    • Hardenable composition based on a Michael addition product, process for
its preparation and its use
    • 基于迈克尔加成产物的可硬化组合物,其制备方法及其用途
    • US5300571A
    • 1994-04-05
    • US663826
    • 1991-03-26
    • Werner A. JungPeter Hoffmann
    • Werner A. JungPeter Hoffmann
    • C08L33/00C08F20060101C08F8/32C08F290/12C08F299/00C08G18/62C08G73/00C08G73/02C08G73/12C08G81/02C08L33/04C09D133/00C09D133/04C08L61/00
    • C08F299/00C08F290/12C08F8/30
    • The invention relates to a hardenable composition containingA) compounds having at least two activated double bonds (I) based on .alpha.,.beta.-unsaturated carbonyl compounds, .alpha.,.beta.-unsaturated carboxylic acid esters or .alpha.,.beta.-unsaturated nitrile groups,B) compounds containing either at least one primary amino group which is blocked by an aldehyde or ketone having not more than 10 C atoms or at least 2 groups which can be hydrolyzed to NH groups, andC) customary additives, if appropriate catalysts, if appropriate pigments and organic solvents.Either component A or component B or components A and B are based on a branched soluble acrylate copolymer P, which is obtainable by copolymerization ofa) 5 to 30% by weight of monomers having at least two ethylenically unsaturated polymerizable double bonds,b) 5 to 60% by weight of monomers having a functional group andc) 5 to 90% by weight of other ethylenically unsaturated monomers,the sum of a, b and c being 100% by weight.The invention also relates to processes for the preparation of the hardenable composition and its use.
    • PCT No.PCT / EP89 / 00950 Sec。 371日期1991年3月26日 102(e)1991年3月26日PCT PCT 1989年8月11日PCT公布。 出版物WO90 / 03404 本发明涉及一种可硬化组合物,其含有A)具有至少两种基于(α),(β-)不饱和羰基化合物,(α),(β) - 不饱和羧酸酯或(α),(β) - 不饱和腈基,B)含有至少一个被不多于10个碳原子或至少2个基团的醛或酮封闭的伯氨基的化合物, 被水解成NH基,C)常规添加剂,如果合适的话,适当的催化剂,如果合适的颜料和有机溶剂。 组分A或组分B或组分A和B基于支化可溶性丙烯酸酯共聚物P,其可通过a)5至30重量%的具有至少两个烯属不饱和可聚合双键的单体的共聚获得,b)5 至60重量%的具有官能团的单体和c)5-90重量%的其它烯属不饱和单体,a,b和c的总和为100重量%。 本发明还涉及制备可硬化组合物的方法及其用途。