热词
    • 10. 发明授权
    • Magnetooptic recording medium and its manufacturing method
    • 磁光记录介质及其制造方法
    • US07173884B2
    • 2007-02-06
    • US10482424
    • 2002-05-14
    • Yutaka WadaHiroshi Nakayama
    • Yutaka WadaHiroshi Nakayama
    • G11B11/00B32B3/02
    • G11B11/10586G11B7/00
    • A first dielectric layer 3, a multilayer magnetic film 10 in which a first magnetic layer 4 having perpendicular magnetic anisotropy at room temperature, a second magnetic layer 5 having inplane magnetic anisotropy at room temperature, and a third magnetic layer 6 having perpendicular magnetic anisotropy at room temperature are sequentially laminated, a second dielectric layer 7, a reflective layer 8, and a protective layer 9 are sequentially laminated onto one principal plane of a disk substrate 2 on which a land and a groove exist, thereby forming a magnetooptic disk 1. Saturation magnetization of the second magnetic layer 5 is set to a range from 8.80×10−2 to 1.76×10−1 Wb/m2. A gas pressure upon film creation of the second magnetic layer is set to a range from 0.6 to 3.0 Pa. A content ratio of Co in the third magnetic layer 6 is set to a range from 15 to 17 atom %.
    • 第一电介质层3,其中在室温下具有垂直磁各向异性的第一磁性层4,室温下具有平面磁各向异性的第二磁性层5和具有垂直磁各向异性的第三磁性层6的多层磁性膜10 依次层压室温,第二电介质层7,反射层8和保护层9依次层叠在其上存在焊盘和凹槽的盘基板2的一个主平面上,从而形成磁光盘1。 第二磁性层5的饱和磁化强度设定在8.80×10 -2至1.76×10 -1 Wb / m 2范围内。 将第二磁性层成膜时的气体压力设定为0.6〜3.0Pa的范围,将第三磁性层6中的Co含量比设定为15〜17原子%。