    • 1. 发明专利
    • Method for coagulating polymer latex
    • 凝聚聚合物的方法
    • JPS59182801A
    • 1984-10-17
    • JP5770583
    • 1983-03-31
    • Mitsubishi Rayon Co Ltd
    • SUGIMORI TERUHIKOTAJIRI TAKAYUKIHIRONAKA AKIOHABARA HIDEAKI
    • C08F6/00C08F6/22
    • PURPOSE: To obtain a polymer granular or particulate material having excellent powder characteristics, by coagulating the titled latex with a coagulating nozzle, capable of extruding a coagulating solution through the central part of a base board, and obtained by mounting capillaries on the base board under specific conditions.
      CONSTITUTION: A nozzle for coagulating a latex, having a structure capable of extruding a coagulating solution through the central part of a base board 2, and obtained by mounting plural capillaries 1 on the base board 2 to give ≥1mm mutual gap between the capillaries 1 and ≥3mm protrusion length of the capillaries 1 on the base board 2 is usually dipped in a coagulation bath, and a polymer latex is introduced into a holder 3 of the above-mentioned nozzle, extruded through the tips of the capillaries 1 at the same time to come into contact with the coagulating solution around the nozzle and extruded through the central part of the base board 2 and coagulated.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:为了获得具有优异粉末特性的聚合物颗粒或颗粒材料,通过凝结喷嘴的标题胶乳凝结,能够通过基板的中心部分挤出凝固溶液,并将毛细管安装在基板上 具体条件。 构成:用于凝结胶乳的喷嘴,其具有能够通过基板2的中心部分挤出凝结液的结构,并且通过将多个毛细管1安装在基板2上而得到= 1mm。 毛细管1和> = 3mm之间的相互间隙。 通常将基板2上的毛细管1的突出长度浸入凝固浴中,并将聚合物胶乳引入到上述喷嘴的保持器3中,同时通过毛细管1的尖端挤出 与喷嘴周围的凝固溶液接触并通过基板2的中心部分挤出并凝结。
    • 2. 发明专利
    • Production of thermoplastic resin
    • 生产热塑性树脂
    • JPS5924709A
    • 1984-02-08
    • JP13411582
    • 1982-07-30
    • Mitsubishi Rayon Co Ltd
    • SUGIMORI TERUHIKOTAJIRI TAKAYUKI
    • C08F6/00C08F6/22C08F279/00C08F279/04
    • PURPOSE: To obtain the titled resin excellent in blendability and free from a need of washing operation, by coagulating an MBS resin latex at a temperature in a specified range to form a coagulated slurry, and adding thereto an alkaline substance at a temperature in a specified range to adjust its pH to a specified value.
      CONSTITUTION: A latex of a thermoplastic resin is formed which contains a monomer component at least 90wt% of which consisting of butadiene, methyl methacrylate, and styrene. Then, this latex is brought into contact with a coagulating solution (an example of a coagulant being sulfuric acid) at a temperature in the range of 0W80°C to form a coagulated slurry and then an alkaline substance (e.g., sodium hydroxide) is added to the obtained slurry so that the pH of the slurry is higher by at least 0.1 than the initial pH, and that the pH of the entire mixture is adjusted to 7.0 or below. Then, the desired thermoplastic resin is obtained by solidifying the coagulated particles of the coagulated slurry by heating.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:为了获得混合性优异且不需要洗涤操作的标题树脂,通过在特定范围的温度下使MBS树脂胶乳凝固形成凝固的浆料,并在特定温度下加入碱性物质 范围将其pH值调整到指定值。 构成:形成热塑性树脂的胶乳,其包含至少90重量%的由丁二烯,甲基丙烯酸甲酯和苯乙烯组成的单体成分。 然后,使该胶乳在0-80℃的温度下与凝固溶液(作为硫酸的凝结剂的实例)接触以形成凝结的浆料,然后加入碱性物质(例如氢氧化钠 )添加到所获得的浆料中,使得浆料的pH比初始pH高至少0.1,并且将整个混合物的pH调节至7.0以下。 然后,通过加热固化凝固浆料的凝固颗粒,获得所需的热塑性树脂。
    • 3. 发明专利
    • Production of impact-resistant resin by continuous emulsion polymerization
    • 通过连续乳化聚合生产耐冲击树脂
    • JPS5721411A
    • 1982-02-04
    • JP9591180
    • 1980-07-14
    • Mitsubishi Rayon Co Ltd
    • SUGIMORI TERUHIKOTAJIRI TAKAYUKI
    • C08F4/00C08F2/22C08F2/44C08F4/04C08F4/28C08F4/32C08F279/02C08F291/00
    • PURPOSE: To produce title polymer having excellent impact resistance and appearance, by emulsion-polymerizing a monomer in the presence of a rubbery polymer with the aid of a combination of an azo compound type initiator and a peroxide type initiator.
      CONSTITUTION: A rubbery polymer, e.g., polybutadiene, and one or more monomers, e.g., styrene or acrylonitrile, are dispersed in water in an amount of 80W 500pts.wt. per 100pts.wt. solids of the latex after polymerization, with the aid of an emulsifier, and emulsion-polymerized in the presence of an azo compound type initiator, e.g., 2,2'-azobiaisobutyronitrile, and a peroxide type initiator, e.g., 1- hydroxybutyl n-butyl peroxide.
      EFFECT: It is possible to control the grafting ratio and the degree of polymerization of the polymer to be produced at desired values, by properly selecting the ratio of the azo compound type initiator to the peroxide type initiator.
      COPYRIGHT: (C)1982,JPO&Japio
    • 目的:为了制备具有优异的耐冲击性和外观的标题聚合物,通过在偶联化合物型引发剂和过氧化物型引发剂的组合的帮助下,在橡胶状聚合物存在下使单体乳化聚合。 构成:橡胶状聚合物,例如聚丁二烯和一种或多种单体,例如苯乙烯或丙烯腈,以80-500pts.wt。的量分散在水中。 每100pts.wt 聚合后的胶乳的固体,借助于乳化剂,并在偶氮化合物型引发剂例如2,2'-偶氮二异丁腈和过氧化物型引发剂(例如1-羟基丁基)的存在下进行乳液聚合, 丁基过氧化物。 效果:通过适当选择偶氮化合物型引发剂与过氧化物型引发剂的比例,可以控制所需聚合物的接枝率和聚合度。
    • 4. 发明专利
    • Resin for toner
    • 调色剂树脂
    • JP2005202421A
    • 2005-07-28
    • JP2005029738
    • 2005-02-04
    • Mitsubishi Rayon Co Ltd三菱レイヨン株式会社
    • ITO KOICHIIWASAKI HITOSHITAJIRI TAKAYUKI
    • G03G9/087
    • PROBLEM TO BE SOLVED: To provide a resin for a toner which is excellent in fixing properties, non-offset properties, blocking resistance and image stability.
      SOLUTION: The resin for the toner is a polymer comprising (a) an aromatic vinyl unit, (b) a (meth)acrylic-based compound unit and (c) a multi-functional compound unit and containing 5 to 60% of a tetrahydrofuran (THF) insoluble portion of a glass transition temperature 50 to 70°C and ≤5wt% secondary flocculation object of 16 mesh oversize. The molecular weight of the maximum peak in a molecular weight distribution by gel permeation chromatography of a TFH soluble portion is ≤20,000; the weight average degree of polarization (Pw) is ≤180; the Pw ranges Pw≤-3.25X+180 in the case of the the THF insoluble portion
    • 要解决的问题:提供一种固色性,非偏移性,抗粘连性和图像稳定性优异的调色剂用树脂。 调色剂用树脂是包含(a)芳族乙烯基单元,(b)(甲基)丙烯酸系化合物单元和(c)多官能化合物单元,含有5〜60重量% 的玻璃化转变温度为50至70℃的四氢呋喃(THF)不溶部分和≤6重量%的16目超大型二次絮凝物。 通过TFH可溶部分的凝胶渗透色谱法测定的分子量分布中最大峰的分子量≤20,000; 重均极化度(Pw)≤180; 在THF不溶部分<40%的情况下,Pw范围Pw≤-3.25X + 180,在THF不溶部分的情况下Pw≤-0.25X + 60的范围≥40%(其中X表示不溶部分 (%))。 版权所有(C)2005,JPO&NCIPI
    • 6. 发明专利
    • Coagulation of polymer latex
    • 聚合物的凝聚
    • JPS59199704A
    • 1984-11-12
    • JP7441883
    • 1983-04-27
    • Mitsubishi Rayon Co Ltd
    • SUGIMORI TERUHIKOTAJIRI TAKAYUKIHIRONAKA AKIOHABARA HIDEAKI
    • C08F6/00C08F6/22
    • PURPOSE: To obtain powder or granule having high bulk density containing neither fine powder nor coarse particles, by using a nozzle prepared by providing a substrate having a specific wide length with plural thin pipes having a specific length at specified intervals.
      CONSTITUTION: The substrate 2 having ≤150mm wide length is provided with the plural thin pipes 1 in such a way that the intervals between the thin pipes are ≥1mm and the protrusion length A on the substrate 2 is ≥3mm to give a nozzl for coagulating latex. Usually the nozzle is immersed in coagulating solution, and polymer latex is extruded from the interior of the holder 3 through the thin pipes 1 to a coagulating bath, so that the polymer latex is coagulated. Preferably the thin pipes 1 are bonded to the substrate 2 with an adhesive, etc.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:通过使用通过以特定宽度的基板提供具有特定长度的多个细管的规定间隔制备的喷嘴,获得具有既不含细粉末也不含粗颗粒的高堆积密度的粉末或颗粒。 构成:衬底2的<= 150mm。 在多个细管1的宽度方向设有使细管之间的间隔大于等于1mm的方式。 并且基板2上的突出长度A> 3mm。 给乳胶凝乳。 通常将喷嘴浸入凝固溶液中,将聚合物胶乳从保持件3的内部通过细管1挤出至凝固浴,使聚合物胶乳凝结。 优选地,薄管1用粘合剂等粘合到基底2上
    • 7. 发明专利
    • Production of thermoplastic resin
    • 生产热塑性树脂
    • JPS5938208A
    • 1984-03-02
    • JP14887882
    • 1982-08-27
    • Mitsubishi Rayon Co Ltd
    • SUGIMORI TERUHIKOTAJIRI TAKAYUKI
    • C08F6/00C08F6/06C08F6/14
    • PURPOSE: To obtain in good workability a thermoplastic resin excellent in blendability and appearance of a molding, by controlling the pH of a coagulated slurry at a specified value, in producing a thermoplastic resin by coagulating a thermoplastic resin latex prepared by an emulsion polymerization process.
      CONSTITUTION: A thermoplastic resin latex is prepared by emulsion-polymerizing a monomer component consisting of ethyl acrylate and/or butyl acrylate and methyl methacrylte and/or styrene. Then, this resin latex is subjected to a coagylation operation at temperatures lower than the solidification temperature of the thermoplastic resin to form a coagulated slurry. Then, an alkali substance (e.g., sodium hydroxide) is added to the coagulated slurry at the same temperature range so that the pH of the coagulated slurry at this point may be higher than its initial pH by at least 0.1, and that the pH of the entire mixture may be below 7. Then, this coagulated slurry is heated to solidify the coagulated particles. In this way, the purpose thermoplastic resin is obtained.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:为了通过凝固通过乳液聚合法制备的热塑性树脂胶乳来制造热塑性树脂,为了获得良好的可加工性,通过将凝固浆料的pH控制在特定值,可以使模塑品的混合性和外观优异的热塑性树脂。 构成:通过乳液聚合由丙烯酸乙酯和/或丙烯酸丁酯和甲基丙烯酸甲酯和/或苯乙烯组成的单体组分制备热塑性树脂胶乳。 然后,使该树脂胶乳在低于热塑性树脂的凝固温度的温度下进行凝固操作,形成凝固的浆料。 然后,在相同的温度范围内将碱性物质(例如,氢氧化钠)加入到凝固的浆料中,使得此时凝固的浆料的pH可能高于其初始pH至少0.1,并且pH 整个混合物可能低于7.然后,将该凝固的浆料加热固化凝固的颗粒。 以这种方式获得目的热塑性树脂。
    • 8. 发明专利
    • Filter for polymer latex
    • 聚合物过滤器
    • JPS6114203A
    • 1986-01-22
    • JP13417984
    • 1984-06-29
    • Mitsubishi Rayon Co Ltd
    • SUGIMORI TERUHIKOTAJIRI TAKAYUKIHIRONAKA AKIOHABARA HIDEAKI
    • C08F6/00C08F6/14C08J3/02
    • PURPOSE: To remove coarse particles in a polymer latex continuously in good efficiency without encountering clogging of a filter medium in pressure filtration, by providing a rotatable filter equipped with a perforated plate for removing cullet.
      CONSTITUTION: An inlet 1 for feeding a polymer latex of, e.g., ABS resin or butadiene rubber is provided with a seal member 2 at its upstream end. A filter member 4 which can rotate in close contact with the seal member 2 is equipped with a perforated plate 3 for removing cullet. An exit 6 for the filtered latex is connected to the back side of the filter member 4 through a seal member 5 provided in close contact with the filter member 4. A rotary shaft 7 rotates the filter member 4. A back-washing liquid feed inlet 8 for removing coarse particles such as coarse polymer particles deposited on the perforated plate 3 in the filter member 4 or other coarse foreign matter particles by washing with the liquid is provided in a position outside the exit 6.
      COPYRIGHT: (C)1986,JPO&Japio
    • 目的:为了高效率地连续地除去聚合物胶乳中的粗颗粒,而不会在压力过滤中遇到过滤介质的堵塞,通过提供一种装有多孔板的可旋转过滤器来去除碎玻璃。 构成:用于供给例如ABS树脂或丁二烯橡胶的聚合物胶乳的入口1在其上游端设有密封件2。 可以与密封构件2紧密接触的过滤构件4配备有用于去除碎玻璃的多孔板3。 过滤胶乳的出口6通过与过滤构件4紧密接触地设置的密封构件5连接到过滤构件4的背面。旋转轴7使过滤构件4旋转。反洗液体进料口 在出口6的外侧设置用于除去沉积在过滤构件4中的多孔板3上的粗大颗粒,或者用液体洗涤等其它粗异物颗粒的粗颗粒。
    • 9. 发明专利
    • Coagulation of polymer latex
    • 聚合物的凝聚
    • JPS59174625A
    • 1984-10-03
    • JP4844783
    • 1983-03-23
    • Mitsubishi Rayon Co Ltd
    • SUGIMORI TERUHIKOTAJIRI TAKAYUKIHIRONAKA AKIOHABARA HIDEAKI
    • C08J3/16C08C1/00C08C1/14C08F6/00C08F6/22
    • PURPOSE: To coagulate a polymer latex in the form of powder having high bulk density and excellent powder characteristics, by dividing the substrate plate into several regions, and attaching thin tubes having specific length as the nozzle for latex coagulation to the divided region interposing specific distance between the tubes.
      CONSTITUTION: The substrate plate 2 is divided into two or more regions placing a gap of ≥5mm between the regions, and each region is furnished firmly with thin tubes 1 having a protruded length of ≥3mm above the plate and a gap of ≥1mm between the tubes, and the assembly is used as the nozzle for the coagulation of a polymer latex. The nozzle is attached to the holder 3 interposing a gasket 4 with the clamp 5, and the polymer latex is extruded through the thin tubes 1 into a coagulation bath. The coagulated polymer is transferred to the solidification tank and heated to obtain solidified polymer particles.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:为了使具有高堆积密度和优异粉末特性的粉末形式的聚合物胶乳凝固,将基板分隔成几个区域,并将具有特定长度的细管作为胶乳凝结用喷嘴粘附到插入特定距离的分割区域 管之间。 构成:衬底板2被分成两个或更多个区域,放置> = 5mm的间隙。 在区域之间,并且每个区域牢固地配备具有> = 3mm的突出长度的细管1。 在板上方,间隙> = 1mm。 在管之间,组件用作聚合物胶乳凝结的喷嘴。 喷嘴连接到夹持器3上,夹具5夹着夹具5,并将聚合物胶乳通过细管1挤出成凝固浴。 将凝结的聚合物转移到固化罐中并加热,得到固化的聚合物颗粒。
    • 10. 发明专利
    • Coagulation of polymer latex
    • 聚合物的凝聚
    • JPS59172523A
    • 1984-09-29
    • JP4752383
    • 1983-03-22
    • Mitsubishi Rayon Co Ltd
    • SUGIMORI TERUHIKOTAJIRI TAKAYUKIHIRONAKA AKIOHABARA HIDEAKI
    • C08J3/16C08C1/00C08C1/14C08F6/00C08F6/22
    • PURPOSE: To obtain polymer powder or grains of excellent powder or grain properties from a polymer latex, by using a nozzle for latex coagulation comprising a base plate provided with a plurality of small tubes each having a specified gap and a specified length.
      CONSTITUTION: In coagulating a polymer latex, use is made of a nozzle for latex cogulation, comprising a base plate provided with a plurality of small tubes in such a manner that the gap between the tubes is at least 1mm and the projection of the tube beyond the base plate is at least 3mm. When the tubes protrude beyond the base plate by at least 3mm, their tips are to reach the laminar region outside the eddy region, and therefore the polymer latex extruded from these tips can be gently carried by the laminar flow of the coagulation solution and coagulated to form high-bulk density polymer powder or grains free of fine powder and coarse grains. If the gap between the tubes is as narrow as 1mm or below, the flowing of the coagulation solution into the tubing becomes difficult, so that satisfactory coagulation becomes impossible in the area outside the periphery of the tubing. Therefore, the gap between the tubes must be at least 1mm.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:为了从聚合物胶乳获得具有优异粉末或颗粒性质的聚合物粉末或颗粒,通过使用用于胶乳凝结的喷嘴,其包括设置有多个小管的基板,每个小管具有指定的间隙和指定的长度。 构成:在凝聚聚合物胶乳时,使用用于胶乳结合的喷嘴,包括设置有多个小管的基板,使得管之间的间隙至少为1mm。 并且管超过基板的突起至少为3mm。当管突出超过基板至少3mm时,其尖端将到达涡流区域外的层流区域,因此聚合物胶乳从 这些尖端可以通过凝固溶液的层流轻轻地携带,并凝结成形成高密度聚合物粉末或不含细粉末和粗颗粒的颗粒。 如果管之间的间隙窄至1mm。 或以下时,凝结液流入管路变得困难,因此在管外周边的区域内不可能令人满意的凝固。 因此,管之间的间隙必须至少为1mm ..