    • Optical recording medium and method for making the same
    • 光记录媒体及其制作方法
    • US06399173B1
    • 2002-06-04
    • US09503171
    • 2000-02-14
    • Mori NagayamaJiro Yoshinari
    • Mori NagayamaJiro Yoshinari
    • B32B302
    • G11B7/268G11B7/24G11B7/243G11B7/2534G11B7/2542G11B7/257G11B7/2585G11B7/26G11B2007/24308G11B2007/2431G11B2007/24314G11B2007/24316Y10T428/21
    • In phase change optical recording media wherein initialization process of the recording layer has been the rate determining and cost-increasing factor in the production of the medium, the production cost is reduced by reducing the time required for the initialization and simplification of the initialization process. Stable writing/reading properties are also realized from immediately after the initialization. The present invention provides an optical recording medium comprising a substrate and a recording layer formed over the substrate, wherein the recording layer comprises two or more unit recording layers wherein adjacent two unit recording layers are constituted from different materials and mixture layers between the two adjacent unit recording layers containing all of the elements included in the adjacent two unit recording layers; at least one of the two adjacent unit recording layers is a crystalline layer; and the overall composition of the recording layer falls within the composition of a phase change recording material.
    • 在其中记录层的初始化处理一直是介质生产中的速率确定和成本增加因素的相变光学记录介质中,通过减少初始化所需的时间并简化初始化过程来降低生产成本。 写入/读取的稳定性也可以从初始化之后立即实现。 本发明提供了一种光记录介质,包括基板和形成在基板上的记录层,其中记录层包括两个或多个单元记录层,其中相邻的两个单元记录层由两个相邻单元之间的不同材料和混合层构成 包含相邻两个单元记录层中包含的所有元素的记录层; 两个相邻单元记录层中的至少一个是晶体层; 并且记录层的总体组成落入相变记录材料的组成之内。
    • 107. 发明授权
    • Hologram recording medium
    • 全息记录介质
    • US08420280B2
    • 2013-04-16
    • US11847819
    • 2007-08-30
    • Jiro YoshinariAtsuko KosudaNaoki Hayashida
    • Jiro YoshinariAtsuko KosudaNaoki Hayashida
    • G03H1/02
    • G03F7/001G03F7/0043
    • The present invention provides a hologram recording medium which can attain high refractive index change, flexibility, high sensitivity, low scattering, environment resistance, durability, low dimension change (low shrinkage) and high multiplicity in holographic memory record using a blue laser. A hologram recording medium (11) comprising at least a hologram recording material layer, wherein the hologram recording material layer (21) comprises at least a metal oxide and a photopolymerizable compound; and said hologram recording medium has a light transmittance of 50% or more at a wavelength of 405 nm, or a light reflectance of 25% or more at a wavelength of 405 nm.
    • 本发明提供一种全息图记录介质,其能够使用蓝色激光获得全息记录记录中的高折射率变化,柔性,高灵敏度,低散射性,耐环境性,耐久性,低尺寸变化(低收缩)和高倍数。 包括至少全息记录材料层的全息记录介质(11),其中全息记录材料层(21)至少包含金属氧化物和可光聚合化合物; 并且所述全息记录介质的波长为405nm时的透光率为50%以上,波长405nm的光反射率为25%以上。
    • 108. 发明授权
    • Hologram recording material, and hologram recording medium
    • 全息记录材料和全息记录介质
    • US08367274B2
    • 2013-02-05
    • US11556813
    • 2006-11-06
    • Jiro YoshinariNaoki Hayashida
    • Jiro YoshinariNaoki Hayashida
    • G03C1/72G03H1/04
    • G03H1/02G03F7/001G03F7/0042G03F7/0757G03H2001/0264G03H2260/12
    • The present invention provides a hologram recording material which attains high refractive index change, flexibility, high sensitivity, low scattering, environment resistance, durability, low shrinkage, and high multiplicity, and is suitable for volume hologram recording. Also, the present invention provides a hologram recording medium. A hologram recording material comprising: an organometallic compound at least containing at least two kinds of metals, oxygen, and an aromatic group, and having an organometallic unit wherein two aromatic groups are bonded directly to one metal; and a photopolymerizable compound containing at least a monofunctional compound (A) having one polymerizable functional group in the molecule. The hologram recording material may comprise, as the photopolymerizable compound, a polyfunctional compound (B) having two or more polymerizable functional groups in the molecule. A hologram recording medium 11 has a hologram recording material layer 21.
    • 本发明提供一种获得高折射率变化,柔韧性,高灵敏度,低散射性,耐环境性,耐久性,低收缩率和高倍数的全息记录材料,适用于体积全息图记录。 此外,本发明提供一种全息记录介质。 一种全息记录材料,包括:至少含有两种金属,氧和芳族基团的有机金属化合物,并且具有有机金属单元,其中两个芳族基团直接键合到一个金属上; 和至少含有分子内具有一个聚合性官能团的单官能化合物(A)的光聚合性化合物。 作为光聚合性化合物,全息记录材料可以包含在分子中具有2个以上聚合性官能团的多官能化合物(B)。 全息记录介质11具有全息记录材料层21。
    • 109. 发明申请
    • HOLOGRAM RECORDING MATERIAL AND HOLOGRAM RECORDING MEDIUM
    • HOLOGRAM记录材料和HOLOGRAM记录介质
    • US20110287343A1
    • 2011-11-24
    • US13107281
    • 2011-05-13
    • Naoki HAYASHIDAKazushi TanakaJiro Yoshinari
    • Naoki HAYASHIDAKazushi TanakaJiro Yoshinari
    • G03F7/00
    • G03F7/001G03F7/027
    • The present invention provides a hologram recording material and a hologram recording medium that can stably maintain the shape of a recording layer and achieve high diffraction efficiency. A hologram recording material comprising a photoradical polymerizable compound (A), a photopolymerization initiator (B), and a dispersion medium (C). The medium (C) is selected from the group consisting of: a compound of the formula (I): wherein R11 is a divalent C2-4 hydrocarbon group, R12 and R13 each independently represent a C1-10 hydrocarbon group, k, l, m and n are each independently a number of 0 or more and 5 or less; and a compound of the formula (II): wherein R21 represents a divalent C1-6 hydrocarbon group, R22 and R23 each independently represent a C1-12 hydrocarbon group, and at least one of R22 and R23 represents a C5-12 hydrocarbon group.
    • 本发明提供一种可以稳定地保持记录层的形状并实现高衍射效率的全息记录材料和全息记录介质。 包含光自由基聚合性化合物(A),光聚合引发剂(B)和分散介质(C)的全息记录材料。 介质(C)选自:式(I)化合物:其中R 11是二价C 2-4烃基,R 12和R 13各自独立地表示C 1-10烃基,k,l, m和n各自独立地为0以上且5以下的数; 和式(II)的化合物:其中R21表示二价C1-6烃基,R22和R23各自独立地表示C1-12烃基,R22和R23中的至少一个表示C5-12烃基。
    • 110. 发明授权
    • Hologram recording material, process for producing the same and hologram recording medium
    • 全息记录材料,其制造方法和全息记录介质
    • US08021800B2
    • 2011-09-20
    • US12109000
    • 2008-04-24
    • Atsuko KosudaNaoki HayashidaJiro Yoshinari
    • Atsuko KosudaNaoki HayashidaJiro Yoshinari
    • G03H1/02
    • G03F7/001G03F7/0042G03F7/0043
    • The present invention provides a hologram recording material which is suitable for volume hologram record and attains high refractive index change, flexibility, high sensitivity, low scattering, environment resistance, durability, low shrinkage and high multiplicity in holographic memory record using not only a green laser but also a blue laser; a process for producing the same; and a hologram recording medium having the hologram recording material. A hologram recording material comprising: a metal oxide containing at least Si and Zr as metals, wherein an aromatic carboxylic acid compound is coordinated to Zr; and a photopolymerizable compound. The aromatic carboxylic acid compound is, for example, toluic acid. A hologram recording medium (11) comprising the hologram recording material layer (21).
    • 本发明提供一种全息记录材料,其适用于体积全息记录,并且在全息记录记录中不仅使用绿色激光,而且获得高折射率变化,柔性,高灵敏度,低散射,环境耐久性,耐久性,低收缩率和高倍数 也是一个蓝色激光; 其制造方法; 以及具有全息图记录材料的全息图记录介质。 一种全息记录材料,包括:至少含有Si和Zr作为金属的金属氧化物,其中芳族羧酸化合物与Zr配位; 和光聚合性化合物。 芳族羧酸化合物是例如甲苯甲酸。 包括全息记录材料层(21)的全息记录介质(11)。