    • 1. 发明专利
    • Method for manufacturing spiral steel pipe and apparatus for measuring shape
    • 用于制造螺旋钢管和测量形状的装置的方法
    • JP2010044016A
    • 2010-02-25
    • JP2008209758
    • 2008-08-18
    • Sumikin Weld Pipe Co LtdSumitomo Metal Ind Ltd住友金属工業株式会社住金大径鋼管株式会社
    • KANO YUTAKAFUKUSHIMA HISAFUMIKOSEKI DAISUKEMIYAZAWA KAZUNARI
    • G01B21/20B21C37/12G01B21/02
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a spiral steel pipe and an apparatus for measuring the shape, capable of measuring the shape of the steel pipe online after a forming/welding process of a steel strip in a manufacturing process of the spiral steel pipe, and capable of carrying out the measurement by using a facility which is altered simply as much as possible by utilizing a current facility.
      SOLUTION: The apparatus for measuring the shape of the spiral steel pipe, which is used for a welding process of the method for manufacturing the spiral steel pipe wherein the steel strip 2 is molded in a tube shape by using a molding device 3 equipped with an internal roller 4 and an external roller 4, and then a submerge arc welding is applied to abutting edges of the steel strip 2 in the width direction to form a steel pipe 7, incudes: a distance meter 17 which is disposed at the head of a mandrel 1 supporting the internal roller 4 and measures a distance from the inner surface of the steel pipe 7 in a noncontact fashion; a motor 15 for rotating the distance meter 17 in the circumferential direction of the steel pipe 7; and a rotation angle measuring means for measuring a rotation angle of the distance meter 17.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种制造螺旋钢管的方法和用于测量形状的装置,其能够在制造过程中在钢带的成形/焊接过程之后在线测量钢管的形状 的螺旋钢管,并且能够通过使用通过利用当前设施尽可能简单地改变的设施来进行测量。 解决方案:用于测量螺旋形钢管的形状的装置,其用于螺旋钢管的制造方法的焊接工艺,其中钢带2通过使用成型装置3成型为管状 配备有内辊4和外辊4,然后在宽度方向上对钢带2的邻接边缘施加浸没电弧焊,形成钢管7,其包括:距离计17 支撑内辊4并且以非接触方式测量与钢管7的内表面的距离的心轴1的头部; 用于使距离计17在钢管7的圆周方向上旋转的马达15; 以及用于测量距离计17的旋转角度的旋转角度测量装置。(C)2010,JPO&INPIT
    • 2. 发明专利
    • Method of manufacturing spiral steel pipe and system for controlling circumference of spiral steel pipe
    • 制造螺旋钢管的方法及控制螺旋钢管循环的系统
    • JP2010120077A
    • 2010-06-03
    • JP2008298552
    • 2008-11-21
    • Sumikin Weld Pipe Co LtdSumitomo Metal Ind Ltd住友金属工業株式会社住金大径鋼管株式会社
    • KANO YUTAKAFUKUSHIMA HISAFUMIKOSEKI DAISUKEMIYAZAWA KAZUNARI
    • B21C37/12
    • PROBLEM TO BE SOLVED: To easily adjust circumference of a spiral steel pipe while preventing defective offset of welding in the process of manufacturing the spiral steel pipe. SOLUTION: The inside circumference or the outside circumference in the portion which is formed into a pipe shape of the spiral steel pipe 7 in the middle of manufacturing is measured in a position which is just after welding. The variation of the inside circumference or the outside circumference on the basis of the measured value of the inside circumference or the outside circumference of the spiral steel pipe 7 is obtained. The spiral steel pipe 7 in the middle of the manufacturing just after internal welding is rotationally moved so that the inside circumference or the outside circumference of the spiral steel pipe 7 approaches the target value. At this time, the corrected angle to a steel strip 2 of the spiral steel pipe 7 is obtained from the variation of the outside circumference and the spiral steel pipe 7 is rotationally moved to the steel strip 2 by the corrected angle. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:为了容易地调节螺旋钢管的周长,同时防止在制造螺旋钢管的过程中焊接的不良偏移。 解决方案:在制造中间形成为螺旋状钢管7的管状的部分的内周或外周被测量在刚刚焊接之后的位置。 基于螺旋状钢管7的内周或外周的测定值,求出内圆周或外周的变化。 在内部焊接刚刚制造的中间的螺旋钢管7被旋转移动,使得螺旋钢管7的内周或外周接近目标值。 此时,螺旋钢管7的钢带2的修正角度是从外周的变化得到的,螺旋钢管7通过修正的角度旋转移动到钢带2。 版权所有(C)2010,JPO&INPIT
    • 5. 发明专利
    • Method for producing welded steel tube
    • 生产焊接钢管的方法
    • JP2006281313A
    • 2006-10-19
    • JP2005290560
    • 2005-10-03
    • Sumikin Daikeikoukan KkSumitomo Metal Ind Ltd住友金属工業株式会社住金大径鋼管株式会社
    • KANO YUTAKASAMOTO HIROSHIKOSEKI DAISUKE
    • B23K9/032B23K9/18B23K9/235B23K101/06B23K103/04
    • PROBLEM TO BE SOLVED: To provide a method for producing a welded steel tube easily applicable to the production of a spiral steel tube without performing large-scale equipment modification, and capable of remarkably improving the efficiency thereof.
      SOLUTION: In the method for producing a welded steel tube, the butting parts in the width direction of hot rolled steel strips bent to a spiral shape are first subjected to submerged arc welding (SAW) at the inner face side in an inner face welding position P1 by an inner face welding machine, thereafter, the steel tube is conducted to a high frequency heating coil 30 located in the downstream side going one-half round along a welding line, so as to perform the preheating of the butting parts in the steel strips before outer face welding, thereafter, the outer face side is subjected to SAW at an outer face welding position P2 by an outer face welding machine. In this case, the surface temperature of the butting parts in the edge faces in the width direction of the steel sheets before the SAW is preferably controlled to ≥400°C.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种容易适用于螺旋钢管的制造的焊接钢管的制造方法,而不进行大规模的设备改造,并且能够显着提高其效率。 解决方案:在焊接钢管的制造方法中,弯曲成螺旋状的热轧钢带的宽度方向的对接部首先在内侧的内侧面进行埋弧焊(SAW) 通过内表面焊接机进行面焊接位置P1,然后将钢管沿着焊接线传导到位于下游侧的高频加热线圈30,以进行对接部的预热 在外表面焊接之前的钢带中,此后,外表面侧通过外表面焊接机在外表面焊接位置P2进行SAW。 在这种情况下,SAW之前的钢板的宽度方向的边缘面的对接部的表面温度优选控制在≥400℃以下。 版权所有(C)2007,JPO&INPIT
    • 6. 发明专利
    • Steel plate connection welding method
    • 钢板连接焊接方法
    • JP2006122930A
    • 2006-05-18
    • JP2004311748
    • 2004-10-27
    • Sumikin Daikeikoukan KkSumitomo Metal Ind Ltd住友金属工業株式会社住金大径鋼管株式会社
    • KANO YUTAKASAMOTO HIROSHIKOSEKI DAISUKE
    • B23K9/18B23K9/235B23K103/04
    • PROBLEM TO BE SOLVED: To provide a plate connection welding method by which steel plates are butted against each other and the butt part of the steel plates is subjected to submerge welding only from either side to perform plate connection such as the case of coil connection welding, e.g., used in the production of a spiral steel pipe, and by which a weld bead can be formed to the rear side of each steel plate, and repair welding on the rear side is therefore made unnecessary, e.g., after the formation of the steel pipe.
      SOLUTION: In a state where steel plates 1, 1 are butted and a backing strip 4 is abutted against the rear face on the side opposite from a welding torch 3 in the butt part 2 of the steel plates 1, 1, a coil 5 for high frequency induction heating is arranged ahead in the progressing direction of the welding torch 3, and while heating is performed beforehand so that the temperature of the butt part 2 reaches the prescribed temperature, submerge arc welding is performed and the plates are connected.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种钢板彼此对接的板连接焊接方法,并且钢板的对接部分仅从两侧进行淹没焊接以执行板连接,例如 线圈连接焊接,例如用于生产螺旋钢管,并且可以在每个钢板的后侧形成焊缝,因此不需要在后侧修补焊接,例如,在 形成钢管。 解决方案:在钢板1,1对接的状态下,背板4与钢板1,1的对接部2的焊炬3相反的一侧的背面抵接在一起 在焊炬3的前进方向上配置有用于高频感应​​加热的线圈5,并且预先进行加热,使对接部2的温度达到规定温度,进行淹没电弧焊接,并且连接板 。 版权所有(C)2006,JPO&NCIPI
    • 7. 发明专利
    • Butt welding method for steel tube, and method of manufacturing welded steel tube
    • 钢管焊接方法及制造焊接钢管的方法
    • JP2008221245A
    • 2008-09-25
    • JP2007059542
    • 2007-03-09
    • Sumikin Daikeikoukan KkSumitomo Metal Ind Ltd住友金属工業株式会社住金大径鋼管株式会社
    • KANO YUTAKASHINTANI SUSUMUKOSEKI DAISUKE
    • B23K9/028B23K9/18B23K9/235B23K101/06B23K103/04
    • PROBLEM TO BE SOLVED: To provide a butt welding method for steel tube by which the quality of a weld bead part is stabilized and work trouble due to interference between a heating coil and the weld bead part is prevented when performing a butt welding of steel tube while performing a high frequency induction heating, and to provide a method of manufacturing a welded steel tube.
      SOLUTION: In the butt welding method, after end faces in the axial direction of steel tubes 1 are butted on each other, submerged arc welding is performed while the steel tubes 1 are rotated in the circumferential direction. Using a high frequency induction heating coil 2, the butting parts of steel tubes are preheated at least in either one of the inner faceord the outer face, and then the submerged arc welding is performed. Concurrently, a relative position in the vertical direction of the high frequency induction heating coil 2 is controlled relative to the inner or the outer face of the steel tubes so that an interval t between the high frequency induction heating coil 2 and the inner or outer face of the butted part of the steel tubes becomes nearly constant, during the rotation of the steel tubes 1.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种用于钢管的对接焊接方法,其中焊道质量受到稳定,并且当进行对接焊时可以防止由于加热线圈和焊道部分之间的干扰而引起的工作故障 的钢管,同时进行高频感应加热,并提供焊接钢管的制造方法。 解决方案:在对接焊接方法中,在钢管1的轴向的端面彼此对接之后,在钢管1沿圆周方向旋转的同时进行埋弧焊。 使用高频感应加热线圈2,钢管的对接部分至少在内表面的外表面中的任一个中预热,然后进行埋弧焊。 同时,相对于钢管的内表面或外表面控制高频感应加热线圈2的垂直方向的相对位置,使得高频感应加热线圈2与内表面或外表面之间的间隔t 在钢管1的旋转期间,钢管的对接部分变得几乎恒定。版权所有(C)2008,JPO&INPIT
    • 8. 发明专利
    • Steel plate connection welding method
    • 钢板连接焊接方法
    • JP2007030015A
    • 2007-02-08
    • JP2005220084
    • 2005-07-29
    • Sumikin Daikeikoukan KkSumitomo Metal Ind Ltd住友金属工業株式会社住金大径鋼管株式会社
    • KANO YUTAKASHINTANI SUSUMUKOSEKI DAISUKE
    • B23K9/18B23K9/032B23K9/235B23K101/06B23K103/04
    • PROBLEM TO BE SOLVED: To provide a steel plate connection welding method in which steel plates are butted to each other like the coil connection welding used in manufacturing a spiral steel tube, the butted portion of the steel plates is submerged-arc welded only from one face side to perform the connection welding, a welding bead (penetration bead) can be generated to back sides of the steel plates, and any repair welding (corrective welding) of the back side of the welding bead becomes unnecessary, e.g., after forming the steel tube.
      SOLUTION: Steel plates 1, 1 are butted to each other, a butted portion 2 of the steel plates 1, 1 is submerged-arc welded only from one face side. In such a condition, while a backing 4 is abutted on a back side opposite to welding torches, a coil 5 for induction heating is arranged ahead in the advancing direction of welding torches 3a, 3b, the butted portion 2 is heated in advance, and the submerge-arc welding is performed using two electrodes (the welding torches 3a, 3b).
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供钢板相互接合的钢板连接焊接方法,就像制造螺旋钢管的线圈连接焊接一样,钢板的对接部分被埋弧焊 仅从一个面侧进行连接焊接,可以在钢板的背面产生焊珠(贯通珠),并且不需要焊缝的背面的任何修补焊(矫正焊接),例如, 形成钢管后。 钢板1相互对接,钢板1,1的对接部分2仅从一个正面侧浸没电弧焊接。 在这样的状态下,当背面4与焊枪相反的背面抵接时,感应加热用线圈5在焊枪3a,3b的前进方向前方配置,预先对接部2被加热, 使用两个电极(焊枪3a,3b)进行埋弧焊。 版权所有(C)2007,JPO&INPIT
    • 9. 发明专利
    • Method and apparatus for cutting steel product
    • 用于切割钢产品的方法和装置
    • JP2010234473A
    • 2010-10-21
    • JP2009084262
    • 2009-03-31
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • KANO YUTAKAMAEDA HIROYUKI
    • B23D47/04B23D36/00
    • PROBLEM TO BE SOLVED: To solve the problem that saw cutting cannot be done by wear and abrasion of a saw blade during a hot saw cutting step located on the downstream of a production line, for a steel product with a large section such as an extremely thick H-section steel or a highly strong steel product rapidly cooled after finish-rolling such as in TMCP specifications among section steels manufactured by hot rolling.
      SOLUTION: When a long H-section steel 23 is cut in a widthwise direction at a predetermined longitudinal position of the H-section steel 23 while pushing it at a position in the vicinity of the predetermined position into two directions including a direction reverse to an advancing direction of a saw blade 18 and an upward direction, using the saw blade 18 advancing widthwise in the H-section steel 23 in a horizontal plane while turning, the H-section steel 23 is cut while independently controlling force of pushing in the two directions.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了解决在位于生产线下游的热切割步骤期间锯锯的磨损不能进行锯切的问题,对于具有大截面的钢产品 作为在热轧制造的截面钢中的TMCP规格等精轧后的极厚H型钢或高强度钢产品迅速冷却。 解决方案:当长H形钢23在H型钢23的预定纵向位置处沿宽度方向切割,同时将其在预定位置附近的位置处推动到包括方向 与锯片18的前进方向相反,向上方向,使用锯切刀18在H剖面钢23的横向方向上在水平面上转动的同时切割H剖面钢23,同时独立地控制推压力 在两个方向。 版权所有(C)2011,JPO&INPIT
    • 10. 发明专利
    • Steel pipe sheet pile and steel pipe sheet pile wall
    • 钢管板和钢管板块墙
    • JP2010144207A
    • 2010-07-01
    • JP2008321799
    • 2008-12-18
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • KAMIMURA TAKAYUKIYUKI HIDEAKIKAJIMA KAZUYUKIKOBAYASHI YOICHIKANO YUTAKA
    • C22C38/00C22C38/58E02B3/06E02D5/04E02D31/06
    • PROBLEM TO BE SOLVED: To provide a steel pipe sheet pile and a steel pipe sheet pile wall having sufficient corrosion resistance. SOLUTION: The steel pipe sheet pile is composed of: a steel pipe part; and joint parts provided at the side faces in the longitudinal direction of the steel pipe part, wherein at least a part of the outer face of the steel pipe part is coated with a corrosion prevention treated steel prescribed by the following (i), and also, at least a part of the joint parts is substituted with corrosion prevention joint parts composed of a corrosion prevention treated steel prescribed in the following (ii): (i) the corrosion prevention treated steel has a corrosion prevention film layer on the surface of a steel having a chemical composition containing, by mass, C, Si, Mn, P, S, Cu, Ni, Cr, Al, N and Sn, and the balance Fe with impurities, wherein a Cu/Sn ratio is ≤1; and (ii) the corrosion prevention treated steel has the corrosion prevention film layer on the surface of a steel having a chemical composition containing, by mass, C, Si, Mn, P, S, Cu, Ni, Cr, Al, N and Sn, and the balance Fe with impurities, wherein a Cu/Sn ratio is ≤1. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供具有足够耐腐蚀性的钢管板桩和钢管桩桩壁。

      解决方案:钢管桩桩由钢管部分组成; 以及设置在所述钢管部的长度方向的侧面的接合部,其中,所述钢管部的外表面的至少一部分涂覆有由以下(i)规定的防腐处理钢,并且还 ,所述接合部的至少一部分被由以下(ii)中规定的防腐处理钢构成的防腐蚀接合部代替:(i)所述防腐处理钢在其表面上具有防腐蚀膜层 钢的化学成分含有质量比C,Si,Mn,P,S,Cu,Ni,Cr,Al,N和Sn,余量为Fe的杂质,其中Cu / Sn比≤1; (ii)防锈处理钢在具有以质量计含有C,Si,Mn,P,S,Cu,Ni,Cr,Al,N的化学组成的钢的表面上具有防腐蚀膜层, Sn,余量为Fe与杂质,其中Cu / Sn比≤1。 版权所有(C)2010,JPO&INPIT