热词
    • 5. 发明授权
    • Zirconium hydroxide
    • 氢氧化锆
    • US07794687B2
    • 2010-09-14
    • US12278074
    • 2007-01-24
    • Heather BradshawClive ButlerHazel Stephenson
    • Heather BradshawClive ButlerHazel Stephenson
    • C01G25/02
    • C01G25/02B01J21/066B01J35/1019B01J35/1042B01J35/1061B01J35/1085C01P2002/72C01P2006/12C01P2006/13C01P2006/14C01P2006/16Y10T428/249953
    • This invention relates to an improved amorphous zirconium hydroxide and a method for its production. The hydroxide has a surface area of at least 300 m2/g, a total pore volume of at least 0.70 cm3/g and an average pore size of between 5 nm and 15 nm, and is prepared by a process which comprises the steps of: a) preparing an aqueous solution comprising sulphate anions and a zirconium salt such that the ZrO2:SO3 ratio is 1:0.40 to 1:0.52, (b) chilling the solution to below 25° C., (c) adding an alkali in order to precipitate the amorphous zirconium hydroxide, (d) filtering and washing the precipitated zirconium hydroxide with water or an alkali to remove residual sulphate and chloride, (e) hydrothermally treating the zirconium hydroxide at a pressure of less than 3 barg, and (f) drying the zirconium hydroxide. The zirconium hydroxide of the present invention, which can be doped, is particularly useful in catalytic applications.
    • 本发明涉及一种改进的无定形氢氧化锆及其制备方法。 氢氧化物具有至少300m 2 / g的表面积,至少0.70cm 3 / g的总孔体积和5nm至15nm的平均孔径,并且通过包括以下步骤的方法制备: a)制备包含硫酸根阴离子和锆盐的水溶液,使得ZrO 2 :SO 3比为1:0.4至1:0.52,(b)将溶液冷却至低于25℃,(c)依次加入碱 (d)用水或碱过滤和洗涤沉淀的氢氧化锆以除去残余的硫酸盐和氯化物,(e)在小于3巴的压力下水热处理氢氧化锆,和(f) 干燥氢氧化锆。 可以掺杂的本发明的氢氧化锆在催化应用中特别有用。