    • Method for the Preparation of High-Efficient, Tuneable and Switchable Optical Elements Based on Polymer-Liquid Crystal Composites
    • 基于聚合物 - 液晶复合材料制备高效,可调和可切换的光学元件的方法
    • US20080063808A1
    • 2008-03-13
    • US11571426
    • 2005-06-28
    • Joachim StumpeSergej SlussarenkoOksana Sakhno
    • Joachim StumpeSergej SlussarenkoOksana Sakhno
    • B05D5/06B05D3/06
    • G02F1/13342
    • A homogeneous isotropic mixture of photocurable monomers and/or oligomers, one or more liquid crystals or a liquid crystal mixture, and optionally a photoinitiator is provided that is homogeneous and optically clear within a temperature range of between 15 and 25° C. An optically transparent film of the homogenous isotropic mixture on a substrate or in a space between two substrates is prepared. The optically transparent film is irradiated with an inhomogeneous light field of actinic light such that areas of the film are irradiated while others are not. The intensity is sufficiently low that first areas solely, substantially or mainly composed of photocured polymer are formed, while the liquid crystals or liquid crystal mixture completely, substantially or mainly escapes into second areas that are not or substantially not irradiated. The substrates are removed depending on whether the rigid or flexible film is to be prepared alone or on a substrate.
    • 提供可光固化单体和/或低聚物,一种或多种液晶或液晶混合物以及任选的光引发剂的均匀各向同性混合物,其在15至25℃的温度范围内是均匀的和光学透明的。光学透明 准备在基板上或两个基板之间的空间中均匀各向同性混合物的膜。 光学透明膜用光化不均匀的光场照射,使得膜的面积不被照射。 强度足够低,仅形成基本上或主要由光固化聚合物构成的第一区域,而液晶或液晶混合物完全,基本上或主要逸出到不被或基本上不被照射的第二区域。 取决于刚性或柔性膜是单独制备还是在基材上制备基材。