    • 3. 发明专利
    • WEAR RESISTANT IRON-BASE SINTERED ALLOY AND ITS PRODUCTION
    • JPH06220591A
    • 1994-08-09
    • JP25870993
    • 1993-10-15
    • TOYOTA MOTOR CORP
    • TAKAHASHI YOSHITAKAMANABE AKIRAKANEKO TADATAKAOKAJIMA HIROSHI
    • C22C33/02C22C38/00
    • PURPOSE:To produce an iron-base sintered alloy for valve seat excellent in wear resistance. CONSTITUTION:A powder mixture is prepared by mixing, by weight ratio, 2-30% of Ni-base alloy powder having a composition consisting of 5-20% Mo, 20-40% Cr, 10-20% W, and the balance Ni with inevitable impurities and 0.2-2% of graphite powder with an iron-base alloy powder having a composition consisting of, by weight ratio, 2-15% Co, 2-10%, preferably >3%-10%, Mo, and the balance Fe with inevitable impurities, which is compacted. Further, 0.2-2% of solid lubricant is mixed with the above, if necessary, and they are compacted. The resulting green compact is sintered at a temp. between 1323K and the melting point of the Ni-base alloy powder. Because alloy powders are used and matrix structure is sintered, the degree of homogenization of entering into solid solution of alloying elements in a matrix is increased and superior corrosion resistance, oxidation resistance, and wear resistance can be obtained with minimal alloy quantity, and further, wear resistance can be improved because Mo, Cr, and W in the Ni-base alloy powder combine with C to form carbides. Moreover, machinability can be improved by adding free cutting agent.