    • Heat-shrinkable laminated film, molded product using it, heat-shrinkable label and container on which molded product or heat-shrinkable label is mounted
    • 热收缩层压膜,使用它的模制产品,热缩标签和容器在模制产品或热收缩标签安装
    • JP2008044365A
    • 2008-02-28
    • JP2007188668
    • 2007-07-19
    • Mitsubishi Plastics Ind Ltd三菱樹脂株式会社
    • HIRUMA TAKASHITOZAKI HIROYUKITEJIMA TOMOJIMIYASHITA KAZUHISAYAMADA TAKEMIKITAKAGI JUN
    • B32B27/32B32B27/36B65D65/40
    • Y02W30/801Y02W30/805Y02W90/12
    • PROBLEM TO BE SOLVED: To provide a heat-shrinkable laminated film excellent in low temperature shrinkability, shrink finish properties and transparency and suitable for user in a heat-shrinkable label or the like capable of keeping good transparency even at the time of regeneration and addition, and a plastic container on which the heat-shrinkable label comprising the heat-shrinkable laminated film is mounted. SOLUTION: In the heat-shrinkable film composed of at least two layers, that are, a layer (I) and a layer (II), the layer (I) is constituted using a polyolefinic resin (A), a polylactic acid resin (B) and an adjusting agent (C) which adjusts the refractive indexes of the polyolefinic resin (A) and the polylactic acid resin (B) and having a predetermined SP value and a predetermined refractive index as main components and the layer (II) is constituted based on the polylactic acid resin and the heat shrinkage factor in the main shrink direction of the film when the film is immersed in hot water of 80°C for 10 sec is set to 30% or above. COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供低温收缩性,收缩整理性和透明性优异的热收缩层压膜,并且适用于能够保持良好透明性的热收缩标签等中的用户,即使在 再生和添加,以及塑料容器,其上装有包含该热收缩层压膜的热收缩标签。 解决方案:在由至少两层(即,层(I)和层(II))组成的热收缩膜中,层(I)使用聚烯烃树脂(A),聚乳酸 酸性树脂(B)和调节聚烯烃树脂(A)和聚乳酸树脂(B)的折射率并具有预定的SP值和预定折射率的折射率作为主要成分的调色剂(C) II)构成时,将膜浸渍在80℃的热水中10秒后,将膜的主收缩方向的热收缩率设定为30%以上。 版权所有(C)2008,JPO&INPIT
    • 6. 发明专利
    • Heat shrinkable laminated film roll
    • 热收缩层压膜
    • JP2010042619A
    • 2010-02-25
    • JP2008208879
    • 2008-08-14
    • Mitsubishi Plastics Inc三菱樹脂株式会社
    • TOZAKI HIROYUKI
    • B32B27/32B29C61/06B29K23/00B29K67/00B29K105/02B29L9/00B32B27/36
    • PROBLEM TO BE SOLVED: To provide a heat-shrinkable film roll which has good high-precision printability over the whole roll even after prolonged storage and which can follow high-speed printing nature and a sealing nature. SOLUTION: The film roll is formed by rolling a heat-shrinkable film, which is composed of at least two layers, a poly lactic acid based resin (I) layer and a polyolefin based resin (II) layer and has effective length of ≥1000 m, around a core, wherein (1) average hardness is 300 to 800 when an unwinding part surface of the film roll is measured at 20 mm intervals in a film width direction by using a drop type hardness tester, (2) variation in the average hardness is ≤±200 and (3) an increasing ratio of the average hardness after unwinding the film from the unwinding part in unit of 500 m is 0.25 to 5.0%. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种即使在长时间储存​​之后也能在全辊上具有良好的高精度印刷性的热收缩膜卷,并且可以跟随高速印刷性和密封性。 解决方案:通过将由聚乳酸类树脂(I)层和聚烯烃类树脂(II)层构成的至少两层的热收缩性膜卷绕而成膜,并且具有有效长度 (1)平均硬度为300〜800,当使用滴式硬度计在膜宽度方向上以20mm的间隔测量膜卷的退绕部分表面时,(2) 平均硬度的变化为≤±200,(3)以500μm为单位将退卷后的膜退绕的平均硬度的比率增加为0.25〜5.0%。 版权所有(C)2010,JPO&INPIT
    • 8. 发明专利
    • Laminated film, formed article using the same, heat shrinkable label, and container equipped with the label
    • 层压膜,成型用品,热收缩标签和装有标签的容器
    • JP2008307896A
    • 2008-12-25
    • JP2008128947
    • 2008-05-15
    • Mitsubishi Plastics Inc三菱樹脂株式会社
    • MUTA TAKATOSHITOZAKI HIROYUKIHIRUMA TAKASHITAKAGI JUN
    • B32B27/36B29C55/02B29C61/06B29K67/00B29K105/02B29L7/00B29L9/00B32B7/02B65D25/36B65D65/04B65D65/40G09F3/04
    • PROBLEM TO BE SOLVED: To provide a laminated film excellent in heat resistance, appearance, and hard to release even if treating at a high temperature. SOLUTION: The laminated film comprising an outer layer composed of a polyester based resin as a principal constituent, an inner layer composed of a thermoplastic resin as a principal constituent, and an adhesive layer composed of an adhesive resin as a principal constituent disposed between the outer layer and the inner layer, has an overlapped part having a width of 2-7 mm formed on the laminated film by sealing an outer layer surface of one end side in the direction of drawing with an inner or outer layer surface of another side in the direction of drawing so as to be parallel with the direction of drawing, wherein a slipped width between the end face of the outer layer sealed at the overlapped part or the end face of the outer layer and the adhesive layer and the end face of the adhesive layer and the inner layer or the end face of the inner layer is not greater than 5% of the overlapped width of the overlapped part when returned to the room temperature after heat-treatment at 90°C. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:即使在高温下处理,也提供耐热性,外观和难以释放的层压膜。 < P>解决方案:将由以聚酯类树脂为主要成分的外层,以热塑性树脂为主要成分的内层和以粘合树脂为主要成分的粘合层构成的层叠膜 在外层和内层之间具有通过将拉伸方向上的一端侧的外层表面与另一层的内层或外层表面密封而形成在层压膜上形成的宽度为2-7mm的重叠部分 在拉伸方向上与拉伸方向平行的方向,其中在外层的重叠部分或端面密封的外层的端面与粘合层之间的滑动宽度和端面 的粘合剂层和内层或内层的端面在热处理后返回室温时不大于重叠部分的重叠宽度的5% C。 版权所有(C)2009,JPO&INPIT