    • Process for producing silicon carbide ceramic micro tube with thin wall
    • 生产具有薄壁的碳化硅陶瓷微管的方法
    • US20060239887A1
    • 2006-10-26
    • US11274504
    • 2005-11-16
    • Masaki SugimotoAkira Idesaki
    • Masaki SugimotoAkira Idesaki
    • C01B31/36
    • C04B35/62655B82Y30/00C01B32/956C04B35/62281C04B2235/483C04B2235/5264C04B2235/5284
    • An improved process for producing a silicon carbide ceramic micro tubes (SiC micro tube) from a silicon-based polymer fiber by applying an ionizing radiation such that the surface part of the fiber selectively undergoes oxidative crosslinking, extracting the uncrosslinked core part of the fiber with an organic solvent to form a hollow fiber, and firing it in an inert gas is characterized by using a polymer blend of polycarbosilane and polyvinylsilane as the silicon polymer or applying the ionizing radiation to the silicon-based polymer fiber as it is cooled. The two methods may be performed either individually or in combination to produce tubes with their wall thickness controlled at a desired value in the range of 2-10 μm although this has been impossible to achieve in the prior art.
    • 一种通过施加电离辐射从硅基聚合物纤维制造碳化硅陶瓷微管(SiC微管)的改进方法,使得纤维的表面部分选择性地进行氧化交联,用纤维提取纤维的未交联核心部分 形成中空纤维的有机溶剂,并在惰性气体中烧成,其特征在于使用聚碳硅烷和聚乙烯基硅烷的聚合物共混物作为硅聚合物,或者在冷却时将电离辐射施加到硅基聚合物纤维上。 这两种方法可以单独地或组合地进行,以产生其壁厚度控制在2-10μm范围内的期望值的管,尽管这在现有技术中是不可能实现的。