热词
    • 5. 发明专利
    • THERMOSETTING ADHESIVE SHEET
    • JPS6286078A
    • 1987-04-20
    • JP22759185
    • 1985-10-11
    • NITTO ELECTRIC IND CO
    • SAITO KIYOSHITAKAHIRA HITOSHIKAWAMOTO NORIO
    • C09J7/02C09J163/00
    • PURPOSE:To obtain the titled adhesive sheet which is excellent in electrical insulation and gap-filling properties, etc., applying a mixture of a solid crystalline epoxy resin with a curing agent and a mixture of a solid non-crystalline epoxy resin with a curing agent respectively onto the sides of a fibrous substrate. CONSTITUTION:A compsn. (A) comprising a crystalline epoxy resin which is solid at room temp. [e.g., 4,4'-bis(2'',3''-epoxypropoxy)-3,3',5,5'-tetramethyl biphenyl] and a curing agent which is solid at room temp. (e.g., novolak phenol resin) and a compsn. (B) comprising a non-crystalline epoxy resin which is solid at room temp. (e.g., solid bisphenol A epoxy resin) and a curing agent which is solid at room temp. are applied respectively onto the sides of a fibrous substrate to obtain an intended thermosetting adhesive sheet. The sheet thus formed is advantageously used for enhancement in adhesion and insulation of a member, such as electromagnetic valve coil, having an uneven bonding surface by filling the gaps with the sheet.
    • 9. 发明专利
    • Painted steel material
    • 涂漆钢材
    • JPS6176682A
    • 1986-04-19
    • JP19888684
    • 1984-09-22
    • Nitto Electric Ind Co Ltd
    • TAJIRI KAZUHIROSAITO KIYOSHIKAWAMOTO NORIOTAKAHIRA HITOSHI
    • C23C22/00B32B15/08B32B15/092C08K3/40C09D163/00C25D11/36C25D11/38
    • C08K3/40C08K2201/016C09D163/00C08L63/00C08L2666/54
    • PURPOSE:To provide a painted steel material having excellent flexibility and impact resistance by forming the chemical treating film of a phosphate treating agent and the coated film of a specifically composed epoxy resin on the surface of the steel material having specific surface roughness. CONSTITUTION:The chemical treating film having 0.1-10g/m dry film weight is formed by a phosphate treating liquid, chromate treating liquid or chromic acid treating liquid on the surface of the steel material which is subjected prelim inarily to a surface treatment so as to have 10-120mu surface roughness (max. roughness specified in JISB0601). The coated film consisting of an epoxy resin powder paint having >=0.1mm thickness is then formed thereon by 100pts.wt. bisphenol A type epoxy resin having =50mu average length subjected to the surface treatment by a silane coupling agent and >=5 aspect ratio, >=30pts.wt. granular inorg. filler (titanium dioxide, etc.) having
    • 目的:通过在具有特定表面粗糙度的钢材的表面上形成磷酸盐处理剂的化学处理膜和具体组成的环氧树脂的涂膜,提供具有优异的柔韧性和耐冲击性的涂漆钢材。 构成:通过预先进行表面处理的钢材表面上的磷酸盐处理液,铬酸盐处理液或铬酸处理液形成具有0.1-10g / m 2干膜重量的化学处理膜 以具有10-120μm的表面粗糙度(JISB0601中规定的最大粗糙度)。 然后在其上形成具有> = 0.1mm厚度的环氧树脂粉末涂料的涂膜,100psa.wt。 双酚A型环氧树脂,其末端基数不超过非活性末端基团数的5%,30-100pts.wt。 ≥5μm的平均长度的针状玻璃粉末,通过硅烷偶联剂进行表面处理,> = 5的纵横比> 30pts.wt。 粒状inorg。 填充剂(二氧化钛等)具有平均粒度<=1.0μm,纵横比大约<= 2和硬化剂。