    • Lithium secondary battery
    • 锂二次电池
    • US20070202365A1
    • 2007-08-30
    • US11709252
    • 2007-02-22
    • Shouichirou SawaKazuyuki SatouAtsushi FukuiYasuyuki KusumotoMaruo Kamino
    • Shouichirou SawaKazuyuki SatouAtsushi FukuiYasuyuki KusumotoMaruo Kamino
    • H01M14/00H01M4/58H01M4/62
    • H01M4/134H01M4/622H01M4/661H01M2004/021H01M2010/4292
    • In a lithium secondary battery using negative electrode active material particles containing silicon, excellent charge-discharge characteristics are achieved and swelling of the negative electrode is minimized. A lithium secondary battery has a positive electrode containing a positive electrode active material, a negative electrode containing an active material layer and a current collector made of a conductive metal foil, and a non-aqueous electrolyte. The active material layer has a binder and active material particles containing silicon, and is formed by sintering the active material layer on a current collector surface in a non-oxidizing atmosphere. The active material particles have an average particle size of from 7.5-15 μm and a particle size distribution such that 60 volume % or more of the active material particles falls within the ±40% range of the average particle size, and the lithium secondary battery has a negative/positive electrode capacity ratio of 1.7 or greater.
    • 在使用含有硅的负极活性物质粒子的锂二次电池中,实现了优异的充放电特性,并使负极的膨胀最小化。 锂二次电池具有包含正极活性物质的正极,含有活性物质层的负极和由导电性金属箔构成的集电体和非水电解质。 活性物质层具有粘合剂和含有硅的活性物质颗粒,并且通过在非氧化性气氛中在集电体表面上烧结活性物质层而形成。 活性物质粒子的平均粒径为7.5〜15μm,粒径分布为60体积%以上的活性物质粒子落入平均粒径的±40%范围内,锂二次电池 负极/正极容量比为1.7以上。