    • KR101845530B1
    • 2018-04-04
    • KR1020160122229
    • 2016-09-23
    • 에스케이씨 주식회사
    • 이장원허영민강호천정다우이세철
    • G02B5/28G02B5/22
    • 본발명은색상조절이가능한윈도우용열차단필름에관한것이다. 구체적으로는굴절율이 1.6 내지 1.7인고굴절층과굴절율이 1.48 내지 1.50인저굴절층을교대로적층하여적외선을반사할수 있고, 상기고굴절층과저굴절층의굴절율비대 두께비를 1.1 내지 1.3으로조절하여가시광선을반사시킴으로써특정한색상을구현할수 있는열차단필름에관한것이다. 나아가굴절율비대 두께비를유지하면서상기고굴절층과저굴절층의두께를조절하여반사되는가시광선의파장대역을조절함으로써구현되는색상을자유롭게변경할수 있는열차단필름에관한것이다.
    • 本发明涉及一种用于窗户的可调色的热遮光膜。 具体来说euroneun它可以是1.6至1.7锭折射率层的折射率和折射率交替地层叠1.48〜1.50变换器折射层反射红外辐射,通过控制的高折射率层的肥大厚度比和低折射率层的折射率为1.1至1.3,所述可见光 哪个能够实现特定的颜色。 此外,在保持的肥大厚度比折射率涉及高折射率层,并且可以自由地改变其是通过控制可见光的波长带被反射控制低折射率层的厚度实现的颜色的热阻挡膜。
    • 8. 发明公开
    • 단층 PVdF 필름 및 이의 제조방법
    • 单层PVDF薄膜及其制备方法
    • KR1020130006410A
    • 2013-01-16
    • KR1020120153817
    • 2012-12-26
    • 에스케이씨 주식회사
    • 이중규강호천정상윤이용래
    • C08J5/18C08L27/16C08J3/22H01L31/042
    • Y02E10/50C08J5/18C08J3/22C08L27/16H01L31/042
    • PURPOSE: A manufacturing method of a polyvinylidene fluoride film is provided to provide a polyvinylidene fluoride film with excellent weatherability, heat resistance, scratch resistance and dimensional stability. CONSTITUTION: A manufacturing method of a polyvinylidene fluoride film comprises: a step of manufacturing a master batch by compounding a polymethylmethacrylate homopolymer resin or a copolymer resin thereof, and titanium oxide(TiO2); and a step of melting and rolling the master batch, and a polyvinylidene fluoride homopolymer resin or a copolymer resin thereof and extruding the same to a sheet. The concentration of the polymethylmethacrylate homopolymer resin or copolymer resin thereof, the polyvinylidene fluoride single resin or copolymer resin thereof, and titanium oxide are 50-90 weight%, 5-25 weight% and 5-25 weight%, respectively.