    • 4. 发明专利
    • High strength and/or high transparency polypropylene sheet
    • 高强度和/或高透明聚丙烯薄片
    • JP2006015756A
    • 2006-01-19
    • JP2005242135
    • 2005-08-24
    • National Institute Of Advanced Industrial & Technology独立行政法人産業技術総合研究所
    • NAKAYAMA KAZUOSHIMIZU HIROSHI
    • B29C47/88B29C43/46B29C47/14B29C47/92B29K23/00B29L7/00C08J5/18C08L23/00
    • B29C47/0021
    • PROBLEM TO BE SOLVED: To provide a thick object of isotactic polypropylene which is excellent in transparency and mechanical properties. SOLUTION: A transparent sheet of this invention is a polypropylene sheet formed by blending a crystal nucleator, and has an elastic modulus of 1.2 GPa or higher, a fracture strength of 90 MPa or higher, and a haze value of 11% or lower. A sheet is made by adding the crystal nucleator to polypropylene, extrusion-molding the crystal nucleator added polypropylene into a sheet, crystallizing the sheet on the surface of a chilled roll at a temperature of not lower than (Tm-90)°C and not higher than (Tm-40)°C, wherein Tm is the fusing point of the polypropylene and rolling the product under a specified condition at a temperature within the range of (αc-30)°C to (αc+20)°C, wherein αc is the crystal dispersion peak temperature of the loss factor at a frequency of 1 Hz in the dissonance forced oscillation dynamic viscoelasticity temperature curve. The sheet is not less than 1.2 GPa in elastic modulus and 90 MPa in maximum stress, and 11% or less in haze value. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供透明性和机械性能优异的全同立构聚丙烯的粗物体。 解决方案:本发明的透明片是通过混合晶体成核剂而形成的聚丙烯片,其弹性模量为1.2GPa以上,断裂强度为90MPa以上,雾度值为11%, 降低。 通过将晶体成核剂加入到聚丙烯中制成片材,将加成晶体成核剂的聚丙烯挤出成型为片材,在不低于(Tm-90)℃的温度下将片材在冷却辊的表面上结晶,而不是 高于(Tm-40)℃,其中Tm是聚丙烯的熔点,并且在特定条件下在(αc-30)℃至(αc+ 20)℃的范围内的温度下滚动产物, 其中αc是在非谐振强制振荡动态粘弹性温度曲线中在1Hz频率处的损耗因子的晶体分散峰值温度。 片材的弹性模量不小于1.2GPa,最大应力为90MPa,雾度值为11%以下。 版权所有(C)2006,JPO&NCIPI
    • 5. 发明专利
    • Polyamide-containing resin composition
    • 含聚氨酯树脂组合物
    • JP2005162839A
    • 2005-06-23
    • JP2003402233
    • 2003-12-01
    • National Institute Of Advanced Industrial & Technology独立行政法人産業技術総合研究所
    • OYAMA HIDEKONAKAYAMA KAZUOONO YUKO
    • C08L77/00C08K9/04
    • PROBLEM TO BE SOLVED: To obtain a new thermoplastic resin composition which comprises a polyamide and a polypropylene, contains the polypropylene or copolypropylene in the polyamide in an independently dispersed state, and contains an organic-modified inorganic laminar compound in the polyamide, the polypropylene and the copolypropylene and on their interfaces.
      SOLUTION: This thermoplastic resin composition is obtained by melt-kneading (A) 60 to 95 pts.wt. of the polyamide, (B) 5 to 40 pts.wt. of a modified polypropylene or copolypropylene, and (C) 2 to 40 pts.wt. of the organic-modified inorganic laminar compound, wherein the rate of an unsaturated dicarboxylic acid and/or unsaturated dicarboxylic acid derivative and/or an epoxy compound-treated product of the modified polypropylene or copolypropylene is 0.1 to 20 wt.% based on the modified polypropylene or copolypropylene.