    • 3. 发明专利
    • HORIZONTAL ALLOYING FURNACE FOR PLATED STEEL SHEET
    • JPS62185885A
    • 1987-08-14
    • JP2592486
    • 1986-02-10
    • NISSHIN STEEL CO LTD
    • HAYASHI NOBUHIKOITO TAKEHIKOMORIYAMA YOSHITERU
    • C25D5/50C23C2/28C23C14/56C23C14/58C23C26/00C23C30/00
    • PURPOSE:To permit easy installation of a titled furnace in a low building as well and to obtain a good alloyed layer with exact temp. control by successively disposing a heating section, soaking section and cooling section in the conveying direction of a steel strip respectively in horizontal types and providing non- contact supporting means for the steel strip. CONSTITUTION:The plated steel strip 1 is introduced via guide rolls 15 into the heating section 10 and is heated to the temp. necessary for alloying by adequate heating means such as electrical heaters 10a, etc. The temp. of the strip is made uniform and the plating surface is alloyed uniformly up to the surface thereof while the steel strip is passed through the soaking section 11. The steel strip 1 is supported and conveyed without contact and is cooled down to the temp. at which the generation of flaws is obviated even if the steel strip contacts the rolls in the succeeding cooling section 12. A floating system by ejection of the gas from gas ejecting nozzles 11 is more preferable as the above- mentioned non-contact supporting means. The soaking section 11 is segmented to plural pieces of the zones 11a, 11b, 11c... in the conveying direction and temp. control means are preferably provided to each of the blocks.
    • 4. 发明专利
    • PRETREATMENT FOR DRY GALVANIZING
    • JPS60131959A
    • 1985-07-13
    • JP24027783
    • 1983-12-19
    • NISSHIN STEEL CO LTD
    • TAKAI SHIGEMITSUHAYASHI NOBUHIKOYAMAMOTO MASARUHAYASHI YOSHIO
    • C23C2/02C23C2/30
    • PURPOSE:To form a defectless plating layer having excellent adhesion even if stains of fats and oils stick on the surface of a steel material by forming the coated film of a flux soln. contg. a surface active agent on the surface of the steel material then subjecting the surface to galvanizing. CONSTITUTION:A steel sheet 1 unrolled from a payoff reel 10 is pickled by hydrochloric acid, etc. in a pickling tank 11 and after the pickling soln. sticking thereto is removed in a rinsing tank 12, the steel sheet is passed through a flux soln. tank 13. The steel sheet is immersed in a flux soln. consisting essentially of an aq. soln. of about 15 deg. Be' of ZnCl2 and NH4Cl and contg. at least about 0.1%, more preferably about 0.2-0.4% surface active agent, more particularly preferably nonionic surface active agent in said tank to form the coated film thereof on the surface. The sheet 1 coated with the flux soln. is passed through a drying furnace 4 and is dried by which the uniform flux layer is formed over the entire surface of the steel sheet 1. The pretreated steel sheet 1 is passed through a galvanizing cell 15 and is then taken up on a roll 16, by which the dry galvanized steel sheet having the defectless plating layer which is free from non- plating and pinholes, etc. and has excellent adhesion is obtd.
    • 5. 发明专利
    • GAS THROTTLING DEVICE
    • JPS6082652A
    • 1985-05-10
    • JP18698583
    • 1983-10-07
    • NISSHIN STEEL CO LTD
    • KUBOTA MASAROUONO YOSHIOHAYASHI NOBUHIKOTAKAGI KAZUO
    • C23C2/20
    • PURPOSE:To prevent uneven plating due to the clogging of a gas injection port with molten zinc by constituting a gas throttling device for blowing away excess molten zinc of a molten zinc plated steel strip of a rotatable external cylinder having the gas injection ports and an internal cylinder for supplying gas having a sealing member. CONSTITUTION:Excess molten zinc deposited on a zinc plated steel strip 3 coming out from a molten zinc plating bath 2 is blown away from both sides of the steel strip 3 with gas injection by a gas throttling device 1. The gas throttling device 1 is constituted of a circular external cylinder 5 having gas injection ports 8 and nozzles 9 which is rotatable in the circumferential direction, and of an internal cylinder 11 having at the inside a gas supply port 16 and a sealing member 17 on the opposite side. The pressurized gas supplied into the internal cylinder 11 is spouted from a nozzle 9 of the external cylinder 5 on the outer side to blow away excess molten zinc. When the port of the nozzle 9 is clogged by the deposition of molten zinc, the external cylinder 5 is turned to an angle of 180 deg. and the gas is injected from another new nozzle 9. In addition, the injection of the pressurized gas from the nozzle 9 not facing the steel strip 3 is prevented by the sealing member 17.
    • 7. 发明专利
    • UNIFORM COOLING METHOD FOR STEEL STRIP IN CONTINUOUS ANNEALING FURNACE
    • JPS62182226A
    • 1987-08-10
    • JP2420186
    • 1986-02-07
    • NISSHIN STEEL CO LTD
    • OHASHI KYOSUKEITO TAKEHIKOHAYASHI NOBUHIKOSAKO MITSUHIKO
    • C21D9/573C21D11/00C23C14/56
    • PURPOSE:To make the transverse temp. of a steel strip passing in an adjusted cooling zone more uniform by segmenting the adjusted cooling zone of a continuous annealing furnace to a central part and both end parts in the transverse direction thereof and maintaining the heating temp. in both end parts higher than the heating temp. in the central part. CONSTITUTION:The adjusted cooling zone of the continuous annealing furnace is segmented to at least the central part and both end parts. The heating temp. in both end parts is maintained higher than the heating temp. in the central part and the steel strip passing the adjusted cooling zone is uniformly cooled in the transverse direction thereof. Cooling is executed in such a manner that the temp. difference of the steel strip between the central part and both end parts is kept within 15 deg.C by the above-mentioned method, by which the good plating surface having uniform and excellent adhesiveness is obtd. in the subsequent vacuum deposition plating. A thermometer for the steel strip is installed on the outlet side of the adjusted cooling zone to detect the temp. of the steel strip and the heating in the central part and both end parts of the steel strip is controlled in accordance with the detected value in the above-mentioned method, by which the automation of the above-mentioned uniform cooling method is made possible.
    • 10. 发明专利
    • REMOVING METHOD OF TREATING LIQUID REMAINING AFTER CHEMICAL CONVERSION TREATMENT
    • JPS60208482A
    • 1985-10-21
    • JP6453584
    • 1984-03-30
    • NISSHIN STEEL CO LTD
    • HAYASHI NOBUHIKOHAYASHI YOSHIOOGASAWARA MASAO
    • C23C22/73C23C22/82
    • PURPOSE:To remove thoroughly the remaining chemical conversion liquid in the edge parts of a steel strip and to eliminate the uneven chemical conversion treatment in the stage of removing the chemical conversion liquid remaining on the steel strip subjected to the chemical conversion treatment by wringer rolls by directing exactly air nozzles to the edge parts of the steel strip detected by sensors. CONSTITUTION:A chemical conversion treating liquid remains on a steel strip S from a chemical conversion treating stage and therefore the steel strip is passed between wringer rolls 81 and 82 to remove the remaining liquid. The roll gaps corresponding to the thickness of the strip S are produced at both edges of the strip S in this case and the chemical conversion treating liquid remains in said parts, thus making the chemical conversion treatment uneven. The edges of the strip S are detected by an edge detector 3 for the steel strip consisting of plural light projecting phototube parts 31a-31d and photodetecting phototube parts 32a-32d shifted positionally each slightly in order to prevent the above-mentioned uneven treatment. A motor 4 is driven by the detection outputs therefrom to direct correctly the nozzles 71, 72 of an air sprayer 7 connected to the detector 3 toward the center of the edges of the strip S. The treating liquid remaining at the edges is thoroughly removed by the air ejected from the nozzles 71, 72.