    • Process for the manufacture of a non-woven web from synthetic filaments
    • 从合成纤维制造无纺网的方法
    • US4217387A
    • 1980-08-12
    • US945394
    • 1978-09-25
    • Dirk J. ViezeePetrus J. M. MekkelholtJohannes A. Juijn
    • Dirk J. ViezeePetrus J. M. MekkelholtJohannes A. Juijn
    • D04H3/011D04H3/03D04H1/58B29D27/00
    • D04H3/011D04H3/03Y10T442/681
    • Manufacture of a non-woven web of man-made filaments in which one or more strands of filaments, directed parallel to each other, leaving one or more spinnerets are forwarded, each, by means of an air jet to a spreading plate for the filaments, and the resulting layer of spread filaments and air leaves the plate and advances to a moving support, upon which the filaments are deposited randomly to form a web which will then be bonded in known manner. In order to improve the isotropy of the web, the layer of spread filaments and air is guided to a fixed deflector plate forming a slit with the discharge edge of the stationary spreading plate, said slit allowing passage of the filaments but braking the air carried along with the filaments, and the layer is then subjected to an air jet directed transversely to the path of said deflected web and generally in a direction parallel to the surface of the moving support.
    • 制造人造细丝的无纺织物网,其中一根或多根彼此平行的丝线,留下一个或多个喷丝头,每个都通过空气喷射送到长丝的铺展板 ,并且所得到的铺展的细丝和空气层离开板并且前进到移动的支撑件,随后将细丝沉积在其上,以形成纤维网,然后以已知的方式粘合纤维网。 为了改善幅材的各向同性,将扩散的细丝层和空气层引导到固定扩散板的形成狭缝的固定偏转板,所述狭缝允许细丝通过,同时制动所携带的空气 并且该层然后经受横向于所述偏转幅材的路径的空气射流,并且通常在平行于移动支撑件的表面的方向上。
    • 4. 发明授权
    • Process for preparing polyketone fibres
    • 制备聚酮纤维的方法
    • US06495075B1
    • 2002-12-17
    • US09582947
    • 2000-07-28
    • Hendrik MiddeljansJannes VeurinkJohannes A. Juijn
    • Hendrik MiddeljansJannes VeurinkJohannes A. Juijn
    • D01D5084
    • D01F6/30
    • The invention pertains to a process for preparing thermoplastic fibres by melt-spinning an alternating co-polymer composed of alkenes and carbon monoxide in which the polymer is heated to a temperature of at least TNF+5° C., with TNF being the temperature at which the molten polymer is free of crystallization nuclei, and where the residence time of the polymer at a single temperature or different temperatures above the polymer melting point satisfies: [ ∑ n = 1 ∞ ⁢ t n · exp ⁢   ⁢ ( A + B T n ) ] ≤ 1. wherein tn is the residence time (in minutes) of the polymer at a temperature Tn (in K, with Tn>Tm) and A and B are determined by measuring the viscosity of the polymer at different temperatures and residence times.
    • 本发明涉及通过将由烯烃和一氧化碳组成的交替共聚物熔融纺丝制备热塑性纤维的方法,其中将聚合物加热至至少TNF + 5℃的温度,其中TNF为 其中熔融聚合物不含结晶核,并且其中聚合物在单一温度或高于聚合物熔点的不同温度下的停留时间满足:其中tn是在温度Tn下聚合物的停留时间(以分钟为单位) 在K中,Tn> Tm),A和B通过在不同温度和停留时间下测量聚合物的粘度来测定。