    • Vacuum casting method
    • 真空铸造法
    • US5462107A
    • 1995-10-31
    • US266549
    • 1994-06-28
    • Tamotsu HasegawaYasuyuki ArakawaAtushi Ota
    • Tamotsu HasegawaYasuyuki ArakawaAtushi Ota
    • B22D18/08B22D18/06B22D18/04
    • B22D18/06
    • In a vacuum casting method, a molding cavity is reduced in pressure to a vacuum, and when a gate is opened, a molten metal which has been raised to a molten metal retaining dome is charged into the molding cavity at a high speed. When a portion of a molten metal held in a molten metal holding furnace is raised to the molten metal retaining dome via a stalk, (1) the rising speed of a portion of the molten metal is set at 5-10 cm/sec, or (2) the rising speed is varied between an early stage of the rising motion and a later stage of the rising motion. In the latter method, the rising speed at the early stage of the rising motion is set at a speed higher than 10 cm/sec, while the rising speed at the later stage of the rising motion is set at 5-10 cm/sec. Due to the rising speed control, air involvement by the rising molten metal is effectively prevented.
    • 在真空铸造方法中,模制空腔的压力降低到真空,当打开浇口时,已经升高到熔融金属保持圆顶的熔融金属以高速加入到模腔中。 当保持在熔融金属保持炉中的熔融金属的一部分经由柄杆升高到熔融金属保持拱顶时,(1)将熔融金属的一部分的上升速度设定为5-10cm / sec,或 (2)上升速度在上升运动的早期阶段与上升运动的后期阶段不同。 在后一种方法中,将上升运动的早期阶段的上升速度设定为高于10cm / sec的速度,而将上升运动的后期的上升速度设定为5-10cm / sec。 由于速度控制的上升,有效地防止了上升的熔融金属对空气的影响。