    • Hideki KuwataTakayoshi OkuzuMunehiro MiyakeMitsuo YoshidaJunji OkamotoKunihiko OzakiMiyuki KamoshitaReiko Ueno
    • Hideki KuwataTakayoshi OkuzuMunehiro MiyakeMitsuo YoshidaJunji OkamotoKunihiko OzakiMiyuki KamoshitaReiko Ueno
    • B32B27/36B32B9/00B32B27/00B32B27/30B32B27/28
    • B32B7/12B32B27/08C08J7/042C08J7/045Y10T428/31504Y10T428/31786Y10T428/31855Y10T428/31938
    • A gas barrier laminate comprising: a plastic substrate (I); a gas barrier layer (II) formed from a gas barrier layer-forming coating material (C) containing a polyalcohol-based polymer (A) and a polycarboxylic acid-based polymer (B); and an overcoat layer (III) formed from an overcoat layer-forming coating material (F) containing at least one of a monovalent metal compound (D) and a bivalent or higher metal compound (E); wherein the gas barrier layer (II) is laminated to the plastic substrate (I), either directly or with an anchor coat layer disposed therebetween, the overcoat layer (III) is laminated on top of the gas barrier layer (II), and when a laminated product is prepared by laminating a laminate adhesive layer (IV) and a heat seal layer (V), in that order, to either the overcoat layer (III) or the plastic substrate (I) of the gas barrier laminate, either directly or with a printing ink layer disposed therebetween, the lamination strength (X) of the laminated product is not less than 1 N/cm, and the ratio of the lamination strength (Y) following a hot water treatment for 30 minutes at 95° C. relative to the lamination strength (X) (namely, Y/X) is not less than 0.3.
    • 1.一种阻气性层压体,包括:塑料基材(I); 由含有多元醇系聚合物(A)和多元羧酸系聚合物(B)的阻气层形成用涂料(C)形成的阻气层(II) 以及由含有一价金属化合物(D)和二价以上金属化合物(E)中的至少一种的外涂层形成用涂料(F)形成的保护层(III)。 其中所述阻气层(II)直接地或与其间设置的锚涂层层压到所述塑料基板(I)上,所述外涂层(III)层压在所述阻气层(II)的顶部,并且当 通过将层压粘合剂层(IV)和热封层(V)依次层压到阻气性层压体的外涂层(III)或塑​​料基材(I)上,直接制备层压产品 或者设置在其间的印刷油墨层,层压产品的层压强度(X)不小于1N / cm,热水处理后的层压强度(Y)在95℃下30分钟的比例 相对于层压强度(X)(即Y / X)为0.3以上。
    • 3. 发明授权
    • Easy adhesion film
    • 易粘附膜
    • US08309217B2
    • 2012-11-13
    • US12449465
    • 2008-02-12
    • Takayoshi OkuzuHideki Kuwata
    • Takayoshi OkuzuHideki Kuwata
    • B32B7/02B32B27/18B32B27/26B32B27/36B32B38/00
    • C09D5/002C08J7/047C08J2467/00C08K5/34922C09D167/00C09J167/00Y10T428/26Y10T428/265Y10T428/269Y10T428/31786
    • Disclosed is an easy adhesion film which attains sufficient adhesiveness in various processings without using any crosslinking agent such as a melamine resin to possibly pollute the environment and has a primer layer excellent in high-temperature hot water resistance. In the easy adhesion film, a coating film including a polyester resin and a crosslinking agent component in a content of 0.1% by mass or less, inclusive of 0% by mass, is formed on at least one side of a substrate film. The sum of the acid number and the hydroxyl number of the polyester resin is 50 to 200 mg KOH/g, wherein the acid number is 20 to 60 mg KOH/g and the hydroxyl number is 30 to 150 mg KOH/g. The amount of the oligomers contained in the polyester is 2.0% by mass or less. The thickness of the coating film is 0.001 to 0.5 μm.
    • 公开了一种容易的粘合膜,其在各种处理中不会使用三聚氰胺树脂等交联剂,可能污染环境而具有充分的粘合性,并且具有耐高温耐热水性优异的底漆层。 在易粘合膜中,在基材膜的至少一面上形成包含0.1质量%以下,含有0质量%的聚酯树脂和交联剂成分的涂膜。 聚酯树脂的酸值和羟基数之和为50〜200mgKOH / g,酸值为20〜60mgKOH / g,羟值为30〜150mgKOH / g。 聚酯中含有的低聚物的量为2.0质量%以下。 涂膜的厚度为0.001〜0.5μm。
    • 4. 发明申请
    • EASY ADHESION FILM
    • 轻松粘贴胶片
    • US20100136328A1
    • 2010-06-03
    • US12449465
    • 2008-02-12
    • Takayoshi OkuzuHideki Kuwata
    • Takayoshi OkuzuHideki Kuwata
    • B32B5/00B05D3/12
    • C09D5/002C08J7/047C08J2467/00C08K5/34922C09D167/00C09J167/00Y10T428/26Y10T428/265Y10T428/269Y10T428/31786
    • Disclosed is an easy adhesion film which attains sufficient adhesiveness in various processings without using any crosslinking agent such as a melamine resin to possibly pollute the environment and has a primer layer excellent in high-temperature hot water resistance. In the easy adhesion film, a coating film including a polyester resin and a crosslinking agent component in a content of 0.1% by mass or less, inclusive of 0% by mass, is formed on at least one side of a substrate film. The sum of the acid number and the hydroxyl number of the polyester resin is 50 to 200 mg KOH/g, wherein the acid number is 20 to 60 mg KOH/g and the hydroxyl number is 30 to 150 mg KOH/g. The amount of the oligomers contained in the polyester is 2.0% by mass or less. The thickness of the coating film is 0.001 to 0.5 μm.
    • 公开了一种容易的粘合膜,其在各种处理中不会使用三聚氰胺树脂等交联剂,可能污染环境而具有充分的粘合性,并且具有耐高温耐热水性优异的底漆层。 在易粘合膜中,在基材膜的至少一面上形成包含0.1质量%以下,含有0质量%的聚酯树脂和交联剂成分的涂膜。 聚酯树脂的酸值和羟基数之和为50〜200mgKOH / g,酸值为20〜60mgKOH / g,羟值为30〜150mgKOH / g。 聚酯中含有的低聚物的量为2.0质量%以下。 涂膜的厚度为0.001〜0.5μm。