    • PROBLEM TO BE SOLVED: To provide a solid polymer fuel cell having a metal separator 5 restrained from corrosion, maintaining high power generating efficiency for long time. SOLUTION: The solid polymer fuel cell has a structure of interposing an oxidation electrode 2 and a fuel electrode 3, arranged on both surfaces of the solid polymer film 1, between metal separators 5. Products of erosion are preliminarily removed from the solid polymer film 1, the oxidation electrode 2, and the fuel electrode 3 by the cleaning using boiling water, or by the electrolytic reaction of water generated by humid atmosphere or electricity conduction in the water solution, and a stainless steel, on the surface of which, a Ni layer is formed, is used as a metal separator 5. As the products of erosion are preliminarily removed from a thin film electrode assembly, pH is not lowered when the operation of the fuel cell is started, and as the essential excellent electron conductive property of Ni is maintained for long time, a solid polymer fuel cell with small loss of Joule heat is obtained.
    • 要解决的问题:提供具有抑制腐蚀的金属隔板5的固体高分子型燃料电池,长时间保持高发电效率。 解决方案:固体聚合物燃料电池具有在固体聚合物膜1的两个表面上设置在金属隔板5之间的氧化电极2和燃料电极3的结构。预先从固体聚合物膜1中除去侵蚀产物 ,氧化电极2和燃料电极3,通过使用沸水的清洗,或通过在水溶液中产生的潮湿气氛或电传导的水的电解反应,以及不锈钢,其表面上的Ni 作为金属隔膜5使用。由于从薄膜电极组件中预先除去侵蚀的产物,因此当燃料电池的操作开始时,pH值不降低,并且作为基本优异的电子传导性能 Ni长时间保持,获得了焦耳热损失小的固体聚合物燃料电池。