    • 유로피엄을 함유한 티탄산 비스무스 강유전 물질
    • 含有具有高残留极化值,低介电损耗性能的双晶硅酸钛铁氧体材料的欧元,以及对疲劳的极好耐用性
    • KR1020050009777A
    • 2005-01-26
    • KR1020030048600
    • 2003-07-16
    • 심일운김창일
    • 심일운김창일강동희정한철김경태
    • C01G23/04
    • C01G29/006C01F17/0012C01G23/003C01P2006/40
    • PURPOSE: A europium containing bismuth titanate ferroelectric material is provided, which has a high residual polarization value, a low dielectric loss property, and an excellent endurance against fatigue. CONSTITUTION: The europium containing bismuth titanate ferroelectric material represented by the formula 1 is produced by a process comprising the steps of: dissolving a europium containing compound, a bismuth containing compound, and a titanium containing compound in the molar ratio of x:4-x:3(x is 0.2-0.9) in a common solvent to prepare a precursor solution stable in the air; preparing a thin film by using the precursor solution by a spin coating method; drying and calcining the thin film. In the formula, x is 0.2-0.9.
    • 目的:提供含有铋钛酸铁铁氧体材料,其具有高残留极限值,低介电损耗特性和耐疲劳耐久性。 构成:由式1表示的含铋钛酸铁电材料的制造方法包括以下步骤:将含铕化合物,含铋化合物和含钛化合物以x:4-x :3(x为0.2-0.9)在常规溶剂中制备在空气中稳定的前体溶液; 通过旋涂法使用前体溶液制备薄膜; 干燥和煅烧薄膜。 在式中,x为0.2-0.9。