况下增加所述成形支撑件的平均孔径。 通过用至少一种氢化金属浸渍蒸汽处理的载体来制备催化剂。 催化剂可以适用于烃转化方法,例如含有沥青质的烃物流和大量金属的加氢脱金属的方法。
    • 5. 发明授权
    • Process for demetallation and desulfurization of heavy hydrocarbons
    • 重质烃脱金属脱硫工艺
    • US4297242A
    • 1981-10-27
    • US168297
    • 1980-07-14
    • Albert L. Hensley, Jr.Leonard M. Quick
    • Albert L. Hensley, Jr.Leonard M. Quick
    • B01J21/04B01J23/24B01J23/28B01J35/10C10G45/04C10G45/08C10G65/04B01J27/02B01J23/16
    • B01J35/10B01J23/24B01J23/28B01J21/04B01J35/1019B01J35/1042B01J35/1061B01J35/108C10G2300/107
    • Disclosed is a two-stage catalytic process for hydrodemetallation and hydrodesulfurization of heavy hydrocarbon streams containing asphaltenes and a substantial amount of metals. The first stage of this process comprises contacting the feedstock in a first reaction zone with hydrogen and a demetallation catalyst comprising hydrogenation metal selected from Group VIB and/or Group VIII deposed on a large-pore, high surface area inorganic oxide support; the second stage of the process comprises contacting the effluent from the first reaction zone with a catalyst consisting essentially of hydrogenation metal selected from Group VIB deposed on a smaller-pore, catalytically active support comprising alumina, said second-stage catalyst having a surface area within the range of about 150 m.sup.2 /gm to about 300 m.sup.2 /gm, having a majority of its pore volume in pore diameters within the range of about 80 A to about 130 A, and the catalyst has a pore volume within the range of about 0.4 cc/gm to about 0.9 cc/gm.
    • 公开了用于含有沥青质和大量金属的重质烃流的加氢脱金属和加氢脱硫的两阶段催化方法。 该方法的第一阶段包括使第一反应区中的原料与氢气和脱金属催化剂接触,所述脱金属催化剂包含选自分布在大孔,高表面积无机氧化物载体上的VIB族和/或VIII族的氢化金属; 该方法的第二阶段包括将来自第一反应区的流出物与基本上由选自组分VIB的氢化金属组成的催化剂接触,所述组VIB位于包含氧化铝的较小孔催化活性载体上,所述第二级催化剂的表面积在 约150m 2 / gm至约300m 2 / gm的范围,其孔径的大部分孔径在约80至约130的范围内,并且催化剂的孔体积在约0.4的范围内 cc / gm至约0.9cc / gm。
    • 6. 发明授权
    • Process for hydrotreating heavy hydrocarbons
    • 加氢处理重质烃的方法
    • US4225421A
    • 1980-09-30
    • US20072
    • 1979-03-13
    • Albert L. Hensley, Jr.Leonard M. Quick
    • Albert L. Hensley, Jr.Leonard M. Quick
    • B01J23/28B01J35/10C10G45/04C10G45/08C10G65/10C10G49/04
    • B01J35/10B01J23/28B01J35/1019B01J35/1042B01J35/1061B01J35/1066B01J35/109C10G2300/107
    • A process for hydrodemetallation and hydrodesulfurization of hydrocarbon feedstock containing asphaltenes and metals by contacting said feedstock with hydrogen and a bimodal catalyst consisting essentially of at least one active original hydrogenation metal selected from Group VIB deposited on a support comprising alumina wherein said catalyst has a surface area within the range of about 140 to about 300 m.sup.2 /gm, a total pore volume based upon measurement by mercury penetration within the range of about 0.4 cc/gm to about 1.0 cc/gm, and comprising about 60% to about 95% of its micropore volume in micropores having diameters within the range of about 50 A to about 200 A, 0% to about 15% of its micropore volume in pores having diameters within the range of about 200 A to about 600 A and about 3% to about 30% of said total pore volume based upon measurements by mercury penetration in macropores having diameters of 600 A or greater.
    • 通过使所述原料与氢和双键催化剂接触,该催化剂主要由选自沉积在包含氧化铝的载体上的至少一种活性原始氢化金属组成的双峰催化剂进行加氢脱金属和加氢脱硫的方法,其中所述催化剂具有表面积 在约140至约300m 2 / gm的范围内,基于通过汞渗透测量在约0.4cc / gm至约1.0cc / gm范围内的总孔体积,并且包含其约60%至约95% 直径在约50A至约200A范围内的微孔中的微孔体积,其孔径中的微孔体积的0%至约15%,其直径在约200至约600的范围内,并且约3%至约30 基于直径为600A或更大的大孔中汞渗透测量的所述总孔体积的百分比。
    • 8. 发明授权
    • Catalyst and support, their methods of preparation, and processes
employing same
    • 催化剂和载体,它们的制备方法和使用它们的方法
    • US4495062A
    • 1985-01-22
    • US485185
    • 1983-04-15
    • Albert L. Hensley, Jr.Leonard M. Quick
    • Albert L. Hensley, Jr.Leonard M. Quick
    • B01J21/02B01J21/12B01J23/28B01J27/16B01J35/10B01J37/10C10G45/04C10G47/12C10G45/08
    • B01J37/10B01J21/02B01J21/12B01J23/28B01J27/16B01J35/10B01J35/1019B01J35/1042B01J35/1047B01J35/1061B01J35/108C10G2300/107
    • A catalyst support is prepared from a composite comprising two or more inorganic oxides by forming the composite into a shaped support material having at least 0.8 cc/gm of its pore volume in pore diameters of 0 nm (0 .ANG.) to 120 nm (1,200 .ANG.) and at least 0.1 cc/gm of its pore volume in pore diameters of 120 nm (1,200 .ANG.) to 5,000 nm (50,000 .ANG.) and heating said shaped support material in the presence of steam at sufficient elevated temperature, steam pressure, and time period to increase the average pore diameter of said shaped support in the absence of any appreciable reduction in pore volume. The inorganic oxide composite is selected from the group consisting of a mixture of alumina and silica; a mixture of alumina, silica, and oxides of phosphorus; a mixture of alumina and oxides of phosphorus; a mixture of alumina and boria; a mixture of alumina, boria and oxides of phosphorus; and a mixture of alumina, magnesia, and oxides of phosphorus, the oxides of phosphorus being calculated as P.sub.2 O.sub.5 and the quantities being based upon the weight of the composite.A catalyst is prepared by impregnating the steam-treated support with at least one hydrogenating metal.The catalyst can be used suitably in hydrocarbon conversion processes, such as a process for the hydrodemetallization of a hydrocarbon stream containing asphaltenes and a substantial amount of metals.
    • 催化剂载体由包含两种或更多种无机氧化物的复合材料制备,通过将复合材料形成为孔径为0nm(0安格姆)至120纳米(1,200安格姆)的孔体积至少为0.8cc /克的成形载体材料 )和至少0.1cc / gm的孔径为120nm(1,200安格姆)至5,000nm(50,000安培)的孔体积,并在蒸汽存在下在足够高的温度,蒸汽压力和时间下加热所述成形的支撑材料 在没有任何明显的孔体积减小的情况下增加所述成形载体的平均孔径。 无机氧化物复合材料选自氧化铝和二氧化硅的混合物; 氧化铝,二氧化硅和磷的氧化物的混合物; 氧化铝和磷的氧化物的混合物; 氧化铝和氧化硼的混合物; 氧化铝,氧化硼和磷的氧化物的混合物; 以及氧化铝,氧化镁和磷的氧化物的混合物,磷的氧化物计算为P 2​​ O 5,其数量基于复合材料的重量。 通过用至少一种氢化金属浸渍蒸汽处理的载体来制备催化剂。 催化剂可以适用于烃转化方法,例如含有沥青质的烃物流和大量金属的加氢脱金属的方法。
    • 9. 发明授权
    • Three-catalyst process for the hydrotreating of heavy hydrocarbon streams
    • 用于加氢处理重质烃流的三催化过程
    • US4431525A
    • 1984-02-14
    • US371815
    • 1982-04-26
    • Albert L. Hensley, Jr.Leonard M. Quick
    • Albert L. Hensley, Jr.Leonard M. Quick
    • B01J35/10C10G45/04C10G45/08C10G65/04
    • B01J35/10B01J35/1019B01J35/1042B01J35/1061B01J35/1085C10G2300/107
    • There is disclosed a process for hydrotreating a heavy hydrocarbon stream containing metals, asphaltenes, nitrogen compounds, and sulfur compounds to reduce the contents of these contaminants. The process comprises contacting said stream in the presence of hydrogen and under suitable hydrotreating conditions in sequence with a first catalyst in a first reaction zone, a second catalyst in a second reaction zone, and a third catalyst in a third reaction zone. The first catalyst comprises a Group VIB metal and/or a Group VIII metal on a porous inorganic oxide support; the second catalyst consists essentially of at least one hydrogenation metal selected from Group VIB deposed on a support material comprising alumina; and the third catalyst comprises a hydrogenating component comprising molybdenum, chromium, and cobalt on a large-pore, catalytically-active alumina. Each catalyst has specific physical properties.
    • 公开了一种加氢处理含有金属,沥青质,氮化合物和硫化合物的重质烃流的方法,以减少这些污染物的含量。 该方法包括在氢气存在下,在合适的加氢处理条件下,将第一催化剂在第一反应区,第二反应区中的第二催化剂和第三反应区中的第三催化剂依次接触。 第一催化剂在多孔无机氧化物载体上包含VIB族金属和/或Ⅷ族金属; 第二催化剂基本上由至少一种氢化金属组成,所述氢化金属选自ⅤB组,其包含氧化铝的载体材料; 并且第三催化剂包含在大孔催化活性氧化铝上的包含钼,铬和钴的氢化组分。 每种催化剂都具有特定的物理性质。