    • 22. 发明公开
    • 열전도도가 향상된 알루미늄 합금 및 이를 이용한 방열장치
    • 铝合金改进的热传导率和使用其的热辐射装置
    • KR1020140069754A
    • 2014-06-10
    • KR1020120137423
    • 2012-11-29
    • 현대자동차주식회사
    • 김병수
    • C22C21/02
    • C22C21/02B22D17/00C01P2006/32C22C2202/00
    • The present invention relates to an aluminum alloy with improved heat conductivity and a heat radiating device using the same and, more specifically, to an aluminum alloy with improved heat conductivity and a heat radiating device using the same capable of having increased heat conductivity compared to the conventional aluminum alloy and of being applied with a die casting method. The aluminum alloy with improved heat conductivity consists of aluminum as a basic material and, based on the total weight of alloy, 2.5-4.5 wt% of silicone (Si), 0.25-0.35 wt% of magnesium (Mg), 0.1-1.0 wt% of iron (Fe), 0.2-0.5 wt% of nickel (Ni), and inevitable impurities.
    • 本发明涉及一种具有改善的导热性的铝合金和使用该铝合金的散热装置,更具体地说,涉及一种具有改善的导热性的铝合金和一种使用该铝合金的散热装置,该散热装置能够与 常规铝合金,并应用压铸方法。 具有改善的导热性的铝合金由铝作为基础材料组成,基于合金的总重量,2.5-4.5重量%的硅氧烷(Si),0.25-0.35重量%的镁(Mg),0.1-1.0重量% 铁(Fe),0.2-0.5重量%的镍(Ni)和不可避免的杂质。
    • 24. 发明公开
    • 내 변색성 및 다색의 8캐럿 금 합금
    • 8卡拉特金合金耐火和各种颜色
    • KR1020140001017A
    • 2014-01-06
    • KR1020120069251
    • 2012-06-27
    • 주식회사 삼양귀금속거래소
    • 이기식
    • C22C5/02C22C30/02
    • C22C30/02C22C1/02C22C5/02C22C9/00C22C30/04C22C30/06C22C2202/00
    • A composition of an 8 karat gold alloy having for discoloration resistance and various colors according to the present invention is as follows. A composition of a gold-colored gold alloy comprises 33.34 wt% of Au, 10-20 wt% of Ag, 30-50 wt% of Cu, 5-15 wt% of Zn, 0.5-3.0 wt% of Pd, 0.01-0.2 wt% of Ir, 0.01-0.1 wt% of Rh, 0.01-0.1 wt% of Ru, 0.01-0.50 wt% of Ge or Nd, and unavoidable impurities. A composition of a white-colored gold alloy comprises 33.34 wt% of Au , 20-40 wt% of Ag, 5-10 wt% of Cu, 20-30 wt% of Zn, 1.0-30 wt% of Pd, 0.01-0.2 wt% of Ir, 0.01-0.1 wt% of Rh, 0.01-0.1 wt% of Ru, 0.01-0.50 wt% of Ge or Nd, and unavoidable impurities. A composition of a pink-colored gold alloy comprises 33.34 wt% of Au, 10-20 wt% of Ag, 40-60 wt% of Cu, 1-5 wt% of Zn, 0.5-3.0 wt% of Pd, 0.01-0.2 wt% of Ir, 0.01-0.1 wt% of Rh, 0.01-0.1 wt% of Ru, 0.01-0.50 wt% of Ge or Nd, and unavoidable impurities. The oxidation of volatile base metal such as Zn is actively prevented as a smelting atmosphere is controlled with vacuum or argon gas by using a vacuum high-frequency smelting furnace so that gold alloys having various colors are manufactured. Ingots of the gold alloys are cold-rolled after annealing by thermally treating at high temperatures so that a thin plate or a product of a granule form is manufactured.
    • 根据本发明的具有耐变色性和各种颜色的8克拉金合金的组合物如下。 金色金合金的组成包含金属为33.34重量%,Ag为10-20重量%,Cu为30-50重量%,Zn为5-15重量%,Pd为0.5-3.0重量%,0.01〜 Ir的0.2重量%,Rh的0.01-0.1重量%,Ru的0.01-0.1重量%,Ge或Nd的0.01-0.50重量%和不可避免的杂质。 白色金合金的组成包含金属为33.34重量%,Ag为20-40重量%,Cu为5-10重量%,Zn为20-30重量%,Pd为0.01〜 Ir的0.2重量%,Rh的0.01-0.1重量%,Ru的0.01-0.1重量%,Ge或Nd的0.01-0.50重量%和不可避免的杂质。 粉红色金合金的组成包含金属为33.34重量%,Ag为10-20重量%,Cu为40-60重量%,Zn为1-5重量%,Pd为0.5-3.0重量%,0.01〜 Ir的0.2重量%,Rh的0.01-0.1重量%,Ru的0.01-0.1重量%,Ge或Nd的0.01-0.50重量%和不可避免的杂质。 通过使用真空高频熔炼炉通过真空或氩气控制冶炼气氛,可以有效地防止挥发性碱金属如Zn的氧化,从而制造出具有各种颜色的金合金。 通过在高温下进行热处理,在金属合金的锭之后进行冷轧,从而制造薄板或颗粒状产品。
    • 25. 发明公开
    • 고강도 메탈베어링용 알루미늄 합금 및 이를 이용하여 제조된 고강도 메탈베어링
    • 高强度金属轴承铝合金和使用其制造的高强度金属轴承的复合材料
    • KR1020130117310A
    • 2013-10-25
    • KR1020120040495
    • 2012-04-18
    • 현대자동차주식회사
    • 김한재
    • C22C21/00C22C21/10C22C21/02
    • C22C21/10C22C2202/00F16C33/121F16C2204/20
    • PURPOSE: An aluminum alloy for a high strength metal bearing and the high strength metal bearing manufactured by the same are provided to have excellent strength and equivalent wear resistance in comparison with an Al-Sn alloy. CONSTITUTION: An aluminum alloy for a high strength metal bearing is composed of 4-10 wt.% of Zn, 0.1-5 wt.% of Si, 0.1-2 wt.% of Cu, 0.2-2 wt.% of Sn, and the rest of Al and inevitable impurities. The high strength metal bearing is formed of the aluminum alloy. The aluminum alloy is composed of soft particles for reducing the coefficient of friction in a microstructure; and hard particles for increasing wear resistance. The soft particles are the Zn and the Sn. The hard particles are the Si and ZnCu. [Reference numerals] (11) Steel layer; (12) Junction layer; (13) Alloy layer; (AA) Construct bearing members
    • 目的:提供一种用于高强度金属轴承的铝合金和由其制造的高强度金属轴承,与Al-Sn合金相比具有优异的强度和相当的耐磨性。 构成:用于高强度金属轴承的铝合金由4-10重量%的Zn,0.1-5重量%的Si,0.1-2重量%的Cu,0.2-2重量%的Sn, 其余的Al和不可避免的杂质。 高强度金属轴承由铝合金制成。 铝合金由用于降低微结构中的摩擦系数的软颗粒组成; 和用于增加耐磨性的硬质颗粒。 软颗粒是Zn和Sn。 硬颗粒是Si和ZnCu。 (11)钢层; (12)结层; (13)合金层; (AA)构造轴承成员
    • 27. 发明公开
    • 하이드로 포밍용 알루미늄 합금관 및 그 제조방법
    • 用于水压成型的铝合金的制造方法
    • KR1020130113814A
    • 2013-10-16
    • KR1020120036316
    • 2012-04-06
    • 현대하이스코 주식회사
    • 박성필김윤규
    • C22C21/06B21C23/08C21D8/10
    • C22C21/08B21C23/08C22C1/10C22C2202/00C22F1/047
    • PURPOSE: An aluminum alloy pipe for hydro forming is proper to a hydro forming process, thereby being utilized for manufacturing vehicle components of various shapes. CONSTITUTION: A method for manufacturing an aluminum alloy pipe for hydro forming includes the following steps of: preparing a billet of an aluminum alloy comprising 0.09-0.45 wt% of Si, 0.11-0.24 wt% of Fe, 0.02 wt% or less of Cu, 0.02-0.76 wt% of Mn, 2.7-4.1 wt% of Mg, 0.11-0.25 wt% of Cr, 0.003-0.014 wt% of Zn, 0.021-0.0031 wt% of Ti, and the rest of Al and unavoidable impurities; and extrusion-processing the billet into a pipe shape by using a die after homogenization-processing the billet. [Reference numerals] (S-12) Step of preparing a billet; (S-14) Step of homogenization; (S-16) Step of extruding; (S-18) Step of annealing and heat treatment
    • 目的:用于加氢成型的铝合金管适用于水压成型工艺,用于制造各种形状的车辆部件。 构成:用于制造用于加氢成型的铝合金管的方法包括以下步骤:制备铝合金坯料,其包含0.09-0.45重量%的Si,0.11-0.24重量%的Fe,0.02重量%以下的Cu ,Mn:0.02〜0.76重量%,Mg:2.7〜4.1重量%,Cr:0.11〜0.25重量%,Zn:0.003〜0.014重量%,Ti:0.021-0.0031重量%,Al余量和不可避免的杂质; 并在坯料均质化处理之后通过使用模具将坯料挤压加工成管状。 (S-12)准备坯料的工序; (S-14)均质步骤; (S-16)挤出步骤; (S-18)退火和热处理步骤
    • 28. 发明公开
    • 고비중 및 고강도 Mg―Cr계 내화재 및 그 제조방법
    • 具有高特异度和强度的MG-CR型耐火材料及其制造方法
    • KR1020130098528A
    • 2013-09-05
    • KR1020120020114
    • 2012-02-28
    • (주)포스코켐텍
    • 이동하
    • C22C23/00
    • C22C23/00C22C1/00C22C2202/00
    • PURPOSE: A Mg-Cr based refractory material with high specific gravity and strength and a manufacturing method thereof are provided to minimize dust generation and improve workability because a water addition process is not necessary in a construction. CONSTITUTION: A Mg-Cr based refractory material with high specific gravity and strength comprises 65-80 weight% of a Mg-Cr material having a particle size of 0.1-3 mm, 20-35 weight% of a Mg-Cr material having a particle size less than 0.1 mm, other unavoidable impurities, and 4-8 parts by weight of a liquid binder relative to 100 parts by weight of a Mg-Cr base material. The Mg-Cr base material comprises 50-60 weight% of MgO, 5-10 weight% of Al2O3, less than 2 weight% of CaO, 1-3 weight% of SiO2, 5-10 weight% of Fe2O3, 15-25 weight% of Cr2O3, and other unavoidable impurities. The Mg-Cr base material is a crushed waste refractory material. The liquid binder comprises one or more kinds of oils among vegetable oils and animal oils.
    • 目的:提供一种具有高比重和强度的Mg-Cr系耐火材料及其制造方法,以便在施工中不需要添加水的工序,以使粉尘产生最小化,提高加工性。 构成:具有高比重和强度的Mg-Cr基耐火材料包含65-80重量%的粒径为0.1-3mm的Mg-Cr材料,20-35重量%的具有 粒径小于0.1mm,其它不可避免的杂质,相对于100重量份的Mg-Cr基材料为4-8重量份的液体粘合剂。 Mg-Cr基材包含50-60重量%的MgO,5-10重量%的Al 2 O 3,少于2重量%的CaO,1-3重量%的SiO 2,5-10重量%的Fe 2 O 3,15-25 重量%的Cr2O3和其他不可避免的杂质。 Mg-Cr基材料是粉碎的废弃耐火材料。 液体粘合剂包括植物油和动物油中的一种或多种油。