热词
    • 6. 发明公开
    • 자기열효과물질 미세 분말 및 자기열효과물질 소재의 제조방법
    • 生产磁铁效应粉末和磁铁效应材料的方法
    • KR1020130000969A
    • 2013-01-03
    • KR1020110061801
    • 2011-06-24
    • 삼성전자주식회사코쿠리츠켄큐카이하츠호징 붓시쯔 자이료 켄큐키코
    • 권순재다케노리누마자와안경한김현식
    • C09K5/14C09K5/00
    • PURPOSE: A manufacturing method of a magnetocaloric material is provided to reduce heat-treatment temperature by using a halogenated metal as a metal source and to control the growth of magnetocaloric material particles. CONSTITUTION: A manufacturing method a magnetocaloric material comprises: a step(S110) of forming a mixture by mixing a source material of one or more metal selected from manganese halide, halide iron, B, Si, Ge, As, Sb and Te, phosphor and a reducing metal to form a mixture; a step(S120) of heat-treating the mixture; and a step(S130) of cooling the heat-treated mixture. The manganese halide is manganese chloride (II), manganese chloride (III), manganese bromide (II), manganese fluoride (III), manganese fluoride (IV) or manganese iodine (II). [Reference numerals] (S110) Mixture of mixing manganese halide, iron halide, phosphor, T, and reducing metals; (S120) Heating and melting the mixture at 750-1000°C; (S130) Cooling; (S140) Washing
    • 目的:提供一种磁热材料的制造方法,以通过使用卤化金属作为金属源来降低热处理温度并控制磁热材料颗粒的生长。 构成:磁热材料的制造方法包括:通过混合选自卤化锰,卤化铁,B,Si,Ge,As,Sb和Te中的一种或多种金属的源材料形成混合物的步骤(S110),荧光体 和还原金属形成混合物; 对该混合物进行热处理的工序(S120) 和冷却经过热处理的混合物的工序(S130)。 卤化锰是氯化锰(II),氯化锰(III),溴化锰(II),氟化锰(III),氟化锰(IV)或锰碘(II)。 (S110)混合卤化锰,卤化铁,磷,T和还原金属的混合物; (S120)在750-1000℃下加热和熔化混合物; (S130)冷却; (S140)洗涤
    • 10. 发明公开
    • 소결자석 제조 방법
    • 制备烧结磁体的方法
    • KR1020150073759A
    • 2015-07-01
    • KR1020130161813
    • 2013-12-23
    • 삼성전자주식회사
    • 문경석강영민강영재안경한이상목이제현조근우
    • H01F41/02
    • 원료혼합물을얻는단계; 상기원료혼합물을 900도씨내지 1350도씨의온도에서하소하여, 하기일반식 1로나타내어지는 M-타입헥사페라이트또는하기일반식 2로나타내어지는 W-타입헥사페라이트를포함하는입자들을포함하는하소생성물을얻는단계; [일반식 1] ARFeMO여기서, A는 Sr, Ba, 및 Ca로부터선택된 1종이상이고, R은희토류원소로부터선택된 1종이상이고, M은 Co, Mn, Zn, Zr, Ni, Ti, Cu, Al, Ge, 및 As로부터선택된 1종이상이고, 0 ≤ x ≤ 0.6, 0 ≤ y ≤ 1.2 임; [일반식 2] AMeFeO여기서, A는 Sr, Ba, 및 Ca 로부터선택된선택된 1종이상이고, Me는 Co, Cu, Zn, Mn, ZrNi, Ti, Al, Ge, 및 As로부터선택된 1종이상이고, x 는 0 내지 2의수임; 상기하소생성물을 CoO, CoO, CoO, MnO, MnO, 및 BiO로부터선택된 1종이상의소결조제와혼합하여혼합물을얻는단계; 상기혼합물을압력하에성형하여성형체를얻는단계; 및상기성형체를 1000도씨내지 1300도씨의온도에서열처리하여소결자석을얻는단계를포함하는소결자석제조방법이제공된다.
    • 本发明涉及一种烧结磁体的制造方法。 根据本发明,提供了一种制造烧结磁体的方法,包括以下步骤:获得原料混合物; 通过在900〜1350摄氏度的温度下烧结原料混合物获得烧结产品; 通过将烧结产物与选自CoO,Co 2 O 4,Co 3 O 4,Mn 2 O 3,Mn 3 O 4和Bi 2 O 3中的一种或多种烧结助剂混合来获得混合物; 通过在压力下形成混合物获得成形体; 通过在1000〜1300℃的温度下对成形体进行热处理而获得烧结磁体。 本发明的一个实施方案涉及制造高密度和改善磁性的六铁氧体烧结磁体的方法。