    • 1. 发明专利
    • Method and device for manufacturing fuel compact
    • 用于制造燃料压缩的方法和装置
    • JP2006315055A
    • 2006-11-24
    • JP2005141642
    • 2005-05-13
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • B30B11/20G21C3/62G21C21/02
    • B30B11/12
    • PROBLEM TO BE SOLVED: To provide a device for manufacturing a fuel compact, which needs no large space, easily sets the temperatures of a die and a punch, and easily sets the drive of the punch.
      SOLUTION: A raw material M of the fuel compact, which contains coated fuel particles, is charged into die cavities 20V of a die 20 and subjected to press molding by pressing punches 30 into the die cavities 20V to manufacture a fuel compact F. The die cavities 20V have the shapes of notches, which are provided so as to be opened toward the peripheral face of the disk-like die 20 at some intervals in the peripheral direction. After the raw material M is sequentially charged into each of the die cavities 20V, the corresponding punches 30 are inserted into the die cavities 20V. The punches 30 are pressed into the die cavities 20V by the relative rotation of the die 20 and a punch press 40, which is provided closely to the peripheral face of the die 20 and has a circular arc face 40S with a cam 40SA.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供一种不需要大空间的燃料压块的制造装置,容易设定模具和冲头的温度,并且容易地设定冲头的驱动。 解决方案:将包含涂覆的燃料颗粒的燃料压块的原料M装入模具20的模腔20V中,并通过将冲模30压入模腔20V进行压制成型,以制造燃料压块F 模腔20V具有凹口形状,其设置成沿着圆周方向以一定间隔向盘状模具20的周面开口。 在将原料M依次装入每个模腔20V之后,将相应的冲头30插入模腔20V。 冲头30通过模具20的相对旋转和紧密地设置在模具20的周面的冲压机40而被压入模腔20V,并且具有带有凸轮40SA的圆弧面40S。 版权所有(C)2007,JPO&INPIT
    • 2. 发明专利
    • Spacer forming method of fuel pin for fast fission reactor
    • 用于快速灭菌反应器的燃料密封件形成方法
    • JP2006133064A
    • 2006-05-25
    • JP2004321973
    • 2004-11-05
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • G21C3/12
    • Y02E30/40
    • PROBLEM TO BE SOLVED: To dispense with a fuel pin rotation mechanism, a winding tool and its moving mechanism required in a conventional technology in order to wind a wire around the fuel pin, and to dispense with control of rotational speed of the fuel pin and moving speed of the winding tool.
      SOLUTION: In order to form a spacer by winding the wire around the fuel pin 1 used for a fuel assembly for a fast fission reactor, the fuel pin 1 is allowed to pass into a spiral coil-shaped wire 10, and the spiral coil-shaped wire 10 is elongated so as to be wound around the fuel pin 1 in the state where one end 10a of the spiral coil-shaped wire 10 is fixed on a lower end stopper 2 of the fuel pin 1.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了省略燃料销旋转机构,卷绕工具及其传统技术中所需的移动机构,以便将线缠绕在燃料销周围,并且不需要控制旋转速度 燃料销和卷绕工具的移动速度。 解决方案:为了通过将线缠绕在用于快速裂变反应堆的燃料组件的燃料销1上而形成间隔件,燃料销1被允许进入螺旋形线状导线10,并且 在螺旋线圈状线10的一端10a被固定在燃料销1的下端止动器2上的状态下,螺旋形线状导线10被拉长以便缠绕在燃料销1上。 版权所有(C)2006,JPO&NCIPI
    • 3. 发明专利
    • Wrapper tube for fast reactor and its joint method
    • 用于快速反应器的缠绕管及其接头方法
    • JP2013117489A
    • 2013-06-13
    • JP2011266017
    • 2011-12-05
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社Japan Atomic Energy Agency独立行政法人日本原子力研究開発機構
    • HONDA MAKINAKAMURA WATARUYANO YASUHIDEMINAFUJI TAKEJI
    • G21C3/324
    • Y02E30/40
    • PROBLEM TO BE SOLVED: To provide a wrapper tube for a fast reactor which is excellent in reliability by reducing bending after welding.SOLUTION: In a wrapper tube for a fast reactor constituted by welding, to an opening end part 2a of a wrapper tube 1 whose outer shape is polygonal, an opening end part of a joint shell 3 whose outer shape is polygonal in the same way as the wrapper tube 1, a butting face 6 to which an opening end face of the wrapper tube 1 is butted and a centering cylinder part 7 extending in an axial direction of the wrapper tube 1 are adjacently arranged in a thickness direction at the opening end part of the joint shell 3, and the opening end part 2a of the wrapper tube 1 is fit along the centering cylinder part 7, and the opening end face of the wrapper tube 1 is butted to the butting face 6 of the joint shell 3, and the opening end face of the wrapper tube 1 and the butting face 6 of the joint shell 3 are welded.
    • 要解决的问题:提供一种通过减少焊接后的弯曲而具有优异的可靠性的快速反应器的包装管。 解决方案:在用于通过焊接构成的快速反应器的包装管中,在外形为多边形的包装管1的开口端部2a处,外形为多边形的接合壳3的开口端部 与包装管1相同的方式,包装管1的开口端面对接的对接面6和沿包装管1的轴向延伸的定心圆筒部7在厚度方向上相邻布置 接头壳3的开口端部,包裹管1的开口端部2a沿定心圆筒部7配合,将包装管1的开口端面与对接壳的对接面6对接 3,将包装管1的开口端面和接合壳3的对接面6焊接。 版权所有(C)2013,JPO&INPIT
    • 4. 发明专利
    • Manufacturing method for pebble bed fuel
    • 泡沫燃料的制造方法
    • JP2007147546A
    • 2007-06-14
    • JP2005345324
    • 2005-11-30
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • G21C3/22
    • Y02E30/40
    • PROBLEM TO BE SOLVED: To manufacture pebble bed fuel of high quality with a uniform graphite matrix density and a uniform distribution of fine particles, using a mold having a simple spherical shape of recess.
      SOLUTION: The pebble bed fuel is manufactured by pressurizing an elastic mold 10 having the mold recess 10C filled with a mixture M of an overcoated particle and a graphite matrix, the mold 10 has the spherical mold recess 10C and a regular hexahedral outer surface 10S, and the pebble bed fuel is manufactured by pressurizing and compressing the whole outer surface, while pressurizing sequentially a plurality of outer surfaces 10S1 and 10S2, 10S3 and 10S4, 10S5 and 10S6, those are one parts of the outer surface 10S of the mold 10.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:使用具有简单的球形凹陷的模具,以均匀的石墨基质密度和均匀的细颗粒分布来制造高质量的卵石床燃料。 解决方案:通过对具有填充有外涂层颗粒和石墨基质的混合物M的模具凹槽10C的弹性模具10进行加压来制造卵石床燃料,模具10具有球形凹槽10C和规则的六面体外部 表面10S,并且卵石床燃料通过对整个外表面进行加压和压缩来制造,同时依次对多个外表面10S1和10S2,10S3和10S4,10S5和10S6加压,这些是外部表面10S的一部分 模具10.版权所有(C)2007,JPO&INPIT
    • 5. 发明专利
    • Machine for sorting fine particle based on sphericity
    • 基于球面分选细颗粒的机器
    • JP2006289279A
    • 2006-10-26
    • JP2005114830
    • 2005-04-12
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • B07B13/11G21C3/62G21C21/02
    • Y02E30/33Y02E30/38
    • PROBLEM TO BE SOLVED: To make it possible to sort fine particles in terms of sphericity while avoiding inclusion of defective particles with acceptable particles, even when fine particles are supplied at a high rate. SOLUTION: With the use of the machine for sorting fine particles based on sphericity, defective particles 50B are separated from acceptable particles 50A by a vibrator mechanism 30, the defective particles 50B are guided to a direction by a guide part 24 on a particle fall plate 22, so as to cause the defective particles 50B to move away from an acceptable particle fall region GA, and thus the acceptable particles 50A are further clearly separated from acceptable particles 50A while they are rolling and falling on the particle fall plate 22. Therefore, the defective particles 50B will never be mixed with the acceptable particles 50A, even when fine particles 50 are supplied at a high supply rate to the particle fall plate 22, causing the defective particles 50B to move around or be flicked by collision with each other. COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:即使在以高速率供给细颗粒时,也可以避免包含具有可接受的颗粒的有缺陷的颗粒,从而可以在球形度方面对细颗粒进行分类。 解决方案:通过使用机器根据球形度分选细颗粒,通过振动器机构30将有缺陷的颗粒50B与可接受的颗粒50A分离,将有缺陷的颗粒50B通过引导部分24引导到一个方向上 颗粒落下板22,使得有缺陷的颗粒50B远离可接受的颗粒落下区域GA移动,并且因此可接受的颗粒50A在它们滚动并落在颗粒坠落板22上时与可接受的颗粒50A进一步清楚地分离 因此,即使当细颗粒50以高供给速率供给到颗粒坠落板22时,有缺陷的颗粒50B也不会与可接受的颗粒50A混合,导致有缺陷的颗粒50B通过与 彼此。 版权所有(C)2007,JPO&INPIT
    • 6. 发明专利
    • Method for manufacturing pebble bed fuel element
    • 生产泡沫燃料元件的方法
    • JP2006208206A
    • 2006-08-10
    • JP2005020987
    • 2005-01-28
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • G21C3/22G21C3/62
    • Y02E30/33Y02E30/36Y02E30/38
    • PROBLEM TO BE SOLVED: To manufacture a pebble bed fuel element having an excellent core concentricity by retaining a core at the center in the interior of a rubber mold when graphite powder is compressed and molded around the core.
      SOLUTION: For the purpose of positioning the core 1 at the center in the interior of the rubber mold 10, a plurality of graphite supporting rods 20 are attached on a lower rubber mold 10L. The core 1 is placed on the tip ends of the support rods 20 and retained at the center in the interior of the lower rubber mold 10L. An intermediate rubber mold 10M is placed on the lower rubber mold 10L, graphite powder 2 is charged through a powder filling port 14 formed in the intermediate rubber mold 10M to fill the gap between the core 1 and the rubber mold 10 with the graphite powder 2. Then, an upper rubber mold 10U is placed on the intermediate rubber mold 10M, and the whole mold 10 is pressed by a press machine or the like to compress and mold the graphite powder 2. Thus, the pebble bed fuel element is manufactured.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了制造具有优异的芯同心度的卵石床燃料元件,当石墨粉被压制和模制在芯周围时,通过将芯保持在橡胶模内部的中心处。 解决方案:为了将芯1定位在橡胶模具10​​的内部的中心,多个石墨支撑杆20附接在下部橡胶模具10​​L上。 芯1放置在支撑杆20的顶端,并保持在下橡胶模10L的内部的中心。 将中间橡胶模具10​​M放置在下橡胶模具10​​L上,石墨粉末2通过形成在中间橡胶模具10​​M中的粉末填充口14填充,以用石墨粉末2填充芯体1和橡胶模具10​​之间的间隙 然后,将上橡胶模10U放置在中间橡胶模10M上,并且通过压力机等挤压整个模10以压缩和模制石墨粉2。因此,制造卵石床燃料元件。 版权所有(C)2006,JPO&NCIPI
    • 7. 发明专利
    • Apparatus for forming spacer pad of wrapper tube
    • 用于形成包装管的间隔垫的装置
    • JP2006145364A
    • 2006-06-08
    • JP2004335370
    • 2004-11-19
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • G21C3/33
    • Y02E30/40
    • PROBLEM TO BE SOLVED: To provide an apparatus for forming a spacer pad of a wrapper tube, capable of easily forming the spacer pad on the wrapper tube used for the fuel assembly of a fast reactor.
      SOLUTION: The method of forming the spacer pad at a predetermined position of the wrapper tube, having a regular hexagonal shape and used in the fuel assembly of the fast reactor comprises a die frame covering the whole circumference, including the spacer pad forming section of the wrapper tube in the longitudinal direction and having a spacer-pad shaped recess formed in a predetermined position, a punch member inserted to an interior position of the wrapper tube facing the recess of the die frame and having a spacer-pad shaped protrusion formed on its outer wall and a punch pressing means for pressing the punch member to the outer side.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种用于形成包装管的间隔垫的装置,其能够容易地在用于快堆的燃料组装的包裹管上形成间隔垫。 解决方案:在包装管的预定位置处形成间隔垫的方法,其具有规则的六边形形状并用于快速反应器的燃料组件中的方法包括覆盖整个圆周的模架,包括间隔垫形成 并且具有形成在预定位置的间隔垫形凹部,冲压件插入到所述包装管的面向所述模框的凹部的内部位置,并且具有间隔垫形突起 在其外壁上形成有冲压构件到外侧的冲压装置。 版权所有(C)2006,JPO&NCIPI
    • 8. 发明专利
    • Plating method to wrapper tube for fuel assembly, and plating electrolytic cell
    • 用于燃料组装的包装管的镀覆方法和电镀电解槽
    • JP2005139478A
    • 2005-06-02
    • JP2003374226
    • 2003-11-04
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • G21C21/00C25D5/02C25D7/00G21C3/324
    • Y02E30/40
    • PROBLEM TO BE SOLVED: To provide a plating method to a wrapper tube for a fuel assembly where hard chromium plating with a fixed thickness can be effectively applied to a spacer pad part with a compact plating electrolytic cell without dipping the whole of the wrapper tube into the plating electrolytic cell, and the subsequent treatment can be facilitated without causing the sticking of an electrolytic solution to the part of the wrapper tube other than the spacer pad part, and to provide a plating electrolytic cell.
      SOLUTION: In the method, at least one surface part 5S in the spacer pad part 5 of a wrapper tube is covered with a plating electrolytic cell 10, electric current is made to flow between the wrapper tube as the cathode and the anode 16 fixed to the inside of the plating electrolytic cell 10, hard chromium plating is applied to the surface part 5S in the spacer pad part 5 contacted with the plating electrolytic cell 10, and the operation is performed at the other surface part 5S in the spacer pad part 5, thus the hard chromium plating is applied to the whole surface of the spacer pad part 5 in the wrapper tube.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:为了提供一种用于燃料组件的包装管的电镀方法,其中具有固定厚度的硬铬镀层可以有效地施加到具有紧凑的电镀电解池的间隔垫部分,而不会将整个 将包装管装入电镀电解槽中,并且可以容易地进行处理,而不会使电解液粘附到除垫片部分之外的包裹管的部分上,并且提供电镀电解槽。 解决方案:在该方法中,包覆管的间隔垫部分5中的至少一个表面部分5S被镀覆电解槽10覆盖,使电流作为阴极和阳极在包裹管之间流动 固定在电镀电解槽10的内部,在与镀敷电解槽10接触的间隔垫部5中的表面部5S上施加硬铬电镀,在间隔物的另一个表面部5S进行操作 垫部分5,因此将硬铬电镀施加到包装管中的间隔垫部分5的整个表面。 版权所有(C)2005,JPO&NCIPI
    • 9. 发明专利
    • Sphericity sorter for fine particle
    • 细颗粒微球
    • JP2007216160A
    • 2007-08-30
    • JP2006040404
    • 2006-02-17
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • B07B13/11
    • PROBLEM TO BE SOLVED: To sort a sphericity of fine particles without contaminating qualified products with defective products even in the case where the fine particles are supplied at a high particle supply speed. SOLUTION: The sphericity sorter of fine particles drops fine particles 50 by applying vibration to a particle dropping plate in a transverse direction and separates qualified products 50A with good sphericity and defective products 50B with bad sphericity and the defective products 50B are dropped from a particle dropping plate 22 through a notch 46N formed in a middle of the particle dropping plate 22 and recovered under the particle dropping plate 22. COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:即使在以高的颗粒供给速度供给细颗粒的情况下,也可以不污染具有缺陷产物的合格产品来分选细颗粒的球形度。

      解决方案:细颗粒的球形分选机通过在横向上对颗粒滴落板施加振动而滴落细颗粒50,并且将具有良好球形度的合格产品50A和具有差的球形度的有缺陷的产品50B分离,并且不良产品50B从 颗粒落下板22通过形成在颗粒滴落板22中间并在颗粒滴下板22下面回收的凹口46N。(C)2007,JPO&INPIT

    • 10. 发明专利
    • Chiller for welding
    • 焊接用焊接机
    • JP2006231342A
    • 2006-09-07
    • JP2005045370
    • 2005-02-22
    • Nuclear Fuel Ind Ltd原子燃料工業株式会社
    • NAKAMURA WATARU
    • B23K37/06B23K9/00G21C3/324G21C3/33G21C21/00
    • Y02E30/40
    • PROBLEM TO BE SOLVED: To provide a chiller for welding, which chiller can prevent a crack of a welded portion, and can reduce welding deformation, and can be easily mounted to and dismounted from the neighborhood of the welding portion.
      SOLUTION: The chiller for welding 10 to be arranged on the inner wall surface of a cylindrical member of an object to be welded comprises: a cooling block 11 which is divided into a plurality of blocks capable of moving in the radial direction from the longitudinal axis of the cylindrical member, of which the respective blocks have abutting surfaces to be brought into contact with the inner wall surface of the cylindrical member; a tapered piece 14 which has a tapered surface 13 to be brought into contact with the central side wall surfaces opposed to the respective abutting surfaces of the cooling block, which presses the individual abutting surfaces against the inner wall surface by sliding the central side surfaces on the tapered surface by axially moving the tapered piece; and a tapered piece moving means for axially moving the tapered piece.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了提供一种用于焊接的冷却器,该冷却器可以防止焊接部分的裂纹,并且可以减少焊接变形,并且可以容易地从焊接部分附近安装和拆卸。 解决方案:用于焊接的冷却器10布置在待焊接的物体的圆柱形构件的内壁表面上,包括:冷却块11,其被分成多个能够沿径向移动的块 圆柱形构件的纵向轴线,其各个块具有与圆柱形构件的内壁表面接触的邻接表面; 锥形件14具有锥形表面13,该锥形表面13与与冷却块的各个邻接表面相对的中央侧壁表面接触,该中间侧壁表面通过将中间侧表面滑动而将各个邻接表面压靠在内壁表面上 所述锥形表面通过轴向移动所述锥形件; 以及用于轴向移动所述锥形件的锥形件移动装置。 版权所有(C)2006,JPO&NCIPI