    • 18. 发明申请
    • Conductive primer composition for ambient cure
    • 用于环境固化的导电底漆组合物
    • US20040149960A1
    • 2004-08-05
    • US10357828
    • 2003-02-04
    • Henry Stever Tremper IIIHenry A. Tronco JR.Valentina Gordin
    • B05D003/02H05C001/00
    • C09D175/06C08G18/283C08G18/4202C08G18/4219C08G18/6229C08G18/6295C08G18/792C08K3/013C08K3/04C09D5/24
    • The present invention provides electrically conductive and flexible primer compositions that harden to form conductive materials under room temperature or low bake temperature curing conditions. The primer composition contains solvents and 40-75% by weight of film forming binder and pigments in an overall pigment to binder weight ratio of about 1:100 to 100:100; wherein the binder contains (A) a flexible hydroxy containing polyester resin and (B) an organic polyisocyanate crosslinking agent; and wherein the pigments include electrically conductive pigments in a pigment to binder weight ratio of about 1:100 to 130:100 and the electrically conductive pigments consists essentially of a combination of graphite and conductive carbon black pigments in a graphite to carbon black weight ratio of about 120:1 to 1:1, and the composition forms a hard, flexible coating having a surface conductivity of at least 100 Ransburg units when cured at room temperature or low bake conditions. The coating composition can be used on metal or plastic substrates to render the substrate conductive.
    • 本发明提供在室温或低烘烤温度固化条件下硬化以形成导电材料的导电和柔性底漆组合物。 底漆组合物含有溶剂和40-75重量%的成膜粘合剂和颜料,其总颜料与粘合剂的重量比为约1:100至100:100; 其中所述粘合剂含有(A)含柔性羟基的聚酯树脂和(B)有机多异氰酸酯交联剂; 并且其中所述颜料包括颜料与粘合剂重量比为约1:100至130:100的导电颜料,并且导电颜料基本上由石墨和导电炭黑颜料的组合组成,石墨与炭黑的重量比为 约120:1至1:1,并且当在室温或低烘烤条件下固化时,组合物形成具有至少100兰斯堡单位的表面电导率的硬质柔性涂层。 涂料组合物可用于金属或塑料基材上以使基材导电。