    • 2. 发明授权
    • Production of magnetic iron oxides
    • 生产磁性氧化铁
    • US4358431A
    • 1982-11-09
    • US286134
    • 1981-07-23
    • Horst BrunnPeter KiemleFranz HundHeribert Bade
    • Horst BrunnPeter KiemleFranz HundHeribert Bade
    • C01G49/02C01G49/06G11B5/706H01F1/10H01F1/11C01G49/08
    • G11B5/70642C01G49/06C01P2004/03C01P2004/10C01P2004/61C01P2006/42
    • In the production of needle-shaped magnetic iron oxide pigments by treating iron with a nitro-aromatic in the presence of .alpha.-FeOOH nuclei to form .alpha.-FeOOH particles and an amino-aromatic, and thereafter dehydrating the .alpha.-FeOOH particles and reducing them, the improvement which comprises forming the .alpha.-FeOOH nuclei at about 0.degree. to 90.degree. C. in a suspension of metallic iron, an iron-(II)-salt and a nitro-aromatic by adding a basic precipitant in about 10 to 95% of the amount required for the complete precipitation of the iron in the iron-(II)-salt. Advantageously the metallic iron comprises cast iron, the nitro-aromatic comprises nitrobenzene, the amino-aromatic comprises aniline, the basic precipitant comprises at least one of ammonia and a basically reacting alkali metal, alkaline earth metal or ammonium salt, the nuclei formation is carried out at about 10.degree. to 60.degree. C., and the basic precipitant is added in about 20 to 80% of the amount required for the complete precipitation of the iron in the iron-(II)-salt, additional iron and nitrobenzene being added to the suspension of precipitated nuclei to form the .alpha.-FeOOH particles.
    • 在通过在α-FeO​​OH核的存在下用硝基芳族化合物处理铁以形成α-FeO​​OH颗粒和氨基芳族化合物来生产针状磁性氧化铁颜料,然后使α-FeO​​OH颗粒脱水并还原 包括在金属铁,铁 - (II) - 盐和硝基 - 芳族化合物的悬浮液中在约0至90℃下形成α-FeO​​OH核的改进,通过在约10至95 在铁 - (II) - 铁中完全沉淀铁所需的量的%。 有利地,金属铁包括铸铁,硝基芳族包括硝基苯,氨基 - 芳族包括苯胺,碱性沉淀剂包括氨和基本上反应的碱金属,碱土金属或铵盐中的至少一种,承载核形成 在约10℃至60℃下加入碱性沉淀剂,其中添加铁(II) - 铁中完全沉淀所需的量的约20至80%,添加额外的铁和硝基苯 到析出的核的悬浮液以形成α-FeO​​OH颗粒。
    • 4. 发明授权
    • CaZn.sub.2 (PO.sub.4).sub.2 .2H.sub.2 O anticorrosion pigment
    • CaZn {hd 2 {b(PO {HD 4 {B){HD 2 {B.2H {HD 2 {B O防腐颜料
    • US4153465A
    • 1979-05-08
    • US855482
    • 1977-11-28
    • Franz HundPeter Kresse
    • Franz HundPeter Kresse
    • C09C1/00C01B25/45C09C1/04C09D5/08
    • C01B25/45C09C1/046C09D5/084C01P2002/30C01P2006/12
    • An anticorrosion pigment suited for paints and lacquers and consisting of CaZn.sub.2 (PO.sub.4).sub.2 . 2H.sub.2 O crystallizing in the Scholzite lattice and having a specific surface according to BET of from 0.1 to 50 m.sup.2 /g is produced by a process wherein(a) (i) a salt solution containing calcium and zinc cations in a ratio of about 1:2 is normally, inversely or simultaneously precipitated in air at temperatures of up to about 100.degree. C. with an equivalent or substantially equivalent quantity of a solution containing an alkali metal or ammonium phosphate ion; or (ii) compounds of calcium and zinc, which can be decomposed with relatively strong acids or neutralized with acids, in a ratio of about 1:2, have phosphoric acid or ammonium phosphate added to them in approximately the quantity which is required for decomposition or neutralization, or in a slight excess of that quantity, at temperatures of up to about 100.degree. C.; and(b) the suspension obtained in accordance with (a) (i) or (ii) is heated in air to a temperature of up to about 100.degree. C. or in an autoclave to a temperature of up to about 175.degree. C. over a period of up to about 10 hours, e.g. about 1 to 8 hours, the pigment suspension obtained is washed, filtered off and dried.
    • 一种适用于油漆和漆的防腐颜料,由CaZn2(PO4)2组成。 通过其中(A)(I)含有约1:2比例的钙和锌溶液的盐溶液的方法制备了在Scholzite晶格中结晶并具有0.1至50m 2 / g的BET比表面积的2H 2 O 2 在相当于或基本上相当量的含有碱金属或磷酸铵离子的溶液的情况下,正常地,相反地或同时地在空气中降解高达约100℃的温度。 或(ii)钙和锌的化合物,其可用相对较强的酸分解或用酸中和,以约1:2的比例分解,其中添加了大约为分解所需量的磷酸或磷酸铵 或中和,或略高于该量,在高达约100℃的温度下