    • 1. 发明专利
    • Manufacture of tin-free steel with superior resistance to retorting
    • 具有超耐电阻的无铅钢的制造
    • JPS5974296A
    • 1984-04-26
    • JP18489582
    • 1982-10-21
    • Kawasaki Steel Corp
    • OGATA HAJIMEICHIDA TOSHIROUTSUGAWA SHIYUNICHIYAMAJI KIYOUKOIRIE TOSHIO
    • C25D11/38C25D3/06C25D5/26C25D11/26
    • PURPOSE: To obtain the titled steel for a can by subjecting a steel sheet to reverse electrolysis using the sheet as an anode between a Cr plating stage and an electrolytic chromating stage while restricting the current density and the quantity of electricity.
      CONSTITUTION: A steel sheet is plated with metallic Cr by cathodic electrolysis in an aqueous soln. contg. Cr as the principal component. The plated sheet is subjected to anodizing (reverse electrolysis) in the soln., and it is electrolytically chromated in an aqueous soln. contg. ≥1 kinds of compound selected from chromic anhydride, dichromates and chromates to obtain a tin-free steel (TFS). Said reverse electrolysis is carred out while satisfying equations I WIII [where x is current density (A/dm
      2 ), and y is the quantity (C/dm
      2 ) of electricity].
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:在限制电流密度和电量的同时,通过在铬镀层和电解铬酸盐化阶段之间使用该片材作为阳极,对钢板进行电解反应来获得罐头的标准钢。 构成:通过阴极电解在水性溶胶中钢板上镀金属铬。 contg。 Cr为主要成分。 电镀片在溶胶中进行阳极氧化(反电解),并在水溶液中进行电解铬酸化。 contg。 > = 1种选自铬酸酐,重铬酸盐和铬酸盐的化合物,得到无锡钢(TFS)。 在满足方程式I-III [其中x为电流密度(A / dm 2)],y为电量(C / dm 2)时,表示反向电解。
    • 2. 发明专利
    • Tin-free steel sheet with superior adhesive strength to paint
    • 无铅钢板,具有优异的粘合强度
    • JPS59157296A
    • 1984-09-06
    • JP3046483
    • 1983-02-25
    • Kawasaki Steel Corp
    • OGATA HAJIMEOOHASHI ZENJIYAMAJI KIYOUKOICHIDA TOSHIROUIRIE TOSHIO
    • G01N21/88C25D3/04C25D5/26C25D11/38G01N21/84
    • PURPOSE: To obtain a tin-free steel sheet for a can with improved adhesive strength to paint by specifying the degree of olation of a chromium oxide film on tin-free steel in an ordinary state and the degree of olation of the film after heat treatment.
      CONSTITUTION: A tin-free steel sheet having a two-layered film consisting of a metallic chromium layer and a chromium oxide layer is manufactured. At this time, conditions during electrolysis, etc. are selected so as to satisfy equations 0.50≤x≤1.0, 0.40≤y≤1.0 and y≤x, wherein x is the degree of olation of the chromium oxide film in an ordinary state measured by Fourier-transform infrared spectroscopy (FTIR), and y is the degree of olation of the film after heat treatment at 200°C for 10min. The tin-free steel sheet satisfying the equations has superior adhesive strength to paint and can be used as the material of cans for various drinks.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:通过指定普通状态下的无锡钢上的氧化铬膜的放出程度和热处理后的膜的放电程度,获得具有改善的粘合强度的罐的无锡钢板,进行涂漆 。 构成:制造具有由金属铬层和氧化铬层构成的2层膜的无锡钢板。 此时,选择电解等条件,以满足方程式0.50 <= x <= 1.0,0.40 <= y <= 1.0和y <= x,其中x是氧化铬膜的放电程度 在通过傅里叶变换红外光谱(FTIR)测量的普通状态下,y是在200℃下热处理10分钟后的膜的充气度。 满足方程式的无锡钢板具有优异的涂料粘合强度,可用作各种饮料罐的材料。
    • 3. 发明专利
    • Manufacture of tin-free steel sheet with superior adhesion to paint
    • 无铅钢板的制造与超级粘合剂涂料
    • JPS59170298A
    • 1984-09-26
    • JP4294283
    • 1983-03-15
    • Kawasaki Steel Corp
    • OGATA HAJIMEYAMAJI KIYOUKOTSUGAWA SHIYUNICHIICHIDA TOSHIROUIRIE TOSHIO
    • C25D5/48C25D11/38
    • C25D11/38C25D5/48
    • PURPOSE: To manufacture a tin-free steel sheet with superior adhesion to paint by specifying the concn. of sexivalent Cr in a base and the concn. of F in a compound contg. F as an auxiliary in electrolytic chromating.
      CONSTITUTION: A steel sheet is plated with metallic Cr by cathodic electrolysis in an aqueous soln. contg. Cr, and the Cr plated steel sheet is anodized (reversely electrolyzed) in the Cr plating soln. The reversely electrolyzed steel sheet is electrolytically chromated in an aqueous soln. contg. ≥1 kinds of compounds selected among chromic anhydride, chromates and dichromates as principal components. At this time, the concn. of sexivalent Cr in the base in the bath is adjusted to 0.2W1.4mol/l in terms of CrO
      2 , and a compound contg. F such as H
      2 SiF
      6 or HBF
      4 is added as an auxiliary in 1/1,000W1/20 molar ratio of F
      - /Cr
      6+ .
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:通过指定浓缩液,制造出具有优异涂料附着力的无锡钢板。 基础中的等价性Cr和浓度 的F在复合物 F作为电解铬酸盐的辅助剂。 构成:通过阴极电解在水性溶胶中钢板上镀金属铬。 contg。 Cr,镀铬钢板在Cr镀敷溶液中进行阳极氧化(反向电解)。 反电解钢板在水溶液中电解镀铬。 contg。 > = 1种选自铬酸酐,铬酸盐和重铬酸盐为主要成分的化合物。 在这个时候, 在浴中碱性中的等价Cr调节为0.2-1.4mol / l,以CrO 2计,化合物 在1 / 1,000-1 / 20摩尔比的F 1 / Cr 6+中加入F如H 2 SiF 6或HBF 4作为辅助剂。
    • 4. 发明专利
    • Chromium-plated steel plate for planographic printing
    • 镀铬钢板用于平面印刷
    • JPS59142192A
    • 1984-08-15
    • JP1581583
    • 1983-02-02
    • Kawasaki Steel Corp
    • OGATA HAJIMEICHIDA TOSHIROUTSUGAWA SHIYUNICHIYAMAJI KIYOUKOIRIE TOSHIO
    • B41N1/10
    • B41N1/10
    • PURPOSE:To obtain a chromium-plated steel plate excellent in hydrophilic property, water retention and anti-rusting property and having durability in printing comparable to that of an aluminum planographic printing plate, by providing a metallic chromium layer and a hydrated chromium oxide layer on a surface of a steel plate roughened by an electrolytic treatment with the steel plate as an anode in an aqueous solution of sulfuric acid. CONSTITUTION:In an aqueous solution containing 30-300g/l of H2SO4 and not more than 300g/l of FeSO4 at a temperature of 20-100 deg.C, a steel plate is roughened by electrolytic washing by using the plate as an anode with a quantity of electricity of 200-2,000C/dm so that the surface roughness after providing the metallic chromium layer and the hydrated chromium oxide layer thereon becomes an Ra value of 0.3-1.0mum and a PPI value at 0.5mum of 100-800. The quantity of metallic chromium is preferably 70-200mg/m , and the quantity of chromium in the hydrated chromium oxide layer is preferably 8-60mg/m .
    • 目的:为了获得具有优异的亲水性,保水性和防锈性,并具有与铝平版印刷版相当的印刷耐久性的镀铬钢板,通过将金属铬层和水合氧化铬层提供在 通过在硫酸水溶液中用钢板作为阳极进行电解处理使钢板的表面粗糙化。 构成:在20-100℃的温度下含有30-300g / l的H 2 SO 4和不超过300g / l的FeSO 4的水溶液中,通过使用该板作为阳极的电解洗涤使钢板粗糙化, 电量为200-2,000℃/ dm 2,使得在其上提供金属铬层和水合氧化铬层之后的表面粗糙度为Ra值为0.3-1.0μm,PPI值为0.5μm时为100 -800。 金属铬的量优选为70〜200mg / m 2,水合氧化铬层中的铬的量优选为8-60mg / m 2。