会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 29. 发明申请
    • Method for making an alloy coated battery grid
    • 制造合金涂层电池网格的方法
    • US20020090554A1
    • 2002-07-11
    • US09755337
    • 2001-01-05
    • Yu-Lin Chen
    • H01M004/74H01M004/68B23P013/00B05D005/12
    • H01M4/745H01M4/20H01M4/667H01M4/685H01M4/73Y10T29/10Y10T29/49108Y10T29/49115
    • A method of forming battery grids or plates that includes the step of applying a lead alloy coating to a continuous strip of interconnected battery grids formed from a lead alloy grid material is disclosed. The battery grids may be formed by a continuous battery grid making process such as strip expansion, strip punching, or continuous grid casting. In one version of the method, the grid wires of a continuous strip of battery grids produced by a punching process are immersed in a melt of the lead alloy coating. In another version of the method, the grid wires of a continuous strip of battery grids produced by a punching process are deformed such that the grid wires have a cross-section other than the rectangular cross-section produced by the punching process and the strip of interconnected grids is immersed in a melt of the lead alloy coating. The method increases the cycle life of a battery.
    • 公开了一种形成电池栅格或板的方法,其包括将铅合金涂层施加到由铅合金网格材料形成的互连电池栅格的连续条带上的步骤。 电池栅格可以通过连续电池网格制作过程形成,例如条带扩张,条带冲压或连续网格铸造。 在该方法的一个版本中,通过冲压工艺生产的连续的电池网格条的网格线浸入铅合金涂层的熔体中。 在该方法的另一种方案中,通过冲压工艺产生的电池网格的连续条带的栅格线变形,使得栅格线具有除穿孔工艺产生的矩形横截面之外的横截面和 互连网格浸入铅合金涂层的熔体中。 该方法增加了电池的循环寿命。
    • 30. 发明授权
    • Lead-acid cells and batteries
    • 铅酸电池和电池
    • US5874186A
    • 1999-02-23
    • US872811
    • 1997-06-11
    • Purushothama RaoThomas F. Uhlemann
    • Purushothama RaoThomas F. Uhlemann
    • C22C11/06H01M4/68H01M4/74
    • H01M4/685C22C11/06H01M4/745
    • A lead-acid cell or battery includes positive plates made from a lead-based alloy containing calcium, tin, and silver in amounts selected based upon the type of application and the plate fabrication method utilized, starting, lighting and ignition battery grids being directly cast and having calcium present in an amount of 0.03% to 0.050%, tin in an amount of 0.65% to 1.25%, and silver in an amount of from 0.018% to 0.030%, and the grids used in sealed, lead-acid cells comprising, when made by gravity casting, from about 0.035% to 0.055% calcium, 0.95% to 1.45% tin, and 0.018% to 0.030% silver, and, when made by continuous strip casting, calcium in the range of from 0.030% to 0.050%, tin in the range of from 0.95% to 1.25%, and silver in the range of from 0.017% to 0.030%, all of the alloy percentages being based upon the total weight of the grid.
    • 铅酸电池或电池包括由包含钙,锡和银的铅基合金制成的正极板,其基于应用的类型和使用的板制造方法选择的量,起始,照明和点火电池网格直接铸造 并且具有0.03%至0.050%的钙,0.65%至1.25%的锡和0.018%至0.030%的量的银,以及用于密封的铅酸电池中的电池,包括 当通过重力铸造制成时,约0.035%至0.055%的钙,0.95%至1.45%的锡和0.018%至0.030%的银,并且当通过连续带铸造制成时,钙在0.030%至0.050的范围内 %,锡在0.95%至1.25%的范围内,银在0.017%至0.030%的范围内,所有合金百分比均基于电网的总重量。