    • 1. 发明专利
    • Method of producing slaked lime slurry
    • 生产水泥浆的方法
    • JP2008266051A
    • 2008-11-06
    • JP2007108634
    • 2007-04-17
    • Okutama Kogyo Co Ltd奥多摩工業株式会社
    • SASAKI ATSUSHIISHIHARA MASAYUKI
    • C04B2/04C01F11/02
    • PROBLEM TO BE SOLVED: To provide a method of producing slaked lime slurry by using slaked lime powder obtained by slaking and drying quick lime, and preparing the slaked lime slurry to be used for example as a neutralizing agent for an acidic waste gas, wherein the decrease of BET specific surface area of the slaked lime powder particle is prevented to keep high activity.
      SOLUTION: In the production of the slaked lime slurry by mixing the slaked lime obtained by slaking the quick lime with water, 75-140 pts.mass slaking water is added into 100 pts.mass quick lime to slake the quick lime until the hydrous slaked lime having 15-30 pts.mass water content is obtained and the resultant hydrous slaked lime is formed into the slurry by adding water.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种通过使用熟石灰粉碎和干燥而得到的熟石灰粉生产熟石灰浆料的方法,并制备用作酸性废气中和剂的熟石灰浆料 其中防止熟石灰粉末颗粒的BET比表面积的降低保持高活性。

      解决方案:在生产熟石灰浆料时,将通过将生石灰与水相比较得到的熟石灰混合,将75-140磅的水加入到100磅的生石灰中,以将生石灰切片直至 得到15-30质量%含水量的水合熟石灰,并通过加入水将所得水合熟石灰制成浆料。 版权所有(C)2009,JPO&INPIT

    • 2. 发明专利
    • Method for producing planar calcium hydroxide
    • 生产平版氢氧化钙的方法
    • JP2010111532A
    • 2010-05-20
    • JP2008284417
    • 2008-11-05
    • Okutama Kogyo Co Ltd奥多摩工業株式会社
    • TANAKA KOICHISASAKI ATSUSHI
    • C01F11/02
    • PROBLEM TO BE SOLVED: To provide a method for producing planar calcium hydroxide having a sheet face length of ≥100 μm.
      SOLUTION: The method for producing the planar calcium hydroxide comprises: a first stage S1 where the suspension of calcium hydroxide is prepared; a second stage S2 where the prepared suspension of calcium hydroxide is made into a first temperature state; a third stage S3 where the prepared suspension of calcium hydroxide is made into a second temperature state lower than the first temperature; and a fourth stage S4 where the second stage and the third stage are repeatedly performed thereto.