    • 31. 发明授权
    • Method of using aqueous polymer dispersions as lamination adhesives for
glossy films
    • 使用聚合物水分散体作为光泽膜的层压粘合剂的方法
    • US5474638A
    • 1995-12-12
    • US201266
    • 1994-02-24
    • Klaus KohlhammerWilfried HusterWalter Dobler
    • Klaus KohlhammerWilfried HusterWalter Dobler
    • B32B27/00B32B7/12C08F28/00C08F220/10C08F220/12C08F220/26C08F220/28C08F228/02C08J5/12C09J133/04C09J133/06C09J133/08C09J129/02
    • B32B7/12C09J133/06
    • The invention relates to a method of using aqueous polymer dispersions based on acrylate-methacrylate copolymers as lamination adhesives for heat sealed glossy films, where the aqueous polymer dispersions have a solids content of from 20 to 65% by weight, the copolymer has a glass transition temperature of from -35.degree. to -10.degree. C., a K value of from 40 to 100 and a mean particle size of less than 200 nm, and the copolymer is obtainable by free-radical emulsion polymerization of:a) from 50 to 80 parts by weight of one or more comonomers from the group consisting of alkyl acrylates of alcohols having 2 to 10 carbon atoms,b) from 10 to 25 parts by weight of one or more comonomers from the group consisting of alkyl methacrylates of alcohols having 1 to 10 carbon atoms, andc1) from 0 to 10 parts by weight of one or more vinyl-aromatic comonomers,c2) from 0.1 to 4.0 parts by weight of one or more .alpha.,.beta.-unsaturated, monoolefinic carboxylic acids,c3) from 0 to 4.0 parts by weight of one or more .alpha..beta.-unsaturated, monoolefinic carboxamides,c4) from 0 to 8 parts by weight of one or more comonomers from the group consisting of hydroxyalkyl (meth)acrylates made from esters of acrylic acid or methacrylic acid and diols having 2 to 10 carbon atoms, andc5) from 0.1 to 4.0 parts by weight of one or more .alpha..beta.-unsaturated, monoolefinic compounds containing sulfonyl or sulfonate groups.
    • 本发明涉及使用基于丙烯酸酯 - 甲基丙烯酸酯共聚物的水性聚合物分散体作为热密封光泽膜的层压粘合剂的方法,其中聚合物水分散体的固体含量为20-65重量%,该共聚物具有玻璃化转变 温度为-35〜-10℃,K值为40〜100,平均粒径小于200nm,共聚物可通过自由基乳液聚合得到:a)从50〜 80重量份由具有2至10个碳原子的醇的丙烯酸烷基酯组成的组中的一种或多种共聚单体,b)10至25重量份的一种或多种共聚单体,其由具有1个 至少10个碳原子,和c1)0至10重量份的一种或多种乙烯基芳族共聚单体,c2)0.1至4.0份重量的一种或多种α,β-不饱和单烯烃羧酸,c3) 0〜4.0份重量 t的一种或多种αβ-不饱和单烯烃甲酰胺,c4)0至8份重量的一种或多种由丙烯酸或甲基丙烯酸的酯和二醇制成的(甲基)丙烯酸羟烷基酯的共聚单体,其具有2 至10个碳原子,和c5)0.1至4.0重量份的一种或多种含有磺酰基或磺酸酯基团的α不饱和单烯烃化合物。
    • 32. 发明授权
    • Photosensitive recording element
    • 感光记录元素
    • US5112723A
    • 1992-05-12
    • US476939
    • 1990-02-08
    • Wolfgang HuemmerWalter DoblerDieter Littmann
    • Wolfgang HuemmerWalter DoblerDieter Littmann
    • G03F7/004G03F7/027G03F7/031G03F7/032
    • G03F7/027G03F7/032
    • In a photosensitive recording element which contains at least one photopolymerizable recording layer (B) consisting ofb.sub.1) at least one partially of virtually completely hydrolyzed poly(vinyl alkanecarboxylate) and/or at least one partially or virtually completely hydrolyzed vinyl alkanecarboxylate/alkylene oxide graft copolymer as a binder,b.sub.2) at least one photopolymerization initiator,b.sub.3) at least one photopolymerizable olefinically unsaturated compound (monomer) which is compatible with the binder (b.sub.1), and/or photopolymerizable olefinically unsaturated radicals which are bonded as side radicals and/or terminal radicals to the binder (b.sub.1), andb.sub.4) at least two assistants, at least one of the said assistants (b.sub.4) has been selected from the group consisting ofb.sub.41) the isoalloxazines and the alloxazines, and at least one of the other assistants has been selected from the group consisting ofb.sub.42) the potassium salt of N-nitrosocyclohexylhydroxlamine, N-nitrosodiphenylamine and hydroquinone monomethyl ether,the amounts used of the assistants (b.sub.41) and (b.sub.42) being from 0.01 to 6% by weight, based on the total weight of the photopolymerizable recording layer (B), and the weight ratio (b.sub.41) : B.sub.42) being from 1:2 to 1:1,000.
    • 在含有至少一种可光聚合记录层(B)的光敏记录元件中,所述光致聚合记录层(B)由b1)至少部分实质上完全水解的聚(乙烯基链烷羧酸酯)和/或至少一种部分或几乎完全水解的乙烯基烷羧酸酯/烯化氧接枝 共聚物作为粘合剂,b2)至少一种光聚合引发剂,b3)与粘合剂(b1)相容的至少一种可光聚合的烯属不饱和化合物(单体)和/或可光聚合的烯属不饱和基团作为侧基键合和/ 或末端基团,和b4)至少两种助剂,所述助剂(b4)中的至少一种选自b41)异卤代氮杂和氧氟烷,并且至少一种 其他助剂选自b42)N-亚硝基环己基羟胺的钾盐,N-亚硝基二苯胺和水解剂 (b41)和(b42)的助剂(b41)和(b42)所用的量为0.01-6重量%,基于可光聚合记录层(B)的总重量和重量比(b41):B42) 从1:2到1:1,000。
    • 37. 发明授权
    • Continuous process for producing pseudoionones and ionones
    • 连续生产假阳离子和紫罗兰酮的方法
    • US07141698B2
    • 2006-11-28
    • US10533969
    • 2003-10-28
    • Walter DoblerNicolaus BahrKlaus BreuerAlois Kindler
    • Walter DoblerNicolaus BahrKlaus BreuerAlois Kindler
    • C07C45/72
    • C07C403/16C07C45/54C07C2601/14C07C2601/16C07C49/203
    • The invention relates to a continuous process for producing pseudoionones of general formulas (I) and (I′) as well as isomers thereof, whereby: R1 represents CH3 or (a); R2 and R3 represent hydrogen, CH3 or C2H5, and; R4 and R5 represent hydrogen or CH3. These pseudoionones are produced by reacting an aldehyde of formula (II) with an excess of a ketone of general formula (III), whereby R1, R2 and R3 have the aforementioned meanings, in the presence of water and alkali hydroxide at an increased temperature and in a homogeneous solution. The inventive process is characterized in that: a) the intermixing of the homogeneous solution consisting of aldehyde, ketone and aqueous alkali lye occurs at a temperature ranging from 10 to 120° C.; b) the undissolved water and alkali hydroxide contained in the reaction mixture are subsequently separated out; c) while avoiding back mixing, the homogeneous reaction mixture is then guided through a reactor, which permits a residence time ranging from 2 to 300 minutes, at a temperature that is 10 to 120° C. higher than the boiling point of the lowest-boiling component and under a vapor pressure p ranging from 106 to 107 Pa; d) the reaction mixture is cooled by expansion; e) ketone is removed from the reaction mixture using vapor flowing in the opposite direction and; f) the raw product is dried and rid from excessive aldehyde and secondary components via a rectification column
    • 本发明涉及用于生产通式(I)和(I')的假阳离子及其异构体的连续方法,其中:R 1表示CH 3或( 一个); R 2和R 3代表氢,CH 3或C 2 H 5, ,和 R 4和R 5代表氢或CH 3。 这些假性离子是通过使式(II)的醛与过量的通式(III)的酮反应制得的,其中R 1,R 2和R 2 在水和碱金属氢氧化物的存在下,在升高的温度下和均匀的溶液中具有上述含义。 本发明的方法的特征在于:a)由醛,酮和碱性碱液组成的均匀溶液的混合在10至120℃的温度下进行; b)随后将反应混合物中所含的未溶解的水和氢氧化碱分离出来; c)同时避免反混合,然后将均匀的反应混合物引导通过反应器,其允许停留时间为2至300分钟,温度高于最低浓度的沸点为10至120℃, 沸腾成分,并且在10 -6至10 7 Pa范围内的蒸汽压力p; d)反应混合物通过膨胀冷却; e)使用沿相反方向流动的蒸汽从反应混合物中除去酮; f)将原料干燥并通过精馏塔除去过量的醛和次要组分