    • 1. 发明专利
    • Method and apparatus for molding photocurable material
    • 用于模塑可光材料的方法和装置
    • JP2012176591A
    • 2012-09-13
    • JP2011041862
    • 2011-02-28
    • Toshiba Mach Co Ltd東芝機械株式会社
    • KITAHARA HIDETOSHIHASHIMOTO YUKIOMAGARI HIROAKINISHIHARA HIROMI
    • B29C39/44B29C39/02
    • PROBLEM TO BE SOLVED: To provide a molding method for photocurable material that can drop out generation of hardened unevenness in photocurable material and harden photocurable material efficiently without exception when the molding object of photocurable material is molded using upper and lower dies including materials, such as metals and the like.SOLUTION: The photocurable material 11 is supplied to at least either an upper die 7 or a lower die 9 including a materials of protection from light, such as ultraviolet rays, and the upper die 7 is moved closer to the lower die 9 for positioning, whereas light UR emitted from light sources 19A and 19B outside the upper die 7 and the lower die 9 is radiated, through turning the path, to the photocurable material 11 placed between the upper die 7 and the lower die 9.
    • 要解决的问题:提供一种光固化材料的成型方法,其可以在光固化材料中产生硬化不均匀并且在使用包括材料的上模和下模成型光固化材料的成型对象时有效地硬化光固化材料 ,如金属等。 解决方案:将光固化材料11供给到包括防紫外线等光的材料的上模7或下模9中的至少一个,上模7更靠近下模9移动 用于定位,而从上模7和下模9之外的光源19A和19B发射的光UR通过转动路径被辐射到放置在上模7和下模9之间的光固化材料11.

      版权所有(C)2012,JPO&INPIT

    • 5. 发明专利
    • Device and method for joining faces
    • 用于接合面的装置和方法
    • JP2003015007A
    • 2003-01-15
    • JP2001198832
    • 2001-06-29
    • Toshiba Mach Co Ltd東芝機械株式会社
    • NISHIHARA HIROMIFUJIWARA SHIGERU
    • G02B7/02G03B5/00G03B5/06
    • PROBLEM TO BE SOLVED: To provide a faces joining device and a faces joining method capable of improving faces joining accuracy and expanding types of available components.
      SOLUTION: The faces joining device, for making one component of a face joining object confront the other component of a face joining object and joining the faces for face joining of the both components, is provided with a lifting and lowering holding mechanism 2 for holding the one component of a face joining object in a vertically movable way, a gimbal mechanism 7 for holding the other component of a face joining object around a turning center 8 in a freely turnable way, a level adjustment holder 13 for holding the other component of a face joining object so as to confront the one component of a face joining object, and a vertical movement guide mechanism 14 for moving the other component of a face joining object held by the level adjustment holder vertically so that the height level of the face for face joining of the other component of a face joining object can meet the turning center of the gimbal mechanism in accordance with the length of the other component of a face joining object.
      COPYRIGHT: (C)2003,JPO
    • 要解决的问题:提供一种能够改善面接合精度和扩大可用部件类型的面接合装置和面接合方法。 解决方案:面接合装置设置有用于使面接合对象的一个​​部件与面接合对象的另一部件接合并且接合用于两部件的面接合的面的面接合装置,具有用于保持 以可垂直移动的方式接合物体的一个部件,用于以可自由转动的方式将转接中心8的面接合物体的另一部件保持的万向接头机构7,用于保持另一部件的液位调节保持器13 面接合对象,以面对面接合对象的一个​​部件;以及垂直移动引导机构14,用于垂直移动由平面调节支架保持的面接合对象的另一部分,使得面部的面部的高度水平 面接合对象的其他部件的接合可以根据面接合对象的另一部件的长度来满足万向节机构的转动中心 ct。
    • 6. 发明专利
    • Molding method for molding, and molding
    • 成型和成型的成型方法
    • JP2012176592A
    • 2012-09-13
    • JP2011041868
    • 2011-02-28
    • Toshiba Mach Co Ltd東芝機械株式会社
    • NISHIHARA HIROMIKITAHARA HIDETOSHIHASHIMOTO YUKI
    • B29C39/24B29C39/10B29C59/02B29C59/18B29L11/00
    • PROBLEM TO BE SOLVED: To provide a molding method, etc. for a molding which has a pattern corresponding to a molding pattern formed in a mold without directly contacting the mold and a molding material.SOLUTION: A substrate 3 for molding, which has elasticity and is formed in a plate-like shape, is arranged on the right face of the mold 11 where the molding pattern 13 is formed, and air is passed into the mold 11, so that the substrate 3 for molding is vacuum adsorbed to be elastically deformed, the substrate 3 for molding is made to follow in the shape of the molding pattern 13 of the mold 11, the molding material 5 is supplied onto the right face of the substrate 3 for molding, the molding material 5 is cured, and the substrate 3 for molding is released from the mold 11 together with the cured molding material 5.
    • 要解决的问题:为了提供具有对应于模具中形成的模制图案的图案的模制件的模制方法,而不直接接触模具和模制材料。 解决方案:具有弹性并形成为板状的成型用基板3配置在模具11的形成有模制图案13的右面上,空气通入模具11 ,使得用于成型的基板3被真空吸附而弹性变形,使成型用基板3成为模具11的成形图案13的形状,将成型材料5供给到 用于成型的基板3,成型材料5固化,并且用于模制的基板3与固化的模制材料5一起从模具11中释放。(C)2012,JPO&INPIT
    • 8. 发明专利
    • Glass element molding device
    • 玻璃元件成型设备
    • JP2007204345A
    • 2007-08-16
    • JP2006027951
    • 2006-02-06
    • Toshiba Mach Co Ltd東芝機械株式会社
    • TANAKA TAKASHIKAMANO TOSHINAOSHOGETSU ISAONISHIHARA HIROMI
    • C03B11/12G02B1/00
    • PROBLEM TO BE SOLVED: To provide a glass element molding device continuously enabling a stable and highly accurate molding without vibration and the generation of dust.
      SOLUTION: A hollow insulating member 11 and a partition member 23 are integrally molded. A first inert gas supplied from the top end part of a pipe 17A of an inert gas supply passage 17 directly cools a mold 9 and the back surface side of an outer mold 8 when passing through a discharge groove 21. A second inert gas supplied from an inert gas supply passage 18 indirectly cools the mold 9 and the back surface side of the outer mold 8 when passing through a discharge groove 22 from a passage 23A by the partition member 23. Highly accurate glass element moldings can be stably and continuously formed without the generation of dust because the hollow heat insulating member and the partition member are integrally molded and accordingly the vibration and friction are not generated even when the inert gas flows to the groove.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种玻璃元件模制装置,其连续地实现稳定和高精度的模制而不产生振动和产生灰尘。 解决方案:中空绝缘构件11和分隔构件23一体地模制。 从惰性气体供给通道17的管17A的顶端部供给的第一惰性气体,在通过排出槽21时,直接冷却模具9和外模具8的背面侧。第二惰性气体从 惰性气体供给通道18通过分隔构件23从通道23A通过排出槽22时,间接地冷却模具9和外部模具8的背面侧。可以稳定且连续地形成高精度的玻璃元件模制件而不用 由于空心绝热构件和分隔构件一体地模制而产生灰尘,因此即使当惰性气体流到凹槽时也不产生振动和摩擦。 版权所有(C)2007,JPO&INPIT
    • 9. 发明专利
    • Method for manufacturing mold
    • 制造模具的方法
    • JP2012006233A
    • 2012-01-12
    • JP2010143720
    • 2010-06-24
    • Toshiba Mach Co Ltd東芝機械株式会社
    • KOKUBO MITSUNORIMUROFUSE ISAMUKITAHARA HIDETOSHINISHIHARA HIROMI
    • B29C33/38
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a mold capable of easily obtaining a number of molds for imprinting.SOLUTION: The method for manufacturing the mold includes: a primary mold forming process S1 which uses a master mold M0 on which a fine transfer pattern MA is formed and forms a primary mold M1 on which a fine transfer pattern MB is formed by using a metal; a spin-on glass substrate forming process S3 which provides a spin-on glass 5 on a substrate 3 and forms a spin-on glass-installed substrate 7; a spin-on glass transferring process S5 which presses the spin-on glass-installed substrate by the primary mold and transfers the fine transfer pattern formed on the primary mold on the spin-on glass provided on the spin-on glass-installed substrate; and a secondary mold forming process S7 which uses the spin-on glass-installed substrate on which the fine transfer pattern is transferred and forms a secondary mold M2 on which a fine transfer pattern MC is formed.
    • 要解决的问题:提供一种能够容易地获得多个用于压印的模具的模具的制造方法。 解决方案:用于制造模具的方法包括:一次成型工艺S1,其使用形成有微细转印图案MA的母模M0,并形成其上形成有精细转印图案MB的初级模具M1,其中通过 使用金属; 旋涂玻璃基板形成工艺S3,其在基板3上提供旋涂玻璃5并形成旋涂玻璃基板7; 旋转玻璃转印工艺S5,其通过第一模具按压旋涂玻璃安装的基板,并将形成在第一模具上的精细转印图案转印在设置在旋涂玻璃上的基板上的旋涂玻璃上; 以及二次成型工序S7,其使用转印微细转印图案的旋涂玻璃的基板,形成形成微细转印图案MC的二次模M2。 版权所有(C)2012,JPO&INPIT