热词
    • 1. 发明专利
    • Method for supporting honeycomb molding
    • 支持蜂窝模糊的方法
    • JP2014100810A
    • 2014-06-05
    • JP2012252674
    • 2012-11-16
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • B28B3/20B28B13/04
    • B29D99/0089B28B3/20B28B11/243B28B13/04B29C47/0028B29C47/34
    • PROBLEM TO BE SOLVED: To provide a method for supporting a honeycomb molding, in which the honeycomb molding molded by a horizontal extrusion molding machine can be restrained effectively from being deformed when supported by a receiving base thereof and even a large-sized honeycomb molding can be supported while hardly generating buckling and while keeping high shape accuracy as it is.SOLUTION: When the honeycomb molding 1 extruded horizontally from a mouthpiece 13 of an extrusion molding machine is supported by the receiving base 7, the lowermost edge of the supporting surface 8 of the receiving base 7 when moved horizontally is made lower than that of the honeycomb molding 1 just after extruded from the mouthpiece 13 and a vertical distance A between the lowermost edge of the honeycomb molding 1 just after extruded from the mouthpiece 13 and that of the supporting surface 8 of the receiving base 7 when moved horizontally is set to be 5-15 mm.
    • 要解决的问题:提供一种用于支撑蜂窝模制件的方法,其中通过水平挤出成型机成型的蜂窝模塑件可以有效地被其受其底座支撑而变形,甚至大型蜂窝模制罐 被支撑,同时几乎不产生屈曲,同时保持高的形状精度。解决方案:当从挤出成型机的接口管13水平挤出的蜂窝成型体1被接收基座7支撑时,支撑表面8的最下边缘 在从接口管13挤压出来之后,接收基座7水平移动的距离小于蜂窝成型体1的高度,并且在从接口管13挤出之后的蜂窝成型体1的最下边缘与垂直距离A之间的垂直距离A 将水平移动时的接收基座7的支撑面8设定为5〜15mm。
    • 2. 发明专利
    • Method for manufacturing ceramic honeycomb structure
    • 制造陶瓷蜂窝结构的方法
    • JP2014008603A
    • 2014-01-20
    • JP2012144231
    • 2012-06-27
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • B28B11/12B28B11/02
    • B29D99/0089B23D59/001B28B11/12B28B17/0072B28D7/04G01B11/2408
    • PROBLEM TO BE SOLVED: To provide a manufacturing method of a ceramic honeycomb structure capable of manufacturing a ceramic honeycomb structure excellent in squareness.SOLUTION: A contour of the outer diameter size of a ceramic honeycomb dried body 50 is measured in a first measuring part Q1 and a second measuring part Q2 on the outer wall 63 surface of the ceramic honeycomb dried body 50, and the total of absolute values of each difference of four contours C1x, C1y, C2x, C2y measured at a first measuring point P1x and a second measuring point P1y of the first measuring part Q1, and a third measuring point P2x and a fourth measuring point P2y of the second measuring part Q2 is determined, and one end face 61 and the other end face 62 of the ceramic honeycomb dried body 50 are finished in the state where the four measuring points at which the total of the absolute values of each difference of the contours becomes minimum, on the outer wall 63 of the ceramic honeycomb dried body 50, are supported by a first pedestal and a second pedestal.
    • 要解决的问题:提供一种陶瓷蜂窝结构体的制造方法,该陶瓷蜂窝结构体能够制造出具有优异的矩形度的陶瓷蜂窝结构体。解决方案:陶瓷蜂窝干燥体50的外径尺寸的轮廓在第一测量部分Q1 和陶瓷蜂窝干燥体50的外壁63表面上的第二测量部Q2,以及在第一测量点P1x处测量的四个轮廓C1x,C1y,C2x,C2y的每个差的绝对值的总和,第二测量 确定第一测量部分Q1的点P1y和第二测量部分Q2的第三测量点P2x和第四测量点P2y,并且陶瓷蜂窝干燥体50的一个端面61和另一个端面62被完成 在陶瓷蜂窝干燥体50的外壁63上,轮廓的各个差异的绝对值的总和的最小值的四个测定点为最小的状态下, 由第一基座和第二基座支撑。
    • 3. 发明专利
    • Manufacturing method of ceramic
    • 陶瓷制造方法
    • JP2006264237A
    • 2006-10-05
    • JP2005088580
    • 2005-03-25
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • B28B3/20
    • PROBLEM TO BE SOLVED: To suitably manufacture a ceramic having a stable quality by favorably controlling a mass of a body for shaping.
      SOLUTION: The manufacturing method of the ceramic comprises mixing and kneading a body containing a ceramic material, extruding the body 1 with a kneader 6, cutting the body 1 into pieces of a predetermined length to give the body 1a for shaping, filling the body 1a for shaping in a shaping machine and shaping it to give a shaped body, and firing the shaped body to produce the ceramic, wherein a mass of the body 1a for shaping to be filled in the shaping machine is measured, and quality control of the body 1a for shaping is conducted based on the measured mass.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:通过有利地控制用于成型的主体的质量来适当地制造具有稳定质量的陶瓷。 解决方案:陶瓷的制造方法包括将包含陶瓷材料的主体混合和捏合,将本体1挤出捏合机6,将主体1切割成预定长度的片,以使得主体1a成形,填充 主体1a,用于在成形机中成形并成形以形成成形体,并且对成形体进行烧制以制造陶瓷,其中测量用于成形的主体1a的质量,以填充在成型机中,并且质量控制 用于成形的主体1a基于测量的质量进行。 版权所有(C)2007,JPO&INPIT
    • 4. 发明专利
    • Production method of ceramic honeycomb structure
    • 陶瓷蜂窝结构的生产方法
    • JP2014083799A
    • 2014-05-12
    • JP2012235569
    • 2012-10-25
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • B28B11/12B28B11/02
    • PROBLEM TO BE SOLVED: To provide a production method of a ceramic honeycomb structure that can produce a ceramic honeycomb structure that has excellent cylindricity.SOLUTION: In an end of one edge face 61 side, a central part in a direction toward another edge face 62 from the one edge face 61, and an end of the other edge face 62 side of a ceramic honeycomb dried body 50, in respective two or more places, outer peripheral shapes A-A, B-B, C-Cof an exterior wall surface of a ceramic honeycomb dried body 50 are measured, outer peripheral shapes A-A, B-B, C-Care grouped so that three outer peripheral shapes of an outer peripheral shape measured in the end of one edge face 61 side, an outer peripheral shape measured in the central part, and an outer peripheral shape measured in the end of the other edge face 62 side become one group, cylindricity of the ceramic honeycomb dried body 50 is calculated for each of respective groups, measurement places of an outer peripheral shape of the end of one edge face 61 side and the end of the other edge face 62 side of a group in which cylindricity becomes smallest are made finishing processing positions of the ceramic honeycomb dried body 50.
    • 要解决的问题:提供一种陶瓷蜂窝结构体的制造方法,该陶瓷蜂窝结构体可以制造具有优异的圆筒度的陶瓷蜂窝结构体。解决方案:在一个边缘面61侧的朝向另一边缘面62的方向的中央部 在一个边缘面61和陶瓷蜂窝干燥体50的另一个边缘面62侧的端部,在两个或更多个位置中,外周形状AA,BB,C-Cof陶瓷蜂窝体的外壁表面 测量干燥体50,外周形状AA,BB,C-Care组合成使得在一个边缘面61侧的端部测量的外周形状的三个外周形状,在中心部分测量的外周形状,以及 在另一边缘面62侧的端部测量的外周形状为一组,针对各组计算出陶瓷蜂窝干燥体50的圆柱度,末端o的外周形状的测定位置 在一个边缘面61侧和圆柱度变得最小的组的另一边缘面62侧的端部是陶瓷蜂窝干燥体50的精加工位置。
    • 5. 发明专利
    • Method for producing ceramic honeycomb structure
    • 生产陶瓷蜂窝结构的方法
    • JP2014028509A
    • 2014-02-13
    • JP2013105647
    • 2013-05-17
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • B28B11/12B28B11/02
    • B29D99/0089B28B11/243B28B17/0072G01B11/24
    • PROBLEM TO BE SOLVED: To provide a method for producing a ceramic honeycomb structure capable of improving production efficiency by reducing necessity of off-line inspection.SOLUTION: A method for producing a ceramic honeycomb structure 100 includes: a shape determination step A for measuring the outer peripheral shape of each ceramic honeycomb dried body 50 in which a plurality of cells 52 extending from one end face 61 to the other end face 62 are formed sectionally by partitions 51, and removing a ceramic honeycomb dried body 50 not satisfying a specified condition; a finishing step B for obtaining a finished ceramic honeycomb dried body 70 by finishing a ceramic honeycomb dried body 50 satisfying the specified condition so that a length in the direction L from the one end face toward the other end face agrees with a finished dimension; and a firing step C for obtaining the ceramic honeycomb structure 100 by firing the finished ceramic honeycomb dried body 70.
    • 要解决的问题:提供一种能够通过降低离线检查的必要性来提高生产效率的陶瓷蜂窝结构体的制造方法。解决方案:陶瓷蜂窝结构体100的制造方法包括:形状判定步骤A, 每个陶瓷蜂窝干燥体50的外周形状,其中从一个端面61延伸到另一个端面62的多个单元52由分隔壁51分段地形成,并且去除不满足特定条件的陶瓷蜂窝干燥体50; 精加工步骤B,用于通过对满足特定条件的陶瓷蜂窝干燥体50进行精加工来获得成品陶瓷蜂窝干燥体70,使得从一端面朝向另一端面的方向L的长度与成品尺寸一致; 以及烧制步骤C,用于通过焙烧成品陶瓷蜂窝干燥体70获得陶瓷蜂窝结构体100。
    • 6. 发明专利
    • Opening-sealed portion forming member and manufacturing method of opening-sealed honeycomb structure using it
    • 打开密封部件成型和使用其打开密封蜂窝结构的制造方法
    • JP2006027206A
    • 2006-02-02
    • JP2004212706
    • 2004-07-21
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • B28B11/00B01D46/00B28B7/34F01N3/02
    • PROBLEM TO BE SOLVED: To provide a manufacturing method of an opening-sealed honeycomb structure capable of easily manufacturing the opening-sealed honeycomb structure having a dome-like opening sealing portion. SOLUTION: The manufacturing method of the opening-sealed honeycomb structure 1 is characterized in that the opening-sealed portion 8 is formed on the edge surface of the honeycomb structure 6 by injecting opening-sealed portion-forming slurry 31 into the concave portions 25 of the opening-sealed portion forming member 35 by using the opening-sealed portion-forming member 35 which is composed of a flat base body 23 having a surface area equal to or larger than that of the edge surface of the honeycomb 6 to be opening-sealed and has many concave portions 25 for storing opening-sealed portion-forming slurry 31 formed on the surface of the base body 23; placing the honeycomb structure 6 so that its edge surface contacts the surface of the opening-sealed portion forming member 35; and attaching the opening-sealed portion-forming slurry 31 to the edge surface of a separating wall 2 located at the circumferential margin of the opening of the opening-sealed portion. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种能够容易地制造具有圆顶状开口密封部的开口蜂窝结构体的开口蜂窝结构体的制造方法。 解决方案:开封蜂窝结构体1的制造方法的特征在于,通过将开口密封部分形成浆料31注入到凹部中而形成在蜂窝结构体6的边缘表面上的开口部8 通过使用开口密封部形成构件35,开口密封部形成构件35的部分25由平面基体23构成,该平坦基体23具有等于或大于蜂窝6的边缘表面的表面积的平坦基体23, 被打开密封并且具有许多用于存储形成在基体23的表面上的开口密封部分形成浆料31的凹部25; 将蜂窝结构体6的边缘面接触开口部形成部件35的表面, 并且将开封部分形成用浆料31安装在位于开口部的开口的周缘的分隔壁2的边缘面上。 版权所有(C)2006,JPO&NCIPI
    • 7. 发明专利
    • Method for manufacturing honeycomb structure and honeycomb structure
    • 蜂窝结构和蜂窝结构的制造方法
    • JP2006298745A
    • 2006-11-02
    • JP2006014749
    • 2006-01-24
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • C04B41/85B01D39/20B01D46/00B01D53/86B01J35/04
    • F01N3/0222B01D39/2093B01J35/04C04B41/009C04B41/5037C04B41/87C04B2111/00793F01N3/2828Y02T10/20Y10T428/24149C04B41/4539C04B35/195C04B38/0006
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a honeycomb structure covered with a coating material on its outer periphery, by which method, even if slurry for forming the material is applied and forcibly dried from the beginning, cracks are hardly generated, and to provide a honeycomb structure, which is obtained by this method and has no cracks on its coating material. SOLUTION: The honeycomb structure 1, whose outer periphery is covered with a coating material 3, is manufactured by working the outer peripheral part of a honeycomb base material 2, which is sectioned with porous ceramic partitions and has a plurality of cells, into a prescribed shape, by applying the slurry, which is used for forming the coating material, on the side surfaces, which are exposed to the outer periphery, of partitions 5 existing on the outermost periphery, and by heating and drying it. The slurry for forming the coating material contains powder of potsherd having 15-75 μm particle diameters and has 26-34 mass% water content. COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供一种在其外周上覆盖有涂料的蜂窝结构体的制造方法,即使从一开始就施加用于形成材料的浆料并强制干燥的方法,几乎​​不发生裂纹 并且提供通过该方法获得并且在其涂层材料上没有裂纹的蜂窝结构。 解决方案:通过对蜂窝状基材2的外周部进行加工来制造外周覆盖有涂料3的蜂窝结构体1,该蜂窝状基材2的外周部分分布有多孔陶瓷隔板并具有多个电池, 通过在外露的外侧的暴露于外周的侧面施加用于形成涂料的浆料,并将其加热干燥,从而形成规定的形状。 用于形成涂料的浆料含有粒径为15-75μm,具有26-34质量%含水量的锅炉粉末。 版权所有(C)2007,JPO&INPIT
    • 8. 发明专利
    • Manufacturing method of opening-sealed honeycomb structure, mask for forming opening-sealed part used in the method and manufacturing method of mask
    • 打开密封蜂窝结构的制造方法,用于形成开放式密封部件的方法和制造方法
    • JP2005059512A
    • 2005-03-10
    • JP2003295519
    • 2003-08-19
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • B01D46/00B01J35/04B28B1/00B28B11/00B32B3/10B32B3/12F01N3/022G06T1/00
    • B32B3/12Y10T428/24273
    • PROBLEM TO BE SOLVED: To provide a manufacturing method of an opening-sealed honeycomb structure which is free from restriction on a working environment, enables inexpensive manufacture of the opening-sealed honeycomb structure in a short time and decreases the quantity of industrial waste. SOLUTION: In this method, at least an image of the end face of the honeycomb structure 48 is picked up to acquire image data which enable specification of the shapes and positions of cells (opening-sealed cells) to be closed and cells (opening-non-sealed cells) not to be closed. Based on the image data, a mask 41B for forming an opening-sealed part having hole portions 46 which can communicate with the opening-sealed cells and a projection 44 which can be fitted at least in a part of the honeycomb structure 48 is prepared by an optical shaping method. The masks 41A, 41B and 41C for forming the opening-sealed part are fixed on the end face of the honeycomb structure 48 by fitting each of the projections 44 at least in a part of the structure 48. In this state, a ceramic slurry is introduced into the opening-sealed cells through the hole portions 46 of the masks 41A, 41B and 41C, so as to form the opening-sealed part. COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:为了提供一种在工作环境中没有限制的开式蜂窝结构体的制造方法,能够在短时间内廉价地制造开封蜂窝结构体,并且减少工业量 浪费。 解决方案:在该方法中,拾取至少蜂窝结构体48的端面的图像,以获取能够指定要封闭的单元(开封单元)的形状和位置的图像数据,以及单元 (开 - 非密封电池)不闭合。 基于图像数据,形成用于形成具有可与开口密封单元连通的孔部分46的开口密封部分的掩模41B和可以至少装配在蜂窝结构体48的一部分中的突起44,其制备为: 光学成形方法。 用于形成开口部的面罩41A,41B,41C至少在构造体48的一部分上嵌合各蜂窝结构体48的端面。在这种状态下,陶瓷浆料 通过掩模41A,41B和41C的孔部分46引入开封密封的单元中,以形成开封部分。 版权所有(C)2005,JPO&NCIPI
    • 9. 发明专利
    • Method and apparatus for positioning columnar structure
    • 定位柱结构的方法和装置
    • JP2007051969A
    • 2007-03-01
    • JP2005238515
    • 2005-08-19
    • Ngk Insulators Ltd日本碍子株式会社
    • KATO SHIGEKI
    • G01B5/25B05C13/02
    • C04B41/508B05C5/0254B05C11/023B05C11/1039C04B41/009C04B41/85C04B2111/00793Y10T83/6563C04B41/5024C04B35/00C04B35/195C04B38/0006
    • PROBLEM TO BE SOLVED: To provide a method and an apparatus for positioning a columnar structure that can improve the quality characteristics, such as thermal shock resistance, isostatic strength, thermal stresses, and mechanical stresses, in the columnar structure (ceramic honeycomb structure), obtained by making the center axis of the columnar structure and that of a pedestal nearly uniform, for unifying a coating thickness when coating the outer-periphery surface of the columnar structure, and can improve the productivity, since the drying properties of a coating section are superior.
      SOLUTION: The columnar structure 1 is placed on the pedestal 3; a positioning fixing jig 24 is brought into contact with the pedestal 3 on which the columnar structure 1 is placed; the columnar structure 1 is moved from the pedestal 3, while the columnar structure 1 is in contact at two points or one point by a positioning adjusting jig 25 that makes it abut against the positioning fixing jig 24; and the columnar structure 1 is brought into contact with the positioning fixing jig 24, so as to position the pedestal 3 to substantially coincide the center axis of the columnar structure 1, and supporting the columnar structure 1 at four points or three points with the positioning fixing jig 24 and the positioning adjusting jig 25.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种用于定位柱状结构的方法和装置,其能够提高柱状结构(陶瓷蜂窝体)中的耐热冲击性,等静压强度,热应力和机械应力的质量特性 结构),通过使柱状结构的中心轴和台座的中心轴几乎均匀,通过在涂覆柱状结构体的外周面时使涂布厚度均匀化,可以提高生产率,因为a 涂层部分优越。

      解决方案:将柱状结构1放置在基座3上; 定位固定夹具24与放置柱状结构1的基座3接触; 柱状结构1从基座3移动,同时柱状结构1通过定位调整夹具25在两点或一点接触,定位调节夹具25抵靠定位固定夹具24; 柱状结构1与定位固定夹具24接触,以便将基座3定位成与柱状结构1的中心轴大致重合,并且将柱状结构1支撑在四点或三点与定位 固定夹具24和定位调整夹具25.版权所有(C)2007,JPO&INPIT