    • 1. 发明授权
    • Propylene/ethylene-.alpha.-olefin block copolymer and process for
processing the same
    • 丙烯/乙烯-α-烯烃嵌段共聚物及其加工方法
    • US5990242A
    • 1999-11-23
    • US863395
    • 1997-05-27
    • Naofumi NagaYoshiaki OobayashiMasatada TasakaKouji Mizunuma
    • Naofumi NagaYoshiaki OobayashiMasatada TasakaKouji Mizunuma
    • C08F297/08C08F297/00
    • C08F297/08
    • A propylene/ethylene-.alpha.-olefin block copolymer obtained by block-copolymerizing a polypropylene component with an ethylene-.alpha.-olefin random copolymer component, which satisfies conditions of the following terms (I) to (III):(I) the content of the polypropylene component having an intrinsic viscosity ([.eta.]) measured in tetralin at 135.degree. C. of from 0.5 to 5.0 dl/g is from 5 to 95% by weight;(II) the content of the .alpha.-olefin in the random copolymer component is from 5 to 40 mol %, and the content of the ethylene-.alpha.-olefin random copolymer component whose .rho. value represented by the following equation:.rho.=2[E].multidot.[A]/[EA](wherein [E] represents a molar fraction of ethylene, [A] represents a molar fraction of the .alpha.-olefin and [EA] represents a molar fraction of a diad chain of ethylene and the .alpha.-olefin) is within the range from 0.5 to 1.5 is from 5 to 95% by weight; and(III) the intrinsic viscosity ([.eta.]) of the propylene/ethylene-.alpha.-olefin block copolymer measured in tetralin at 135.degree. C. is from 0.5 to 5.0 dl/g, and a process for producing the above propylene/ethylene-.alpha.-olefin block copolymer.
    • 通过将聚丙烯组分与乙烯-α-烯烃无规共聚物组分嵌段共聚获得的丙烯/乙烯-α-烯烃嵌段共聚物,其满足以下(I)至(III)的条件:(I) 在135℃下在四氢化萘中测得的特性粘度(η)为0.5-5.0dl / g的聚丙烯组分为5-95重量% (II)中,无规共聚物成分中的α-烯烃的含量为5〜40摩尔%,rho值由下式表示的乙烯-α-烯烃无规共聚物成分的含量:rho = 2 [E ] x [A] / [EA](其中[E]表示乙烯的摩尔分数,[A]表示α-烯烃的摩尔分数,[EA]表示乙烯的二元链的摩尔分数, α-烯烃)在0.5〜1.5的范围内为5〜95重量% 和(III)在135℃下在四氢化萘中测得的丙烯/乙烯-α-烯烃嵌段共聚物的特性粘度(η)为0.5-5.0dl / g,以及制备上述丙烯/乙烯 α-烯烃嵌段共聚物。
    • 2. 发明授权
    • Propylene/ethylene-&agr;-olefin block copolymer and process for producing the same
    • 丙烯/乙烯-α-烯烃嵌段共聚物及其制备方法
    • US06613845B1
    • 2003-09-02
    • US09337502
    • 1999-06-22
    • Naofumi NagaYoshiaki OobayashiMasatada TasakaKouji Mizunuma
    • Naofumi NagaYoshiaki OobayashiMasatada TasakaKouji Mizunuma
    • C08F29300
    • C08F297/08
    • A propylene/ethylene-&agr;-olefin block copolymer obtained by block-copolymerizing a polypropylene component with an ethylene-&agr;-olefin random copolymer component, which satisfies conditions of the following terms (I) to (III): (I) the content of the polypropylene component having an intrinsic viscosity ([&eegr;]) measured in tetralin at 135° C. of from 0.5 to 5.0 dl/g is from 5 to 95% by weight; (II) the content of the &agr;-olefin in the random copolymer component is from 5 to 40 mol %, and the content of the ethylene-&agr;-olefin random copolymer component whose &rgr; value represented by the following equation: &rgr;=2[E]·[A]/[EA] (wherein [E] represents a molar fraction of ethylene, [A] represents a molar fraction of the &agr;-olefin and [EA] represents a molar fraction of a diad chain of ethylene and the &agr;-olefin) is within the range from 0.5 to 1.5 is from 5 to 95% by weight; and (III) the intrinsic viscosity ([&eegr;]) of the propylene/ethylene-&agr;-olefin block copolymer measured in tetralin at 135° C. is from 0.5 to 5.0 dl/g, and a process for producing the above propylene/ethylene-&agr;-olefin block copolymer.
    • 通过将聚丙烯组分与乙烯-α-烯烃无规共聚物组分嵌段共聚获得的丙烯/乙烯-α-烯烃嵌段共聚物,其满足下列条件(I)至(III):( I)的条件: 在135℃下在四氢化萘中测得的特性粘度(η)为0.5-5.0dl / g的聚丙烯组分为5-95重量%;(II)随机的α-烯烃含量 共聚物成分为5〜40摩尔%,rho值由下式表示的乙烯-α-烯烃无规共聚物成分的含量:[其中[E]表示乙烯的摩尔分数,[A]表示摩尔 α-烯烃的分数和[EA]表示乙烯和α-烯烃的二价链的摩尔分数在0.5至1.5的范围内为5至95重量%; 和(III)在135℃下在四氢化萘中测得的丙烯/乙烯-α-烯烃嵌段共聚物的特性粘度(η)为0.5-5.0dl / g,制备上述丙烯/乙烯 α-烯烃嵌段共聚物。