    • 5. 发明申请
    • Binder resin compositions, production process and use thereof
    • 粘合剂树脂组合物,生产工艺及其用途
    • US20060025533A1
    • 2006-02-02
    • US10500111
    • 2002-12-20
    • Naosuke KomotoHidetoshi Yoshioka
    • Naosuke KomotoHidetoshi Yoshioka
    • C08F251/00C08F10/00
    • C08F8/22C08F8/50C08F255/02C08F255/023C08L51/06C08F10/06C08F220/08
    • The invention provides a novel binder resin composition with good adherence onto prime materials of polyolefin, poly (vinyl chloride), polycarbonate, PET, ABS and nylon, and also with excellent solvent solubility. A binder resin composition characterized by being chlorinated propylenic random copolymer with weight average molecular weight of 3000 to 250000, wherein propylenic random copolymer with melting point (Tm) measured by differential scanning calorimeter (DSC) of 115 to 165° C. obtained by copolymerizing propylene with other α-olefin in the coexistence of metallocene type catalyst is chlorinated to chlorine content of 10 to 40% by weight, after thermal degradation or directly without thermal degradation, and/or a binder resin composition characterized by containing carboxyl group-containing chlorinated propylenic random copolymer with weight average molecular weight of 30000 to 220000, wherein propylenic random copolymer with melting point (Tm) measured by differential scanning calorimeter (DSC) of 115 to 165° C. obtained by copolymerizing propylene with other α-olefin in the coexistence of metallocene type catalyst is grafted with α,β-unsaturated carboxylic acid or its anhydride in amounts of 0.1 to 20% by weight, after thermal degradation or directly without thermal degradation, and then chlorinated to chlorine content of 10 to 40% by weight, stabilizer and organic solvent.
    • 本发明提供了对聚烯烃,聚(氯乙烯),聚碳酸酯,PET,ABS和尼龙的主要材料具有良好粘附性的新型粘合剂树脂组合物,并且还具有优异的溶剂溶解性。 一种粘合剂树脂组合物,其特征在于重均分子量为3000〜250000的氯化丙烯酸无规共聚物,其中通过差示扫描量热计(DSC)测定的熔点(Tm)为115〜165℃的丙烯无规共聚物,其通过使丙烯 与茂金属型催化剂共存的其它α-烯烃氯化成氯含量为10〜40重量%,热降解后或直接不进行热降解,和/或以含羧基的氯化丙烯酸为特征的粘合剂树脂组合物 重均分子量为30000至220000的无规共聚物,其中通过差示扫描量热计(DSC)测量的熔点(Tm)为115至165℃的丙烯无规共聚物通过共聚丙烯与其它α-烯烃共聚获得 茂金属型催化剂用α,β-不饱和羧酸或其a 二氢化钠的量为0.1〜20重量%,经热降解后直接进行无热降解,氯化至氯含量为10〜40重量%的稳定剂和有机溶剂。