    • 1. 发明专利
    • Stretch spun fiber product having excellent shape stability and method for producing the same
    • 具有良好形状稳定性的弹力纤维制品及其制造方法
    • JP2005120524A
    • 2005-05-12
    • JP2003357466
    • 2003-10-17
    • Toyobo Co Ltd東洋紡績株式会社
    • NAKAMURA RYOJIYOSHIKAWA MASATOSHI
    • A41B1/00A41D1/18A41D31/00D03D15/00D03D15/08D04B1/16D06M13/127D06M23/00D06M101/06D06M101/20
    • PROBLEM TO BE SOLVED: To provide a stretch spun fiber product composed of a fabric having excellent chemical resistance and high recovery, and also having excellent shape stability; and to provide a method for producing the fiber product.
      SOLUTION: The woven or knitted fabric comprises a crosslinked polyolefin elastic fiber and a cellulosic staple fiber, and has ≥15% constant load elongation, 50% recovery from the elongation, and grade ≥3 rating in wrinkle judgement after laundry. The fiber product composed of the woven or knitted fabric is produced by weaving or knitting a composite yarn comprising the cellulosic staple fiber having ≤50 wt.% cellulose type I crystalline structure based on the whole crystal, and the elastic fiber, subjecting the woven or knitted fabric to a crosslinking treatment by a vapor-phase formalin processing method so that the content of the formalin bonded to the cellulose may be ≥0.5 wt.%.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:提供一种由具有优异的耐化学性和高回收率的织物组成的拉伸纺丝纤维产品,并且还具有优异的形状稳定性; 并提供一种纤维制品的制造方法。 纺织品或针织物包含交联聚烯烃弹性纤维和纤维素短纤维,并且具有≥15%的恒定负荷伸长率,50%的伸长恢复率和洗衣后的皱纹判断​​中的≥3等级。 由编织物或针织物构成的纤维制品通过编织或编织包含基于整个晶体的≤50重量%的纤维素型I晶体结构的纤维素短纤维和弹性纤维,使织物或织物 针织物通过气相福尔马林加工方法进行交联处理,使得与纤维素结合的福尔马林的含量可以≥0.5重量%。 版权所有(C)2005,JPO&NCIPI
    • 2. 发明专利
    • Molded article
    • 模制品
    • JP2007023399A
    • 2007-02-01
    • JP2005204577
    • 2005-07-13
    • Toyobo Co Ltd東洋紡績株式会社
    • NISHIDA SUKEHIROYOSHIKAWA MASATOSHI
    • D06M15/39A43B3/10A43B23/02D06M15/55D06M15/564D06M101/06
    • PROBLEM TO BE SOLVED: To provide a molded article such as lampshade or slipper, in which a cellulosic fiber is combined with other fiber, enabling home washing without problem of deformation and wrinkle.
      SOLUTION: The molded article is obtained by applying resin finish to a woven or knitted fabric containing a cellulosic fiber in a weight ratio of at least 30 wt.% based on fiber material by using a resin capable of crosslinking a cellulose molecule, e.g. a glyoxal-based resin and molding the resin-finished material into a prescribed shape by a shaping method by heating, and the molded article satisfies a specific W&W property, dimensional stability and color fastness to light.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供诸如灯罩或拖鞋的模制品,其中纤维素纤维与其它纤维组合,使得能够进行家庭洗涤而没有变形和皱纹的问题。 解决方案:通过使用能够交联纤维素分子的树脂,将纤维素纤维的重量比至少为30重量%的纤维素纤维的编织物或针织物施加到模制品上来获得模制品, 例如 乙二醛类树脂,通过加热成形法将树脂成品成型为规定形状,成型品满足W&W特性,尺寸稳定性和耐光色牢度。 版权所有(C)2007,JPO&INPIT
    • 4. 发明专利
    • hat
    • 帽子
    • JP2007063707A
    • 2007-03-15
    • JP2005250849
    • 2005-08-31
    • Kinokawa Seibo:KkToyo Senshoku Kogyo KkToyobo Co Ltd東洋染色工業株式会社東洋紡績株式会社株式会社紀之川製帽
    • NISHIDA SUKEHIROYOSHIKAWA MASATOSHIARITAKI MUNESHIGEOKAZAKI NOBUHISAMORIOKA YOSHIYASU
    • A42C1/00A42B1/04
    • PROBLEM TO BE SOLVED: To enable house washing of a hat in which cellulosic fiber is combined with other fiber without causing problems such as dimensional change, deformation and attachment of wrinkle. SOLUTION: In the hat, a woven or knitted fabric containing a cellulosic fiber is used in an amount of ≥30 wt.% based on weight of fiber material and the woven or knitted fabric is formed in a prescribed shape by shaping method by heating after applying resin finishing. The hat satisfies the following items. W&W evaluation: higher than 3.0 class; dimensional change ratio: ≥-3.0% and ≤+3.0%; color fastness to light: ≥3 class. The hat is obtained by applying a resin finishing agent containing at least one kind of compound selected from a group consisting of formaldehyde, glyoxal, glutaraldehyde, diglycidyl ether, tetrabutanecarboxylic acid, dimethylolurea, trimethylol melamine, dimethylolethyleneurea and dimethyloldihydroxyethyleneurea to a hat member and drying the hat member and then heat-forming the hat member. COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了使纤维素纤维与其它纤维组合的帽子能够进行房屋清洗,而不会引起诸如尺寸变化,变形和褶皱附着等问题。

      解决方案:在帽子中,使用含有纤维素纤维的编织物或针织物,其量基于纤维材料的重量为≥30重量%,并且织造或针织织物通过成型方法形成为规定的形状 采用树脂精加工后进行加热。 帽子满足以下条件。 W&W评估:高于3.0级; 尺寸变化率:≥-3.0%和≤+ 3.0%; 耐色牢度:≥3级。 帽子是通过将具有至少一种选自甲醛,乙二醛,戊二醛,二缩水甘油醚,四丁烷羧酸,二羟甲基脲,三羟甲基三聚氰胺,二羟甲基亚乙基脲和二羟甲基二羟基亚乙基脲的化合物的树脂整理剂施加到帽子上并将其干燥 帽子部件,然后热成形帽子部件。 版权所有(C)2007,JPO&INPIT

    • 6. 发明专利
    • Vegetable matter, product comprising the same and manufacturing process for vegetable matter
    • 蔬菜制品,包装食品,蔬菜制造工艺
    • JP2004168041A
    • 2004-06-17
    • JP2003367184
    • 2003-10-28
    • Toyobo Co Ltd東洋紡績株式会社
    • YOSHIKAWA MASATOSHI
    • B27K9/00
    • PROBLEM TO BE SOLVED: To provide a stable vegetable matter, which can maintain initial characteristics such as hygroscopicity, texture, aroma and appearance for a long period, which are the characteristics of a product made of the vegetable matter and prevent occurrence of deformation by laundry or washing, discoloration and nasty smell, a product comprising the vegetable matter, and a manufacturing process for the vegetable matter.
      SOLUTION: The vegetable matter is treated with a crosslinking agent in a crosslinking reaction to prevent from degradation in the initial qualities, such as, moisture content, bulk density and brightness. The product comprising the vegetable matter is provided.
      COPYRIGHT: (C)2004,JPO
    • 待解决的问题:提供一种稳定的植物性物质,其可以长期保持诸如吸湿性,质地,香气和外观的初始特性,这是由植物物质制成的产品的特征并且防止发生 通过洗衣或洗涤变形,变色和令人讨厌的气味,包含植物物质的产品以及植物物质的制造过程。 解决方案:在交联反应中用交联剂处理植物物质,以防止初始品质如水分含量,体积密度和亮度的降解。 提供了包含植物物质的产品。 版权所有(C)2004,JPO