    • Suspension polymerization
    • 悬浮聚合
    • US4833179A
    • 1989-05-23
    • US104092
    • 1987-10-02
    • Chung I. YoungRudyard M. Enanoza
    • Chung I. YoungRudyard M. Enanoza
    • C08F220/10C09J7/02
    • C08F220/10C09J7/0217
    • The present invention relates to a method for suspension polymerization of a pressure-sensitive acrylate copolymer bead having a glass transition temperature of 0.degree. C. or less. The method comprises making a monomer premix comprising an acrylic acid ester of non-tertiary alcohol, the alcohol having from 1 to 14 carbon atoms, with the average number of carbon atoms being about 4 to about 12, a polar monomer copolymerizable with the acrylic acid ester, a chain transfer agent, a free-radical initiator, and a modifier moiety selected from the group consisting of 2-polystyrylethyl methacrylate macromolecular monomers, reactive zinc salts and hydrophobic silicas. The premix is then combined with a water phase containing a sufficient amount of suspending agent to form a suspension. The suspension is concurrently agitated and polymerization of the polymer premix is permitted until polymer beads are formed. The polymer beads are then collected. The amount of the modifier moiety must be sufficient to render the copolymer bead non-agglomerating at room temperature and safely handleable and transportable.
    • 本发明涉及玻璃化转变温度为0℃以下的压敏丙烯酸酯共聚物珠粒的悬浮聚合方法。 该方法包括制备包含非叔醇的丙烯酸酯,具有1至14个碳原子的醇,平均碳原子数为约4至约12的单体预混物,可与丙烯酸共聚的极性单体 酯,链转移剂,自由基引发剂和选自2-聚甲基丙烯酸甲酯高分子单体,反应性锌盐和疏水性二氧化硅的改性剂部分。 然后将预混物与含有足量的悬浮剂的水相合并以形成悬浮液。 同时搅拌悬浮液,并允许聚合物预混物的聚合直到形成聚合物珠粒。 然后收集聚合物珠。 改性剂部分的量必须足以使共聚物珠粒在室温下不附聚并且可安全地处理和运输。
    • 8. 发明授权
    • Suspension polymerization
    • 悬浮聚合
    • US4952650A
    • 1990-08-28
    • US355281
    • 1989-05-22
    • Chung I. YoungRudyard M. Enanoza
    • Chung I. YoungRudyard M. Enanoza
    • C08F220/10C09J7/02
    • C09J7/0217C08F220/10
    • The present invention relates to a method for suspension polymerization of a pressure-sensitive acrylatre copolymer bead having a glass transition temperature of 0.degree. C. or less. The method comprises making a monomer premix comprising an acrylic acid ester of non-tertiary alcohol, the alcohol having from 1 to 14 carbon atoms, with the average number of carbon atoms being about 4 to about 12, a polar monomer copolymerizable with the acrylic acid ester, a chain transfer agent, a free-radical initiator, and a modifier moiety selected from the group consisting of 2-polystyrylethyl methacrylate macromolecular monomers, reactive zinc salts and hydrophobic silicas. The premix is then combined with a water phase containing a sufficient amount of suspending agent to form a suspension. The suspension is concurrently agitated and polymerization of the polymer premix is permitted until polymer beads are formed. The polymer beads are then collected. The amount of the modifier moiety must be sufficient to render the copolymer bead non-agglomerating at room temperature and safely handleable and transportable.
    • 本发明涉及玻璃化转变温度为0℃以下的压敏丙烯酸共聚物珠粒的悬浮聚合方法。 该方法包括制备包含非叔醇的丙烯酸酯,具有1至14个碳原子的醇,平均碳原子数为约4至约12的单体预混物,可与丙烯酸共聚的极性单体 酯,链转移剂,自由基引发剂和选自2-聚甲基丙烯酸甲酯高分子单体,反应性锌盐和疏水性二氧化硅的改性剂部分。 然后将预混物与含有足量的悬浮剂的水相合并以形成悬浮液。 同时搅拌悬浮液,并允许聚合物预混物的聚合直到形成聚合物珠粒。 然后收集聚合物珠。 改性剂部分的量必须足以使共聚物珠粒在室温下不附聚并且可安全地处理和运输。